# US 2009/0014623 A1 · Electrophoretic Casting

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0014623 A1
- Document ID: US20090014623A1
- Status: Published application
- Kind: A1
- Application number: 10/585,564
- Filed: 2005-01-07
- Published: 2009-01-15
- Earliest claimed: 2004-01-09
- Inventors: Douglas M. Matson; Rakesh Venkatesh; John MacChesney; Thomas Stockert
- Web page: https://patentgrep.com/patent/US20090014623A1

## CPC

- B81C 99/0095: {Aspects relating to the manufacture of substrate-free structures, not covered by groups B81C99/008 - B81C99/009}
- B81C 99/009: {Manufacturing the stamps or the moulds}
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)

## Abstract

Methods for electrophoretic deposition of molds for casting processes are provided. Electrophoresis is used to deposit very fine particles on a template from a slurry comprising an ionic dispersion agent. The resulting green shell is then dried and sintered to form a mold.

## Claims

### Claim 1

A method of forming a shell on a template, comprising:
immersing the template in a slurry, the slurry comprising
a plurality of colloidal particles; and
a sufficient quantity of salt to impart an effective charge to the colloidal particles;
applying a voltage to the template, thereby causing the charged colloidal particles to be deposited on the template to form a green shell; and
sintering the green shell to form a solidified shell having greater mechanical integrity than the green shell.

### Claim 2 (depends on 1)

The method of claim 1, wherein the template comprises a conductive material.

### Claim 3 (depends on 1)

The method of claim 1, wherein the template comprises a conductive coating.

### Claim 4 (depends on 3)

The method of claim 3, wherein the conductive coating is a sputtered coating.

### Claim 5 (depends on 1)

The method of claim 1, wherein the slurry is nonaqueous.

### Claim 6 (depends on 5)

The method of claim 5, wherein the slurry has a dielectric breakdown voltage greater than about 50 VDC.

### Claim 7 (depends on 5)

The method of claim 5, wherein the slurry comprises a material selected from the group consisting of butanol, methanol, ethanol, and propanol.

### Claim 8 (depends on 1)

The method of claim 1, wherein the colloidal particles comprise a material selected from the group consisting of silica, glass, alumina, silicon nitride, silicon carbide, yttria, zirconia, and oxides and nitrides of aluminum and titanium.

### Claim 9 (depends on 1)

The method of claim 1, wherein the colloidal particles have an average particle size of less than 75 μm.

### Claim 10 (depends on 1)

The method of claim 1, wherein the colloidal particles have an average particle size of less than 40 μm.

### Claim 11 (depends on 1)

The method of claim 1, wherein the colloidal particles have an average particle size of less than 10 μm.

### Claim 12 (depends on 1)

The method of claim 1, wherein the colloidal particles have an average particle size of less than 1 μm.

### Claim 13 (depends on 1)

The method of claim 1, wherein the colloidal particles have an average particle size of less than 100 nm.

### Claim 14 (depends on 1)

The method of claim 1, wherein the colloidal particles have an average particle size of less than 10 nm.

### Claim 15 (depends on 1)

The method of claim 1, wherein the salt is selected from the group consisting of sodium chloride, potassium chloride, rubidium chloride, cesium chloride, zinc chloride, and potassium carbonate.

### Claim 16 (depends on 1)

The method of claim 1, wherein the salt is a metal salt.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal salt is a halide or a carbonate.

### Claim 18 (depends on 1)

The method of claim 1, wherein the salt is an alkyl halide.

### Claim 19 (depends on 1)

The method of claim 1, wherein the salt is present in a concentration of 5% by weight or less.

### Claim 20 (depends on 1)

The method of claim 1, wherein the salt is present at a concentration in the slurry that is at or below its solubility limit.

### Claim 21 (depends on 1)

The method of claim 1, wherein the applied voltage is about 100 volts.

### Claim 22 (depends on 21)

The method of claim 21, wherein the applied voltage produces a current of about 3-5 mA.

### Claim 23 (depends on 1)

The method of claim 1, wherein the green shell has a pore fraction not greater than 40% by volume.

### Claim 24 (depends on 1)

The method of claim 1, wherein the green shell has a pore fraction not greater than 30% by volume.

### Claim 25 (depends on 1)

The method of claim 1, further comprising drying the green shell prior to sintering.

### Claim 26 (depends on 1)

The method of claim 1, further comprising:
after immersing the template and applying a voltage, immersing the template in a second slurry comprising a second plurality of colloidal particles; and
applying a second voltage to the template to cause the second plurality of colloidal particles to be deposited on the green shell to increase its thickness.

### Claim 27

A method of producing a desired article, comprising:
providing a template having a predetermined shape;
depositing an investment mold on the template, wherein depositing comprises:
immersing the template in a slurry, the slurry comprising a plurality of colloidal particles and a sufficient quantity of salt to impart an effective charge to the colloidal particles;
applying a voltage to the template, thereby causing the charged colloidal particles to be deposited on the template to form a green shell; and
sintering the green shell to form the investment mold;
removing the template; and
casting the desired article in the investment mold.

