# US 2009/0023268 A1 · Isolation method of active area for semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0023268 A1
- Document ID: US20090023268A1
- Status: Published application
- Kind: A1
- Application number: 12/108,306
- Filed: 2008-04-23
- Published: 2009-01-22
- Earliest claimed: 2007-07-19
- Assignees: ProMOS Technologies Inc.
- Inventors: Hsiao-Che WU; Ming-Yen Li; Wen-Li Tsai
- Web page: https://patentgrep.com/patent/US20090023268A1

## CPC

- H10W 10/13: formed using local oxidation of silicon [LOCOS], e.g. sealed interface localised oxidation [SILO] or side-wall mask isolation [SWAMI]
- H10W 10/0121: {in regions recessed from the surface, e.g. in trenches or grooves}
- H10D 84/0188: {Manufacturing their isolation regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

An isolation method of active area for semiconductor forms an isolated active area in a substrate. The substrate is a p-type silicon substrate. A pad oxide layer is formed on the substrate. A patterned sacrificial layer and an upper mask layer are formed on the pad oxide layer, where the upper mask layer is formed over the isolation region of the substrate. A gap is formed between the patterned sacrificial layer and the upper mask layer. An implantation process is performed to dope ions into the substrate through the gap, which forms an n-type barrier to surround the active areas. Lastly, the patterned sacrificial layer is stripped, and an anodization process is utilized to convert p-type bulk silicon into porous silicon. Then, an oxidation process is performed to oxidize the porous silicon to form a silicon dioxide isolation region for the active areas.

## Claims

### Claim 1

An isolation method for use in active areas of a semiconductor device, and the isolation method comprising
providing a substrate where the substrate is a p-type silicon substrate;
forming an oxide layer on the substrate;
forming a patterned sacrificial layer and an upper mask layer on the oxide layer and defining a gap between the patterned sacrificial layer and the upper mask layer where the upper mask layer is located over an isolation region of the substrate;
performing an n-type ion implantation process to implant n-type ions into the substrate through the gap to form an n-type barrier around the isolation region in the substrate;
removing the upper mask layer;
performing an anodization process to the isolation region to convert a bulk silicon portion of the isolation region into a porous silicon portion; and
oxidizing the porous silicon portion to form a silicon dioxide portion.

### Claim 2 (depends on 1)

The isolation method as claimed in claim 1, wherein the substrate has an n-MOS device, and after the step of oxidizing the porous silicon portion to form a silicon dioxide portion further comprises
performing a p-type ion implantation process to the isolation region of the n-MOS device; and
performing a heat treatment process, and removing the patterned sacrificial layer and the oxide layer.

### Claim 3 (depends on 1)

The isolation method as claimed in claim 1, wherein the substrate has a p-MOS device, and after the step of oxidizing the porous silicon portion to form a silicon dioxide portion further comprises
forming a protecting layer covering the isolation region of the p-MOS device; and
removing the protecting layer, the patterned sacrificial layer and the oxide layer after a p-type ion implantation process.

### Claim 4 (depends on 1)

The isolation method as claimed in claim 1, wherein the step of forming a patterned sacrificial layer and an upper mask layer on the oxide layer and defining a gap between the patterned sacrificial layer and the upper mask layer comprises
forming a first sacrificial layer on the substrate;
forming a first mask layer on the first sacrificial layer;
patterning the first mask layer and the first sacrificial layer to form respectively a patterned mask layer and the patterned sacrificial layer;
forming a second sacrificial layer covering the substrate and the patterned mask layer;
forming a second mask layer on the second sacrificial layer and partially etching the second mask layer to form the upper mask layer; and
etching the second sacrificial layer to define the gap between the patterned sacrificial layer and the upper mask layer.

### Claim 5 (depends on 1)

The isolation method as claimed in claim 1, wherein the step of removing the upper mask layer comprises
removing simultaneously the upper mask layer and the patterned mask layer; and
removing the second sacrificial layer to reveal the pad oxide layer over the isolation region.

### Claim 6 (depends on 4)

The isolation method as claimed in claim 4, wherein the upper mask layer and the patterned mask layer are nitride.

### Claim 7 (depends on 1)

The isolation method as claimed in claim 1, wherein the step of oxidizing the porous silicon portion to form a silicon dioxide portion uses a low-temperature wet-oxidization process.

