# US 2009/0020453 A1 · Process oil, process for production of deasphalted oil, process for production of extract, and process for production of process oil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0020453 A1
- Document ID: US20090020453A1
- Status: Published application
- Kind: A1
- Application number: 11/913,124
- Filed: 2006-05-29
- Published: 2009-01-22
- Earliest claimed: 2005-05-31
- Assignees: Idemitsu Kosan Co., Ltd.
- Inventors: Meishi Tanaka; Masashi Nakamura; Kazuhiro Teshima; Akihito Abe; Masami Takasaki
- Web page: https://patentgrep.com/patent/US20090020453A1

## CPC

- C08K 5/01: Hydrocarbons {(C08K5/0091 takes precedence)}
- C10G 21/003: {Solvent de-asphalting}
- C10G 21/14: Hydrocarbons
- C10M 101/02: Petroleum fractions
- C10M 177/00: Special methods of preparation of lubricating compositions; Chemical modification by after-treatment of components or of the whole of a lubricating composition, not covered by other classes
- C10G 2300/1033: Oil well production fluids
- C10G 2300/1062: Lubricating oils
- C10G 2300/1077: Vacuum residues
- C10G 2300/206: Asphaltenes
- C10G 2300/30: Physical properties of feedstocks or products
- C10G 2300/302: Viscosity
- C10G 2300/304: Pour point, cloud point, cold flow properties
- C10G 2300/4025: Yield
- C10G 2300/44: Solvents
- C10M 2203/1085: used as base material
- C10N 2020/01: {Physico-chemical properties}
- C10N 2020/011: {Cloud point}
- C10N 2020/02: Viscosity; Viscosity index
- C10N 2020/067: {Unsaturated Compounds}
- C10N 2030/02: Pour-point; Viscosity index
- C10N 2030/40: {Low content or no content compositions}
- C10N 2070/00: Specific manufacturing methods for lubricant compositions
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

The present invention is related to a process oil using as a raw material a deasphalted oil obtained by deasphalting a vacuum residual oil of a crude oil and a manufacturing method of the process oil, the process oil having properties of: (a) a polycyclic aromatics (PCA) content of less than 3 mass %; (b) a viscosity (100° C.) of 40 to 70 mm2/s; (c) an aniline point of 85 to 100° C.; (d) a flash point of 250° C. or higher; (e) an aromatic hydrocarbon content of 40 to 55 mass %; and (f) a polar substance content of 10 to 15 mass %. The present invention is also related to a process oil and a manufacturing method of the process oil, the process oil obtained by mixing: an extract obtained by deasphalting and solvent-extracting a vacuum residual oil of a crude oil; and a lubricant base oil having a polycyclic aromatics (PCA) content of less than 3 mass %, and having properties of: (a) a polycyclic aromatics (PCA) content of less than 3 mass %; (i) a viscosity (100° C.) of 30 to 80 mm2/s; (j) an aniline point of 90° C. or lower; (k) a flash point of 240° C. or higher; (l) a benzo(a)pyrene content of 1 mass ppm or less; (m) a specified aromatic compound content of 10 mass ppm or less; and (n) a polar substance content of 10 to 30 mass %.

## Claims

### Claim 1

A process oil using as a raw material a deasphalted oil obtained by deasphalting a vacuum residual oil of a crude oil, the process oil comprising properties of:
(a) a polycyclic aromatics (PCA) content of less than 3 mass %;
(b) a viscosity (100° C.) of 40 to 70 mm2/s;
(c) an aniline point of 85 to 100° C.;
(d) a flash point of 250° C. or higher;
(e) an aromatic hydrocarbon content of 40 to 55 mass %; and
(f) a polar substance content of 10 to 15 mass %.

### Claim 2 (depends on 1)

The process oil according to claim 1, further comprising a property of:
(g) a pour point of 40° C. or lower.

### Claim 3 (depends on 1)

The process oil according to claim 1, wherein the process oil shows an ASTM color phase of 8.0 or lower when being diluted with a toluene of sixty times as large volume as the process oil.

