# US 2009/0023891 A1 · Treatment method for imparting self-healing and shape memory properties to certain cbdo copolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0023891 A1
- Document ID: US20090023891A1
- Status: Published application
- Kind: A1
- Application number: 12/173,186
- Filed: 2008-07-15
- Published: 2009-01-22
- Earliest claimed: 2007-07-16
- Assignees: Texas State University
- Inventors: Gary W. Beall; Jesse R. Hancock; Chad J. Booth
- Web page: https://patentgrep.com/patent/US20090023891A1

## CPC

- C08G 63/88: Post-polymerisation treatment
- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

According to the invention, an amorphous CBDO polymer (as described in U.S. Pat. No. 5,705,575, issued Jan. 6, 1998, which U.S. patent is incorporated herein by reference in its entirety) is imparted self healing and shape memory properties by heat treatment.

## Claims

### Claim 1

A method for treating an amorphous CBDO copolymer to impart self healing and shape memory properties comprising:
heating said copolymer to a temperature above its glass transition temperature.

### Claim 2 (depends on 1)

A method as in claim 1, wherein the copolymer is first bent before being heated.

### Claim 3 (depends on 1)

A method as in claim 1, wherein the copolymer is first dented before being heated.

### Claim 4 (depends on 1)

A method as in claim 1, wherein the copolymer is first scratched before being heated.

### Claim 5 (depends on 1)

A method as in claim 1, wherein the copolymer is first deformed by any means before being heated.

### Claim 6 (depends on 1)

The product produced by the process of claim 1.

### Claim 7

The product produced by heating an amorphous CBDO copolymer to a temperature above its glass transition temperature.