# US 2009/0023885 A1 · Treatment method for imparting high impact resistance in certain cbdo copolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0023885 A1
- Document ID: US20090023885A1
- Status: Published application
- Kind: A1
- Application number: 12/173,314
- Filed: 2008-07-15
- Published: 2009-01-22
- Earliest claimed: 2007-07-16
- Assignees: Texas State University—San Marcos
- Inventors: Gary W. Beall; Jesse R. Hancock; Chad J. Booth
- Web page: https://patentgrep.com/patent/US20090023885A1

## CPC

- C08G 63/88: Post-polymerisation treatment
- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

According to the invention, an amorphous CBDO copolymer (as described in U.S. Pat. No. 5,705,575, issued Jan. 6, 1998, which U.S. patent is incorporated herein by reference in its entirety) is treated to impart high impact resistance, also called impact strength.

## Claims

### Claim 1

A method for treating an amorphous CBDO copolymer containing an effective amount of cis isomer comprising heating said copolymer to a temperature above its glass transition temperature and then cooling it to a temperature below its glass transition temperature at a cooling rate fast enough to impart a high impact strength.

### Claim 2 (depends on 1)

A method as in claim 1, wherein the copolymer is cooled at a rate enough greater than about 0.5° C. per minute to impart a high impact strength.

### Claim 3 (depends on 1)

A method as in claim 1, wherein the cooling rate is about 8° C. per minute.

### Claim 4 (depends on 1)

A method as in claim 1, wherein the cooling rate is about 15° C. per minute.

### Claim 5 (depends on 1)

A method as in claim 1, wherein cooling is effected by quenching in an ice water bath.

### Claim 6 (depends on 1)

A method as in claim 1, wherein the cis isomer is present in an amount enough greater than about eighteen percent to impart a high impact strength.

### Claim 7 (depends on 1)

A method as in claim 1, wherein the cis isomer is present in at least an amount of about forty six percent or greater.

### Claim 8

A method for treating an amorphous CBDO copolymer containing an effective amount of cis isomer comprising heating said copolymer to a temperature above its glass transition temperature and then cooling it to a temperature below its glass transition temperature by quenching it in an ice water bath.

### Claim 9

A method for treating an amorphous CBDO copolymer containing an effective amount of cis isomer comprising heating said copolymer to a temperature above its glass transition temperature and then cooling it to a temperature below its glass transition temperature at a rate enough greater than about 0.5° C. per minute to impart a high impact strength.

### Claim 10

A method for treating an amorphous CBDO copolymer comprising heating said copolymer to a temperature above its glass transition temperature and then cooling it to a temperature below its glass transition temperature at a cooling rate fast enough to impart a high impact strength, wherein the cis isomer is present in an amount enough greater than about eighteen percent to be effective to impart high impact strength.