# US 2009/0020225 A1 · Autoadhesive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0020225 A1
- Document ID: US20090020225A1
- Status: Published application
- Kind: A1
- Application number: 12/162,433
- Filed: 2007-01-23
- Published: 2009-01-22
- Earliest claimed: 2006-01-30
- Assignees: BASF SE
- Inventors: Dirk Wulff; Axel Weiss; Jose Maria Torres Llosa; Christofer Arisandy
- Web page: https://patentgrep.com/patent/US20090020225A1

## CPC

- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- C08L 2308/00: Chemical blending or stepwise polymerisation process with the same catalyst
- C08L 2666/02: Organic macromolecular compounds, natural resins, waxes or and bituminous materials
- Y10T 428/31794: Of cross-linked polyester
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The use of a composition of low or no tack at 20° C. as an adhesive that can be adhered to itself (referred to below for short as an autoadhesive).

## Claims

### Claim 1

The method of using a composition of low or no tack at 20° C. as an adhesive that can be adhered to itself (referred to below for short as an autoadhesive).

### Claim 2 (depends on 1)

The method according to claim 1, wherein a polyethylene substrate coated with the composition has an adhesion to steel at 20° C. of less than 0.5 N/2.5 cm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the composition comprises an aqueous polymer dispersion as binder.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the dispersed polymer is composed of at least 60% by weight of principal monomers selected from C1 to C20 alkyl (meth)acrylates, vinyl esters of carboxylic acids comprising up to 20 C atoms, vinylaromatics having up to 20 C atoms, ethylenically unsaturated nitrites, vinyl halides, vinyl ethers of alcohols comprising 1 to 10 C atoms, aliphatic hydrocarbons having 2 to 8 C atoms and one or two double bonds, or mixtures of these monomers.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the polymer is composed of more than 60% by weight of C1 to C20 alkyl (meth)acrylates.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the glass transition temperature of all monomers of which the polymer is composed is 50 to +10° C. as calculated by the method of Fox.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the dispersed polymer is obtainable by multistage emulsion polymerization.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the polymerization takes place in at least two temporally successive stages, the individual stages differing in the glass transition temperature (Tg) of the monomers polymerized in that stage, as calculated by the method of Fox (and also referred to for short as stage Tg), and the Tg of the last stage being greater than 0° C.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the Tg of the last stage is at least 5° C. higher than the Tg of the preceding stage.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the Tg of the stages increases from the first to the last stage.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the polymerization takes place in two stages, 60% to 99% by weight of the monomers being polymerized in a first stage and the glass transition temperature of the monomers of this stage, as calculated by the method of Fox, being from −50 to +5° C., and 1% to 40% by weight of the monomers being polymerized in a second stage, the glass transition temperature of the monomers of this stage, as calculated by the method of Fox, being 20 to 125° C., and the glass transition temperature of the monomers of the 2nd stage being at least 5° higher than that of the first stage.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the polymerization takes place in at least three stages, the weight fraction of the stages with a Tg greater than 0° C. amounting in total to 5% to 40% by weight.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the polymerization takes place in three stages, the monomer amounts and Tgs being as follows:
1st stage:
50% to 90% by weight,
Tg (° C.):
−50 to +20
2nd stage:
2% to 15% by weight,
Tg (° C.):
−20 to +30
3rd stage:
2% to 15% by weight
Tg (° C.):
0 to +125
and the Tg of the 3rd stage is at least 5° higher than that of the 2nd stage, and that of the 2nd stage is at least 5° higher than that of the 1st stage.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the polymerization takes place in four stages, the monomer amounts and Tgs being as follows:
Claim 1st stage:
50% to 80% by weight,
Tg (° C.)
−50 to +20
2nd stage:
2% to 15% by weight
Tg (° C.)
−20 to +30
3rd stage:
2% to 15% by weight
Tg (° C.)
0 to 60
4th stage:
2% to 15% by weight
Tg (° C.)
20 to 125
and the Tg of the 4th stage being at least 5° higher than that of the 3rd stage, and that of the 3rd stage being at least 5° higher than that of the 2nd stage, and that of the 2nd stage being at least 5° higher than that of the 1st stage.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the polymerization of the monomers of the individual stages takes place during or immediately after the addition of the monomers to the polymerization mixture.

### Claim 16

The method of the composition as an adhesive for the hot or cold sealing of packaging.

### Claim 17 (depends on 1)

A method of joining two substrates, which comprises
coating the two substrates at the locations to be bonded with a composition according to claim 1 and
contacting the two substrates under pressure if appropriate,
the temperature in the coated composition being less than 40° C. (cold sealing).

### Claim 18 (depends on 1)

A double-sidedly coated support, wherein the support on one side (referred to below as the front face) has an outer layer of the composition according to claim 1 and on the other side (referred to below as the back face) has an outer layer of a release coating.

### Claim 19 (depends on 18)

The method of using the support according to claim 18 for producing packaging.

### Claim 20

A polymer of low or no tack at 20° C. which is obtainable by multistage emulsion polymerization, with a glass transition temperature of all monomers of which the polymer is composed, calculated by the method of Fox, of −50 to +10° C., wherein the polymerization takes place in at least two temporally successive stages, the individual stages differing in the glass transition temperature (Tg) of the monomers, as calculated by the method of Fox, and the Tg of the last stage being at least 0° C.