### Claim 8 (depends on 1)

The isolation method as claimed in claim 1, wherein after the step of performing an n-type ion implantation process to implant n-type ions into the substrate through the gap to form an n-type barrier around the isolation region in the substrate further comprises
performing a heat treatment process to activate the implanted n-type ions in the substrate.

### Claim 9 (depends on 2)

The isolation method as claimed in claim 2, wherein the heat treatment process is a rapid thermal anneal process.

### Claim 10 (depends on 8)

The isolation method as claimed in claim 8, wherein the heat treatment process is a rapid thermal anneal process.

### Claim 11

An isolation method for use in active areas of a semiconductor device, and the isolation method comprising
providing a substrate where the substrate is a p-type silicon substrate;
forming an oxide layer on the substrate;
forming a patterned sacrificial layer and an upper mask layer on the oxide layer and defining a gap between the patterned sacrificial layer and the upper mask layer where the upper mask layer is located over an isolation region of the substrate;
performing an n-type ion implantation process to implant n-type ions into the substrate through the gap to form an n-type barrier around the isolation region in the substrate;
removing the upper mask layer;
forming a sidewall layer on a sidewall of the patterned sacrificial layer where the sidewall layer is located over the n-type barrier;
performing an anodization process to the isolation region to convert a bulk silicon portion of the isolation region into a porous silicon portion; and
oxidizing the porous silicon portion to form a silicon dioxide portion.

### Claim 12 (depends on 11)

The isolation method as claimed in claim 11, wherein the sidewall layer is formed by depositing a nitride layer on the patterned sacrificial layer and etching partially the nitride layer.

### Claim 13 (depends on 11)

The isolation method as claimed in claim 11, after the step of forming a sidewall layer on a sidewall of the patterned sacrificial layer further comprises removing a portion of the oxide layer over the isolation region.

### Claim 14 (depends on 11)

The isolation method as claimed in claim 11, after the step of performing an anodization process to the isolation region to convert a bulk silicon portion of the isolation region into a porous silicon portion further comprises
removing the sidewall layer.

### Claim 15 (depends on 14)

The isolation method as claimed in claim 14, wherein the substrate has an n-MOS device, and after the step of removing the sidewall layer further comprising
performing a p-type ion implantation process to the isolation region of the n-MOS device; and
performing a heat treatment process and removing the patterned sacrificial layer and the oxide layer.

### Claim 16 (depends on 14)

The isolation method as claimed in claim 14, wherein the substrate has a p-MOS device, and after the step of removing the sidewall layer further comprising
forming a protecting layer covering the isolation region of the p-MOS device; and
removing the protecting layer, the patterned sacrificial layer and the oxide layer after a p-type ion implantation process.

### Claim 17 (depends on 11)

The isolation method as claimed in claim 11, wherein the step of forming a patterned sacrificial layer and an upper mask layer on the oxide layer and defining a gap between the patterned sacrificial layer and the upper mask layer comprises
forming a first sacrificial layer on the substrate;
forming a first mask layer on the first sacrificial layer;
patterning the first mask layer and the first sacrificial layer to form respectively a patterned mask layer and the patterned sacrificial layer;
forming a second sacrificial layer covering the substrate and the patterned mask layer;
forming a second mask layer on the second sacrificial layer and partially etching the second mask layer to form the upper mask layer;
etching the second sacrificial layer to define the gap between the patterned sacrificial layer and the upper mask layer; and
removing the second sacrificial layer to reveal the pad oxide layer over the isolation region after the step of removing the upper mask layer.

### Claim 18 (depends on 17)

The isolation method as claimed in claim 17, wherein the upper mask layer and the patterned mask layer are nitride.

### Claim 19 (depends on 11)

The isolation method as claimed in claim 11, wherein the step of oxidizing the porous silicon portion to form a silicon dioxide portion uses a low-temperature wet-oxidization process.

### Claim 20 (depends on 11)

The isolation method as claimed in claim 11, wherein after the step of performing an n-type ion implantation process to implant n-type ions into the substrate through the gap to form an n-type barrier around the isolation region in the substrate further comprises
performing a heat treatment process to activate the implanted n-type ions in the substrate, where the heat treatment process is a rapid thermal anneal process.