# US 2009/0023275 A1 · Method for forming silicon wells of different crystallographic orientations

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0023275 A1
- Document ID: US20090023275A1
- Status: Published application
- Kind: A1
- Application number: 12/175,877
- Filed: 2008-07-18
- Published: 2009-01-22
- Earliest claimed: 2007-07-20
- Assignees: STMicroelectronics (Crolles 2) SAS
- Inventors: Nicolas Loubet; Didier Dutartre; Frederic Boeuf
- Web page: https://patentgrep.com/patent/US20090023275A1

## CPC

- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3466: {Crystal orientation}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing silicon wells of various crystallographic orientations in a silicon support, including the steps of: forming a silicon layer having a first orientation on a silicon substrate having a second orientation; forming insulating walls, defining wells extend at least down to the border between the silicon substrate and the silicon layer; performing, in first wells, a chemical vapor etch (CVE) of the silicon layer by means of hydrochloric acid, in an epitaxy reactor, at a temperature ranging between 700° C. and 950° C.; and performing, in the first wells, a vapor-phase epitaxy on the silicon substrate in the presence of a precursor of silicon and hydrochloric acid, at a temperature ranging between 700° C. and 900° C. and up to the upper surface of the silicon layer.

## Claims

### Claim 1

A method for manufacturing silicon wells of two crystallographic orientations and having smooth upper surfaces, in a silicon support, comprising the successive steps of:
forming a silicon layer having a first orientation on a silicon substrate having a second orientation;
forming insulating walls which extend at least down to the border between the silicon substrate and the silicon layer, these walls defining wells;
performing, in first wells, a chemical vapor etch of the silicon layer by means of hydrochloric acid, in an epitaxy reactor, at a temperature ranging between 700° C. and 950° C.; and
performing, in the first wells, a vapor-phase epitaxy on the silicon substrate in the presence of a precursor of silicon and hydrochloric acid, at a temperature ranging between 700° C. and 900° C. and up to the upper surface of the silicon layer, this epitaxy being performed in said epitaxy reactor.

### Claim 2 (depends on 1)

The method of claim 1, wherein the etch and epitaxy steps are carried out at a pressure ranging between 600 Pa and 11,000 Pa.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first orientation is orientation and the second orientation is orientation.

### Claim 4 (depends on 1)

The method of claim 1, wherein the silicon precursor belongs to the group comprising trichlorosilane, dichlorosilane, and silicon hydrides.