### Claim 4 (depends on 1)

The process oil according to claim 1, further comprising a property of:
(h) an aniline point of 85 to 95° C.

### Claim 5

A process oil obtained by mixing: an extract obtained by deasphalting and solvent-extracting a vacuum residual oil of a crude oil; and a lubricant base oil having a polycyclic aromatics (PCA) content of less than 3 mass %, the process oil comprising properties of:
(a) a polycyclic aromatics (PCA) content of less than 3 mass %;
(i) a viscosity (100° C.) of 30 to 80 mm2/s;
(j) an aniline point of 90° C. or lower;
(k) a flash point of 240° C. or higher;
(l) a benzo(a)pyrene content of 1 mass ppm or less;
(m) a specified aromatic compound content of 10 mass ppm or lower; and
(n) a polar substance content of 10 to 30 mass %.

### Claim 6 (depends on 5)

The process oil according to claim 5, further comprising a property of:
(o) an aniline point of 60 to 90° C.

### Claim 7

A manufacturing method of a process oil, comprising:
a deasphalting step for deasphalting a vacuum residual oil of a crude oil to obtain a deasphalted oil; and
a solvent-extraction step for solvent-extracting the deasphalted oil to obtain an extract with a yield of 50 mass % or higher of the deasphalted oil, the extract being provided as the process oil.

### Claim 8

A manufacturing method of a process oil, comprising:
a deasphalting step for deasphalting a vacuum residual oil of a crude oil to obtain a deasphalted oil; and
a solvent-extraction step for solvent-extracting the deasphalted oil to obtain an extract; wherein
the extract obtained in the solvent-extraction step and at least one member selected from the group consisting of the deasphalted oil obtained in the deasphalting step and a mineral oil having a polycyclic aromatics (PCA) content of less than 3 mass % are mixed to obtain a mixed oil, the mixed oil being provided as the process oil.

### Claim 9

A manufacturing method of a process oil, comprising:
a deasphalting step for deasphalting a vacuum residual oil of a crude oil to obtain a deasphalted oil;
a dewaxing step for dewaxing the deasphalted oil to obtain a dewaxed oil; and
a solvent-extraction step for solvent-extracting the dewaxed oil to obtain an extract with a yield of 50 mass % or higher of the deasphalted oil, the extract being provided as the process oil.

### Claim 10

A manufacturing method of a process oil, comprising:
a deasphalting step for deasphalting a vacuum residual oil of a crude oil to obtain a deasphalted oil;
a dewaxing step for dewaxing the deasphalted oil to obtain a dewaxed oil; and
a solvent-extraction step for solvent-extracting the dewaxed oil to obtain an extract, wherein
the extract obtained in the solvent-extraction step and at least one member selected from the group consisting of the dewaxed oil obtained in the dewaxing step and a mineral oil having a polycyclic aromatics (PCA) content of less than 3 mass % are mixed to obtain a mixed oil, the mixed oil being provided as the process oil.

### Claim 11 (depends on 8)

The manufacturing method according to claim 8, wherein a content of the extract in the mixed oil is in the range from 40 mass % to below 80 mass %.

### Claim 12 (depends on 7)

The manufacturing method according to claim 7, wherein
a yield of the deasphalted oil obtained in the deasphalting step is 30 mass % or higher of the vacuum residual oil, and
a viscosity (100° C.) of the deasphalted oil is 30 to 50 mm2/s.

### Claim 13 (depends on 9)

The manufacturing method according to claim 9, wherein a pour point of the dewaxed oil obtained in the dewaxing step is 0 to 25° C., and a yield of the dewaxed oil is 90 mass % or higher of the deasphalted oil.

### Claim 14 (depends on 7)

The manufacturing method according to claim 7, wherein an extraction temperature in the solvent-extraction step is 80 to 150° C., and a solvent ratio is 2.0 to 12.0.

