# US 2009/0155710 A1 · Method of manufacturing toner and toner produced by the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0155710 A1
- Document ID: US20090155710A1
- Status: Published application
- Kind: A1
- Application number: 12/332,549
- Filed: 2008-12-11
- Published: 2009-06-18
- Earliest claimed: 2007-12-14
- Assignees: Ricoh Company, Ltd.
- Inventors: Mitsuo AOKI; Satoshi OGAWA
- Web page: https://patentgrep.com/patent/US20090155710A1

## CPC

- G03G 9/081: {by mixing the toner components in a liquefied state; melt kneading; reactive mixing}
- G03G 9/08782: {Waxes}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A method of manufacturing toner including the steps of preparing a preliminary mixture by mixing a colorant and a release agent; preparing a raw material mixture by mixing the preliminary mixture with a binder resin and other raw materials; melt-kneading the raw material mixture using an open system roll type kneader; pulverizing the melt-kneaded raw material mixture into fine particles; and classifying the fine particles to prepare a toner.

## Claims

### Claim 1

A method of manufacturing toner, comprising the steps of:
preparing a preliminary mixture by mixing a colorant and a release agent; and
preparing a raw material mixture by mixing the preliminary mixture with a binder resin and other raw materials;
melt-kneading the raw material mixture using an open system roll type kneader;
pulverizing the melt-kneaded raw material mixture into fine particles; and
classifying the fine particles to prepare a toner.

### Claim 2 (depends on 1)

The method of manufacturing toner according to claim 1, wherein the release agent has a weight average particle diameter of from 5 to 100 μm.

### Claim 3 (depends on 1)

The method of manufacturing toner according to claim 1, wherein the release agent comprises an amount of from 3.0 to 8.0% by weight based on a total weight of the raw materials.

### Claim 4 (depends on 1)

The method of manufacturing toner according to claim 1, wherein the release agent has a penetration of 5 mm or less.

### Claim 5

A toner comprising a binder resin, a colorant, and a release agent, manufactured by a method comprising the steps of:
preparing a preliminary mixture by mixing the colorant and the release agent; and
preparing a raw material mixture by mixing the preliminary mixture with the binder resin and other raw materials;
melt-kneading the raw material mixture using an open system roll type kneader;
pulverizing the melt-kneaded raw material mixture into fine particles; and
classifying the fine particles to prepare the toner.

### Claim 6 (depends on 5)

The toner according to claim 5, wherein the release agent has a weight average particle diameter of from 5 to 100 μm.

### Claim 7 (depends on 5)

The toner according to claim 5, wherein the release agent comprises an amount of from 3.0 to 8.0% by weight based on a total weight of the raw materials.

### Claim 8 (depends on 5)

The toner according to claim 5, wherein the release agent has a penetration of 5 mm or less.