# US 2009/0022958 A1 · Amorphous metal-metalloid alloy barrier layer for ic devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0022958 A1
- Document ID: US20090022958A1
- Status: Published application
- Kind: A1
- Application number: 11/779,894
- Filed: 2007-07-19
- Published: 2009-01-22
- Earliest claimed: 2007-07-19
- Inventors: John J. Plombon; Harsono S. Simka; Adrien R. Lavoie; Juan E. Dominguez
- Web page: https://patentgrep.com/patent/US20090022958A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10P 14/432: {using selective deposition}
- H10W 20/097: {by thermally treating}
- Y10T 428/24545: Containing metal or metal compound
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for fabricating an amorphous metal-metalloid alloy layer for use in an IC device comprises providing a substrate in a reactor that includes a dielectric layer having a trench, pulsing a metal precursor into the reactor to deposit within the trench, wherein the metal precursor is selected from the group consisting of CpTa(CO)4, PDMAT, TBTDET, TaCl5, Cp2Co, Co-amidinates, Cp2Ru, Ru-diketonates, and Ru(CO)4, purging the reactor after the metal precursor pulse, pulsing a metalloid precursor into the reactor to react with the metal precursor and form an amorphous metal-metalloid alloy layer, wherein the metalloid precursor is selected from the group consisting of BH3, BCl3, catechol borane, AlMe3, methylpyrrolidinealane, AICl3, SiH4, SiH2Cl2, SiCl4, tetraalkylsilanes, GeH4, GeH2Cl2, GeCl4, SnCl4, trialkylantimony, SbMe3, SbEt3, arsine, and trimethylarsine, purging the reactor after the metalloid precursor pulse, and annealing the amorphous metal-metalloid layer at a temperature between 50° C. and 700° C. for 5 to 1200 seconds.

## Claims

### Claim 1

A method comprising:
providing a substrate in a reactor;
pulsing a metal-containing precursor into the reactor to deposit on the substrate;
purging the reactor after the metal-containing precursor pulse;
pulsing a metalloid-containing precursor into the reactor to react with the metal-containing precursor and form an amorphous metal-metalloid alloy layer; and
purging the reactor after the metalloid-containing precursor pulse.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metal-containing precursor is selected from the group consisting of CpTa(CO)4, PDMAT, TBTDET, TaCl5, Cp2Co, Co-amidinates, Cp2Ru, Ru-diketonates, and Ru3(CO)12.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metalloid-containing precursor is selected from the group consisting of BH3, BCl3, catechol borane, AlMe3, methylpyrrolidinealane, AICl3, SiH4, SiH2Cl2, SiCl4, tetraalkylsilanes, GeH4, GeH2Cl2, GeCl4, SnCl4, trialkylantimony, SbMe3, SbEt3, arsine, and trimethylarsine.

### Claim 4 (depends on 1)

The method of claim 1, further comprising annealing the amorphous metal-metalloid alloy layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the annealing process occurs at a temperature between 50° C. and 700° C. for a time duration between 5 seconds and 1200 seconds.

### Claim 6 (depends on 1)

The method of claim 1, wherein the pulsing of the metal-containing precursor, the purging after the metal-containing precursor pulse, the pulsing of the metalloid-containing precursor, and the purging after the metalloid-containing precursor are repeated until the amorphous metal-metalloid alloy layer reaches a desired thickness.

### Claim 7 (depends on 6)

The method of claim 6, wherein the amount of metalloid-containing precursor pulsed into the reactor in successive pulses is varied to cause the amorphous metal-metalloid alloy layer to have a variable metalloid concentration across its thickness.

### Claim 8 (depends on 1)

The method of claim 1, wherein a sufficient amount of the metalloid-containing precursor is pulsed into the reactor to fabricate an amorphous metal-metalloid alloy layer having a metalloid concentration that is between around 0.1% and around 50%.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
depositing a metal seed layer on the amorphous metal-metalloid alloy layer using an ALD process; and
depositing a metal layer on the metal seed layer using a plating process.

### Claim 10 (depends on 9)

The method of claim 9, wherein the metal comprises copper.

### Claim 11

A method comprising:
providing a substrate in a reactor, wherein the substrate includes a dielectric layer having a trench;
pulsing a metal-containing precursor into the reactor to deposit within the trench, wherein the metal-containing precursor is selected from the group consisting of CpTa(CO)4, PDMAT, TBTDET, TaCl5, Cp2Co, Co-amidinates, Cp2Ru, Ru-diketonates, and Ru(CO)4;
purging the reactor after the metal-containing precursor pulse;
pulsing a metalloid-containing precursor into the reactor to react with the metal-containing precursor and form an amorphous metal-metalloid alloy layer within the trench, wherein the metalloid-containing precursor is selected from the group consisting of BH3, BCl3, catechol borane, AlMe3, methylpyrrolidinealane, AICl3, SiH4, SiH2Cl2, SiCl4, tetraalkylsilanes, GeH4, GeH2Cl2, GeCl4, SnCl4, trialkylantimony, SbMe3, SbEt3, arsine, and trimethylarsine;
purging the reactor after the metalloid-containing precursor pulse; and
annealing the amorphous metal-metalloid alloy layer at a temperature between 50° C. and 700° C. for a time duration between 5 seconds and 1200 seconds.

### Claim 12 (depends on 11)

The method of claim 11, wherein the pulsing of the metal-containing precursor, the purging after the metal-containing precursor pulse, the pulsing of the metalloid-containing precursor, and the purging after the metalloid-containing precursor are repeated until the amorphous metal-metalloid alloy layer reaches a desired thickness.

### Claim 13 (depends on 12)

The method of claim 12, wherein the amount of metalloid-containing precursor pulsed into the reactor in successive pulses is varied to cause the amorphous metal-metalloid alloy layer to have a variable metalloid concentration across its thickness.

### Claim 14 (depends on 11)

The method of claim 11, wherein a sufficient amount of the metalloid-containing precursor is pulsed into the reactor to fabricate an amorphous metal-metalloid alloy layer having a metalloid concentration that is between around 0.1% and around 50%.

### Claim 15

An apparatus comprising:
a substrate having a dielectric layer formed thereon and a trench etched into the dielectric layer;
an amorphous metal-metalloid alloy layer formed on a bottom surface and sidewalls of the trench; and
a copper layer formed on the amorphous metal-metalloid alloy layer within the trench.

### Claim 16 (depends on 15)

The apparatus of claim 15, wherein the substrate comprises a bulk silicon structure or a silicon-on-insulator structure.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the substrate further includes germanium, indium antimonide, lead telluride, indium arsenide, indium phosphide, gallium arsenide, gallium antimonide, or a Group III-V material.

### Claim 18 (depends on 15)

The apparatus of claim 15, wherein the amorphous metal-metalloid alloy layer comprises:
a metal selected from the group consisting of tantalum, titanium, ruthenium, cobalt, palladium, tungsten, and platinum; and
a metalloid selected from the group consisting of boron, aluminum, silicon, germanium, arsenic, antimony, tellurium, polonium, carbon, nitrogen, and iodine.

### Claim 19 (depends on 15)

The apparatus of claim 15, wherein the amorphous metal-metalloid alloy layer has a thickness between around 1 nm and around 10 nm.

### Claim 20 (depends on 15)

The apparatus of claim 15, wherein the copper layer comprises a copper seed layer and a copper layer formed on the copper seed layer.