### Claim 15

A manufacturing method of a deasphalted oil using as a raw material a vacuum residual oil of a crude oil, the deasphalted oil having properties of (a), (l) and (m) below, the method comprising:
deasphalting the vacuum residual oil using as a solvent a propane or a mixed solvent of a butane and a propane under conditions of: a solvent ratio of 4.5 to 6; a column top temperature of 85 to 100° C.; and a yield for the deasphalted oil of 30 to 40 vol %, the properties being:
(a) a polycyclic aromatics (PCA) content of less than 3 mass %;
(l) a benzo(a)pyrene content of 1 mass ppm or less; and
(m) a specified aromatic hydrocarbon content of 10 mass ppm or less.

### Claim 16

A manufacturing method of an extract using as a raw material a deasphalted oil obtained by deasphalting a vacuum residual oil of a crude oil, the extract having properties of (l) and (m) below, the method comprising:
solvent-extracting the deasphalted oil under conditions of: an extraction temperature of 80 to 150° C.; and a solvent ratio of 2.0 to 15.0, the properties being:
(l) a benzo(a)pyrene content of 1 mass ppm or less; and
(m) a specified aromatic hydrocarbon content of 10 mass ppm or less.

### Claim 17

A manufacturing method of a process oil, comprising:
a deasphalting step for deasphalting a vacuum residual oil of a crude oil to obtain a deasphalted oil; and
a solvent-extraction step for solvent-extracting the deasphalted oil to obtain an extract, wherein
the extract obtained in the solvent-extraction step and a lubricant base oil having a polycyclic aromatics (PCA) content of less than 3 mass % are mixed to obtain a mixed oil, the mixed oil being provided as the process oil.

### Claim 18 (depends on 17)

The manufacturing method according to claim 17, wherein the lubricant base oil has properties of:
(p) a viscosity (100° C.) of 5 to 40 mm2/s;
(q) an aniline point of 75 to 120° C.;
(r) a flash point of 200° C. or higher;
(l) a benzo(a)pyrene content of 1 mass ppm or less; and
(m) a specified aromatic compound content of 10 mass ppm or less.

### Claim 19 (depends on 17)

The manufacturing method according to claim 17, wherein a volume mixing ratio of the extract and the lubricant base oil is 95/5 to 60/40.

### Claim 20 (depends on 10)

The manufacturing method according to claim 10, wherein a content of the extract in the mixed oil is in the range from 40 mass % to below 80 mass %.

### Claim 21 (depends on 8)

The manufacturing method according to claim 8, wherein
a yield of the deasphalted oil obtained in the deasphalting step is 30 mass % or higher of the vacuum residual oil, and
a viscosity (100° C.) of the deasphalted oil is 30 to 50 mm2/s.

### Claim 22 (depends on 9)

The manufacturing method according to claim 9, wherein a yield of the deasphalted oil obtained in the deasphalting step is 30 mass % or higher of the vacuum residual oil, and
a viscosity (100° C.) of the deasphalted oil is 30 to 50 mm2/s.

### Claim 23 (depends on 10)

The manufacturing method according to claim 10, wherein
a yield of the deasphalted oil obtained in the deasphalting step is 30 mass % or higher of the vacuum residual oil, and
a viscosity (100° C.) of the deasphalted oil is 30 to 50 mm2/s.

### Claim 24 (depends on 10)

The manufacturing method according to claim 10, wherein a pour point of the dewaxed oil obtained in the dewaxing step is 0 to 25° C., and a yield of the dewaxed oil is 90 mass % or higher of the deasphalted oil.

### Claim 25 (depends on 8)

The manufacturing method according to claim 8, wherein an extraction temperature in the solvent-extraction step is 80 to 150° C., and a solvent ratio is 2.0 to 12.0.

### Claim 26 (depends on 9)

The manufacturing method according to claim 9, wherein an extraction temperature in the solvent-extraction step is 80 to 150° C., and a solvent ratio is 2.0 to 12.0.

### Claim 27 (depends on 10)

The manufacturing method according to claim 10, wherein an extraction temperature in the solvent-extraction step is 80 to 150° C., and a solvent ratio is 2.0 to 12.0.