# US 2009/0047856 A1 · Area bonded nonwoven fabric from single polymer system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0047856 A1
- Document ID: US20090047856A1
- Status: Published application
- Kind: A1
- Application number: 12/228,656
- Filed: 2008-08-14
- Published: 2009-02-19
- Earliest claimed: 2007-08-17
- Assignees: Fiberweb, Inc.
- Inventors: Gregory W. Farrell; Edward Keith Willis
- Web page: https://patentgrep.com/patent/US20090047856A1

## CPC

- D04H 1/56: in association with fibre formation, e.g. immediately following extrusion of staple fibres
- D01D 5/30: Conjugate filaments; Spinnerette packs therefor
- D01F 8/14: with at least one polyester as constituent
- D04H 1/565: {by melt-blowing}
- D04H 3/011: Polyesters
- D04H 3/147: Composite yarns or filaments
- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- Y10T 428/2913: Rod, strand, filament or fiber
- Y10T 428/2915: including textile, cloth or fabric
- Y10T 428/2929: Bicomponent, conjugate, composite or collateral fibers or filaments [i.e., coextruded sheath-core or side-by-side type]
- Y10T 428/2973: Particular cross section
- Y10T 428/2978: Surface characteristic
- Y10T 442/608: Including strand or fiber material which is of specific structural definition
- Y10T 442/609: Cross-sectional configuration of strand or fiber material is specified
- Y10T 442/611: Cross-sectional configuration of strand or fiber material is other than circular
- Y10T 442/637: Including strand or fiber material which is a monofilament composed of two or more polymeric materials in physically distinct relationship [e.g., sheath-core, side-by-side, islands-in-sea, fibrils-in-matrix, etc.] or composed of physical blend of chemically different polymeric materials or a physical blend of a polymeric material and a filler material
- Y10T 442/641: Sheath-core multicomponent strand or fiber material
- Y10T 442/681: Spun-bonded nonwoven fabric
- Y10T 442/69: Autogenously bonded nonwoven fabric
- Y10T 442/697: Containing at least two chemically different strand or fiber materials
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A nonwoven fabric is provided having a plurality of semi-crystalline filaments that are thermally bonded to each other and are formed of the same polymer and exhibit substantially the same melting temperature. The fabric is produced by melt spinning an amorphous crystallizable polymer to form two components having different levels of crystallinity. During spinning, a first component of the polymer is exposed to conditions that result in stress-induced crystallization such that the first polymer component is in a semi-crystalline state and serves as the matrix or strength component of the fabric. The second polymer component is not subjected to stress induced crystallization and thus remains in a substantially amorphous state which bonds well at relatively low temperatures. In a bonding step, the fabric is heated to soften and fuse the binder component. Under these conditions, the binder component undergoes thermal crystallization so that in the final product, both polymer components are semi-crystalline.

## Claims

### Claim 1

A method of making a nonwoven fabric comprising the steps of melt extruding a crystallizable amorphous polymer to produce a plurality of fibers; subjecting the polymer to processing conditions that produce a first polymer component that is at least partially crystalline and a second polymer component that is substantially amorphous; depositing the fibers on a collection surface to form a web containing both said partially crystalline first polymer component and said amorphous second polymer component; bonding the fibers to one another to form a bonded nonwoven web in which the amorphous second polymer component softens and fuses to form bonds with the first polymer component; and effecting crystallization of the second polymer component so that in the resulting nonwoven fabric both said polymer components are at least partially crystalline.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of subjecting the polymer to processing conditions that produce first and second polymer components comprises subjecting a first portion of the polymer to stress that induces crystallization to form said first polymer component, and subjecting a second portion of the polymer to stress that is insufficient to induce crystallization to form said second polymer component.

### Claim 3 (depends on 1)

The method of claim 1, wherein the step of melt extruding comprises melt extruding the polymer through one or more spinnerets that form first and second groups of continuous filaments, and said step of subjecting the polymer to processing conditions that produce first and second polymer components comprises subjecting the first group of continuous filaments to stress that induces crystallization, and subjecting the second group of continuous filaments to stress insufficient to induce crystallization.

### Claim 4 (depends on 3)

The method of claim 3, wherein the steps of subjecting the first and second groups of filaments to stress to induce or not induce crystallization comprises drawing the filaments under differing draw conditions.

### Claim 5 (depends on 3)

The method of claim 3, wherein the steps of subjecting the first and second groups of filaments to stress to induce or not induce crystallization comprises extruding the filaments at differing extrusion rates.

### Claim 6 (depends on 3)

The method of claim 3, wherein the step of extruding a crystallizable polymer comprising extruding said polymer from first and second extruders, and wherein said step of subjecting the polymer to processing conditions that produce first and second polymer components comprises providing a reduction in the intrinsic viscosity of the polymer in the second extruder relative to the intrinsic viscosity of the polymer in the first extruder.

### Claim 7 (depends on 6)

The method of claim 6, wherein the intrinsic viscosity of the polymer in the second extruder is lowered by adding a viscosity lowering compound to the polymer in the second extruder.

