# US 2009/0023270 A1 · Method for manufacturing SOI wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0023270 A1
- Document ID: US20090023270A1
- Status: Published application
- Kind: A1
- Application number: 12/153,160
- Filed: 2008-05-14
- Published: 2009-01-22
- Earliest claimed: 2007-05-31
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Inventors: Shoji Akiyama; Yoshihiro Kubota; Atsuo Ito; Koichi Tanaka; Makoto Kawai; Yuuji Tobisaka
- Web page: https://patentgrep.com/patent/US20090023270A1

## CPC

- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

There is disclosed a method for manufacturing an SOI wafer comprising at least: implanting a hydrogen ion, a rare gas ion, or both the ions into a donor wafer formed of a silicon wafer or a silicon wafer having an oxide film formed on a surface thereof from a surface of the donor wafer, thereby forming an ion implanted layer; performing a plasma activation treatment with respect to at least one of an ion implanted surface of the donor wafer and a surface of a handle wafer, the surface of the handle wafer is to be bonded to the ion implanted surface; closely bonding these surfaces to each other; mechanically delaminating the donor wafer at the ion implanted layer as a boundary and thereby reducing a film thickness thereof to provide an SOI layer, and performing a heat treatment at 600 to 1000° C.; and polishing a surface of the SOI layer for 10 to 50 nm based on chemical mechanical polishing. A method for manufacturing with excellent productivity an SOI wafer having an SOI layer with a mirror-finished surface and high film thickness uniformity can be provided.

## Claims

### Claim 1

A method for manufacturing an SOI wafer comprising at least:
implanting a hydrogen ion, a rare gas ion, or both the ions into a donor wafer formed of a silicon wafer or a silicon wafer having an oxide film formed on a surface thereof from a surface of the donor wafer, thereby forming an ion implanted layer;
performing a plasma activation treatment with respect to at least one of an ion implanted surface of the donor wafer and a surface of a handle wafer, the surface of the handle wafer is to be bonded to the ion implanted surface;
closely bonding the ion implanted surface of the donor wafer to the surface of the handle wafer;
mechanically delaminating the donor wafer at the ion implanted layer as a boundary and thereby reducing a film thickness thereof to provide an SOI layer, and performing a heat treatment at 600 to 1000° C.; and
polishing a surface of the SOI layer for 10 to 50 nm based on chemical mechanical polishing.

### Claim 2

A method for manufacturing an SOI wafer comprising at least:
implanting a hydrogen ion, a rare gas ion, or both the ions into a donor wafer formed of a silicon wafer or a silicon wafer having an oxide film formed on a surface thereof from a surface of the donor wafer, thereby forming an ion implanted layer;
performing a plasma activation treatment with respect to at least one of an ion implanted surface of the donor wafer and a surface of a handle wafer, the surface of the handle wafer is to be bonded to the ion implanted surface;
closely bonding the ion implanted surface of the donor wafer to the surface of the handle wafer;
mechanically delaminating the donor wafer at the ion implanted layer as a boundary and thereby reducing a film thickness thereof to provide an SOI layer, and performing a heat treatment at 600 to 1000° C.; and
etching a surface of the SOI layer for 10 to 50 nm based on a GCIB processing.

### Claim 3 (depends on 2)

The method for manufacturing an SOI wafer according to claim 2, wherein the surface of the SOI layer after the GCIB processing is polished for 10 to 30 nm based on chemical mechanical polishing.

### Claim 4 (depends on 1)

The method for manufacturing an SOI wafer according to claim 1, wherein the handle wafer is any one of a silicon wafer, a silicon wafer having an oxide film formed on a surface thereof, a quartz wafer, a glass wafer, an alumina (sapphire) wafer, a SiC wafer, and an aluminum nitride wafer.

### Claim 5 (depends on 2)

The method for manufacturing an SOI wafer according to claim 2, wherein the handle wafer is any one of a silicon wafer, a silicon wafer having an oxide film formed on a surface thereof, a quartz wafer, a glass wafer, an alumina (sapphire) wafer, a SiC wafer, and an aluminum nitride wafer.

### Claim 6 (depends on 3)

The method for manufacturing an SOI wafer according to claim 3, wherein the handle wafer is any one of a silicon wafer, a silicon wafer having an oxide film formed on a surface thereof, a quartz wafer, a glass wafer, an alumina (sapphire) wafer, a SiC wafer, and an aluminum nitride wafer.

### Claim 7 (depends on 1)

The method for manufacturing an SOI wafer according to claim 1, wherein the ion implanted surface of the donor wafer is closely bonded to the surface of the handle wafer, then a heat treatment is performed at 400° C. or below, and the donor wafer is mechanically delaminated at the ion implanted layer as a boundary.

### Claim 8 (depends on 2)

The method for manufacturing an SOI wafer according to claim 2, wherein the ion implanted surface of the donor wafer is closely bonded to the surface of the handle wafer, then a heat treatment is performed at 400° C. or below, and the donor wafer is mechanically delaminated at the ion implanted layer as a boundary.

### Claim 9 (depends on 3)

The method for manufacturing an SOI wafer according to claim 3, wherein the ion implanted surface of the donor wafer is closely bonded to the surface of the handle wafer, then a heat treatment is performed at 400° C. or below, and the donor wafer is mechanically delaminated at the ion implanted layer as a boundary.

### Claim 10 (depends on 4)

The method for manufacturing an SOI wafer according to claim 4, wherein the ion implanted surface of the donor wafer is closely bonded to the surface of the handle wafer, then a heat treatment is performed at 400° C. or below, and the donor wafer is mechanically delaminated at the ion implanted layer as a boundary.

### Claim 11 (depends on 5)

The method for manufacturing an SOI wafer according to claim 5, wherein the ion implanted surface of the donor wafer is closely bonded to the surface of the handle wafer, then a heat treatment is performed at 400° C. or below, and the donor wafer is mechanically delaminated at the ion implanted layer as a boundary.

### Claim 12 (depends on 6)

The method for manufacturing an SOI wafer according to claim 6, wherein the ion implanted surface of the donor wafer is closely bonded to the surface of the handle wafer, then a heat treatment is performed at 400° C. or below, and the donor wafer is mechanically delaminated at the ion implanted layer as a boundary.

### Claim 13 (depends on 1)

The method for manufacturing an SOI wafer according to claim 1, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 14 (depends on 2)

The method for manufacturing an SOI wafer according to claim 2, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 15 (depends on 3)

The method for manufacturing an SOI wafer according to claim 3, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 16 (depends on 4)

The method for manufacturing an SOI wafer according to claim 4, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 17 (depends on 5)

The method for manufacturing an SOI wafer according to claim 5, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 18 (depends on 6)

The method for manufacturing an SOI wafer according to claim 6, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 19 (depends on 7)

The method for manufacturing an SOI wafer according to claim 7, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 20 (depends on 8)

The method for manufacturing an SOI wafer according to claim 8, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 21 (depends on 9)

The method for manufacturing an SOI wafer according to claim 9, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 22 (depends on 10)

The method for manufacturing an SOI wafer according to claim 10, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 23 (depends on 11)

The method for manufacturing an SOI wafer according to claim 11, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.

### Claim 24 (depends on 12)

The method for manufacturing an SOI wafer according to claim 12, wherein an RMS value indicative of a surface roughness of the SOI layer after the chemical mechanical polishing or the GCIB processing is set to 0.5 nm or below.