# US 2009/0022614 A1 · Method for Producing Sputtering Target Material for Ni-W Based Interlayer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0022614 A1
- Document ID: US20090022614A1
- Status: Published application
- Kind: A1
- Application number: 12/173,337
- Filed: 2008-07-15
- Published: 2009-01-22
- Earliest claimed: 2007-07-18
- Assignees: Sanyo Special Steel Co., Ltd.
- Inventors: Toshiyuki Sawada; Akihiko Yanagitani
- Web page: https://patentgrep.com/patent/US20090022614A1

## CPC

- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- C22C 1/0433: {Nickel- or cobalt-based alloys}
- C22C 19/05: with chromium
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

There is provided a method for producing sputtering target materials which are used for a Ni—W based interlayer in a perpendicular magnetic recording medium. In this producing method, a Ni—W based alloy powder is prepared as a raw material powder. The alloy powder comprises 5 to 20 at % of W and the balance Ni and unavoidable impurities and is produced by gas atomization. The raw material powder is consolidated at a temperature ranging from 900 to 1150° C. This producing method makes it possible to significantly restrain expansion of the powder-filled billet in the consolidation step, thus efficiently producing Ni—W based sputtering target materials with stable qualities.

## Claims

### Claim 1

A method for producing a sputtering target material for a Ni—W based interlayer, comprising the steps of:
preparing a Ni—W based alloy powder as a raw material powder, the alloy powder comprising 5 to 20 at % of W and the balance Ni and unavoidable impurities and being produced by gas atomization; and
consolidating the raw material powder at a temperature ranging from 900 to 1150° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the temperature in the consolidation step ranges from 900 to 1050° C.