### Claim 8 (depends on 6)

The method of claim 6, wherein the intrinsic viscosity of the polymer in the second extruder is lowered by adding recycled polymer to the second extruder.

### Claim 9 (depends on 6)

The method of claim 6, wherein the step of melt extruding a crystallizable amorphous polymer to produce a plurality of fibers comprises melt extruding the polymer through one or more spinnerets configured to form bicomponent filaments with the first and second polymer components present in distinct portions of the cross section of the filament.

### Claim 10 (depends on 9)

The method of claim 9, wherein the spinnerets are configured to form continuous multilobal filaments with the second polymer component present in at least some of the lobes of the filaments.

### Claim 11 (depends on 1)

The method of claim 1, wherein the crystallizable polymer is selected from the group consisting of polyethylene terephthalate, polytrimethylene terphthalate, polybutylene terephthalate, and polylactic acid, and copolymers, and combinations thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein the second polymer component prior to bonding has a softening temperature that is at least 5° C. less than a softening temperature of the first polymer component.

### Claim 13 (depends on 1)

The method of claim 1, wherein the step of bonding the fibers comprises heating the fibers to a temperature at which the second polymer component softens and becomes tacky while the first polymer component remains solid, maintaining the fibers in the form of a web while the softened second polymer component adheres to portions of other fibers at fiber crossover points, and cooling the fibers to solidify the second polymer component and form a bonded nonwoven web.

### Claim 14

A method of making a nonwoven fabric comprising the steps of:
melt extruding a crystallizable amorphous polymer through one or more spinnerets that form first and second groups of continuous filaments;
subjecting the first and second groups of continuous filaments to processing conditions that impart stress to the first group of filaments producing stress-induced crystallization such that the filaments are at least partially crystallized, and imparts stress to the second group of continuous filaments insufficient to produce stress-induced crystallization such that the filaments remain substantially amorphous;
depositing the first and second groups of continuous filaments on a collection surface to form a web containing both said partially crystalline first filaments as matrix filaments and said amorphous second filaments as binder filaments;
heating the web so that the amorphous binder filaments soften and fuse to form bonds with one another and with the matrix filaments while maintaining their continuous filamentary form; and
effecting crystallization of the amorphous binder filament during the heating step so that in the resulting nonwoven fabric both said matrix filaments and said binder filaments are at least partially crystalline.

### Claim 15 (depends on 14)

The method of claim 14, wherein the crystallizable amorphous polymer comprises polyethylene terephthalate.

### Claim 16 (depends on 14)

The method of claim 14, wherein the step of subjecting the first and second groups of filaments to processing conditions that impart stress comprises providing a different intrinsic viscosity in the polymers of the first and second groups of filaments.

### Claim 17 (depends on 14)

The method of claim 14, wherein the steps of subjecting the first and second groups of filaments to processing conditions that impart stress comprises extruding the filaments at differing extrusion rates.

### Claim 18

A method of making a nonwoven fabric comprising the steps of:
melt extruding a crystallizable amorphous polymer through one or more spinnerets configured to form bicomponent filaments having first and second polymer components present in distinct portions of the cross section of the filament, wherein the intrinsic viscosity of the polymer in the second component is reduced relative to the intrinsic viscosity of the polymer in the first component.
attenuating the filaments to cause stress-induced crystallization in the first polymer component of the filaments but without producing stress-induced crystallization in the second polymer component such that the second polymer component remains substantially amorphous;
depositing the bicomponent filaments on a collection surface to form a web in which the first polymer component of the filaments is partially crystalline and serves as the matrix component of the filaments and the second polymer component of the filament is amorphous and serves as the binder component of the filaments;
heating the web so that the amorphous binder component of the filaments softens and fuses to form bonds with contacting filaments while the filaments maintain their continuous filamentary form; and
effecting crystallization of the amorphous binder component of the filaments during the heating step so that in the resulting nonwoven fabric both the matrix component and the binder component of the bicomponent filaments are at least partially crystalline.

### Claim 19 (depends on 18)

The method of claim 18, including providing the first and second polymer components of differing intrinsic viscosity from two separate sources.

### Claim 20 (depends on 18)

The method of claim 18, including providing the first and second polymer components of from the same source and lowering the intrinsic viscosity of the second polymer component by introducing a viscosity lowering additive.

### Claim 21

An area bonded nonwoven fabric comprising fibers of a semi-crystalline thermoplastic polymer fusion bonded to one another throughout the fabric to form a strong coherent nonwoven fabric, and wherein the fibers of the nonwoven fabric exhibit a single melting peak as evidenced by a DSC trace.

### Claim 22 (depends on 21)

The nonwoven fabric of claim 21, wherein the fibers include matrix fibers crystallized under stress and binder fibers thermally crystallized without stress, and wherein the fibers are fusion bonded only by the binder fibers.

### Claim 23 (depends on 22)

The nonwoven fabric of claim 22, wherein the matrix fibers and the binder fibers exhibit different dye uptakes.

### Claim 24 (depends on 21)

The nonwoven fabric of claim 21, wherein the semi-crystalline polymer of the fibers has a degree of crystallinity of at least 50%.

### Claim 25 (depends on 24)

The nonwoven fabric of claim 24, wherein the polymer has a degree of crystallinity of at least 80%.

### Claim 26 (depends on 21)

The nonwoven fabric of claim 21, wherein the semi-crystalline polymer is a polyester selected from the group consisting of polyethylene terephthalate, polytrimethylene terephthalate, polybutylene terephthalate, and polylactic acid.

### Claim 27 (depends on 21)

The nonwoven fabric of claim 21, wherein the fibers of the nonwoven fabric comprise interconnected continuous filaments in which some of the filaments have fused to adjacent filaments at points contact and wherein some of the filaments have not fused to adjacent filaments at points of contact.

### Claim 28

An area bonded spunbond nonwoven fabric consisting essentially of continuous filaments of a semi-crystalline thermoplastic polymer and a multiplicity of thermal fusion bonds located throughout the fabric, the fusion bonds consisting of areas in which contacting filaments have softened and thermally fused to one another, and wherein the filaments have retained their filamentary form throughout the fabric.

### Claim 29 (depends on 28)

The nonwoven fabric according to claim 28, wherein the filaments have a multilobal cross-section.

### Claim 30 (depends on 29)

The nonwoven fabric according to claim 29, wherein the fusion bonds are present only on the lobes of the multilobal filaments.

### Claim 31 (depends on 28)

The nonwoven fabric of claim 28, wherein the continuous filaments of the nonwoven fabric include matrix filaments crystallized under stress and binder filaments thermally crystallized without stress, and wherein said fusion bonds are formed only by the binder filaments.

### Claim 32 (depends on 28)

The nonwoven fabric of claim 28, wherein the semi-crystalline polymer of the fibers has a degree of crystallinity of at least 95%.

### Claim 33 (depends on 28)

The nonwoven fabric of claim 28, wherein the semi-crystalline polymer is a polyester selected from the group consisting of polyethylene terephthalate, polytrimethylene terephthalate, polybutylene terephthalate, and polylactic acid.

### Claim 34

An area bonded spunbond nonwoven fabric comprising continuous filaments of polyethylene terephthalate homopolymer including matrix filaments melt extruded from a relatively higher intrinsic viscosity polyethylene terephthalate homopolymer and binder filaments melt extruded from a relatively lower intrinsic viscosity polyethylene terephthalate homopolymer, and a multiplicity of thermal fusion bonds located throughout the fabric, the fusion bonds consisting of areas in which the binder filaments have softened and thermally fused to adjacent filaments at points of contact, and wherein the binder and matrix filaments have retained their filamentary form throughout the fabric, and wherein both the matrix and binder filaments are in a semi-crystalline state and exhibit a single melting peak as evidenced by a DSC trace.

### Claim 35 (depends on 34)

The nonwoven fabric of claim 34, wherein the matrix filaments are formed with polyethylene terephthalate homopolymer having an intrinsic viscosity of about 0.65 dl/g or greater and the binder filaments are formed with polyethylene terephthalate homopolymer having an intrinsic viscosity of about 0.62 dl/g or less.

### Claim 36 (depends on 34)

The nonwoven fabric of claim 34, wherein the matrix filaments and the binder filaments exhibit different dye uptakes.

### Claim 37 (depends on 34)

The nonwoven fabric of claim 34, wherein the semi-crystalline polymer of the matrix and binder filaments has a degree of crystallinity of at least 95%.

### Claim 38

An area bonded spunbond nonwoven fabric comprising continuous bicomponent filaments of polyethylene terephthalate homopolymer including a matrix component melt extruded from a relatively higher intrinsic viscosity polyethylene terephthalate homopolymer and a binder component melt extruded from a relatively lower intrinsic viscosity polyethylene terephthalate homopolymer, and a multiplicity of thermal fusion bonds located throughout the fabric, the fusion bonds consisting of areas in which the binder component has softened and thermally fused to adjacent filaments at points of contact, and wherein both the matrix and binder components are in a semi-crystalline state and exhibit a single melting peak as evidenced by a DSC trace.

### Claim 39 (depends on 38)

The nonwoven fabric of claim 38, wherein the matrix component is formed with polyethylene terephthalate homopolymer having an intrinsic viscosity of about 0.65 dl/g or greater and the binder component is formed with polyethylene terephthalate homopolymer having an intrinsic viscosity of about 0.62 dl/g or less.

### Claim 40 (depends on 38)

The nonwoven fabric of claim 38, wherein the bicomponent filaments have a sheath-core cross-sectional configuration with the matrix component occupying the core and the binder component occupying the surrounding sheath.

### Claim 41 (depends on 38)

The nonwoven fabric of claim 38, wherein the semi-crystalline polymer of the matrix and binder components has a degree of crystallinity of at least 95%.

### Claim 42 (depends on 1)

An area bonded nonwoven fabric produced by the method of claim 1.

### Claim 43 (depends on 14)

An area bonded nonwoven fabric produced by the method of claim 14.

### Claim 44 (depends on 18)

An area bonded nonwoven fabric produced by the method of claim 18.