### Claim 28 (depends on 27)

The method of claim 27, wherein the template comprises a conductive material.

### Claim 29 (depends on 27)

The method of claim 27, wherein the template comprises a conductive coating.

### Claim 30 (depends on 29)

The method of claim 29, wherein the conductive coating is a sputtered coating.

### Claim 31 (depends on 27)

The method of claim 27, wherein the slurry is nonaqueous.

### Claim 32 (depends on 31)

The method of claim 31, wherein the slurry has a dielectric breakdown voltage greater than about 50 VDC.

### Claim 33 (depends on 31)

The method of claim 31, wherein the slurry comprises a material selected from the group consisting of butanol, methanol, ethanol, and propanol.

### Claim 34 (depends on 27)

The method of claim 27, wherein the colloidal particles comprise a material selected from the group consisting of silica, glass, alumina, silicon nitride, silicon carbide, yttria, zirconia, and oxides and nitrides of aluminum and titanium.

### Claim 35 (depends on 27)

The method of claim 27, wherein the colloidal particles have an average particle size of less than 75 μm.

### Claim 36 (depends on 27)

The method of claim 27, wherein the colloidal particles have an average particle size of less than 40 μm.

### Claim 37 (depends on 27)

The method of claim 27, wherein the colloidal particles have an average particle size of less than 10 μm.

### Claim 38 (depends on 27)

The method of claim 27, wherein the colloidal particles have an average particle size of less than 1 μm.

### Claim 39 (depends on 27)

The method of claim 27, wherein the colloidal particles have an average particle size of less than 100 nm.

### Claim 40 (depends on 27)

The method of claim 27, wherein the colloidal particles have an average particle size of less than 10 nm.

### Claim 41 (depends on 27)

The method of claim 27, wherein the salt is selected from the group consisting of sodium chloride, potassium chloride, rubidium chloride, cesium chloride, zinc chloride, and potassium carbonate.

### Claim 42 (depends on 27)

The method of claim 27, wherein the salt is a metal salt.

### Claim 43 (depends on 42)

The method of claim 42, wherein the metal salt is a halide or a carbonate.

### Claim 44 (depends on 27)

The method of claim 27, wherein the salt is an alkyl halide.

### Claim 45 (depends on 27)

The method of claim 27, wherein the salt is present in a concentration of 5% by weight or less.

### Claim 46 (depends on 27)

The method of claim 27, wherein the salt is present at a concentration in the slurry that is at or below its solubility limit.

### Claim 47 (depends on 27)

The method of claim 27, wherein the applied voltage is about 100 volts.

### Claim 48 (depends on 47)

The method of claim 47, wherein the applied voltage produces a current of about 3-5 mA.

### Claim 49 (depends on 27)

The method of claim 27, wherein the green shell has a pore fraction not greater than 40% by volume.

### Claim 50 (depends on 27)

The method of claim 27, wherein the green shell has a pore fraction not greater than 30% by volume.

### Claim 51 (depends on 27)

The method of claim 27, further comprising drying the green shell prior to sintering.

### Claim 52 (depends on 27)

The method of claim 27, further comprising:
after immersing the template and applying a voltage, immersing the template in a second slurry comprising a second plurality of colloidal particles; and
applying a second voltage to the template to cause the second plurality of colloidal particles to be deposited on the green shell to increase its thickness.

### Claim 53

A method of producing a desired article by investment casting, comprising:
providing a master template having a predetermined shape;
using the master template to produce a transfer mold having a shape complementary to the master template, wherein the transfer mold comprises a flexible material;
molding a sacrificial template in the transfer mold, the sacrificial template comprising a material that can be melted, burned, or leached;
depositing an investment mold on the sacrificial template, wherein depositing comprises:
immersing the template in a slurry, the slurry comprising a plurality of colloidal particles and a sufficient quantity of salt to impart an effective charge to the colloidal particles;
applying a voltage to the template, thereby causing the charged colloidal particles to be deposited on the template to form a green shell; and
sintering the green shell to form the investment mold;
removing the sacrificial template by melting, burning, or leaching, without damaging the investment mold; and
casting the desired article in the investment mold.

### Claim 54

A casting mold, comprising:
a hollow shell comprising a plurality of partially or fully sintered particles and a measurable quantity of salt residue.

### Claim 55 (depends on 54)

The casting mold of claim 54, wherein the particles comprise a ceramic material.

### Claim 56 (depends on 54)

The casting mold of claim 54, wherein the partially or fully sintered particles have an average particle size of less than about 75 μm.

### Claim 57 (depends on 54)

The casting mold of claim 54, wherein the partially or fully sintered particles have an average particle size of less than about 40 μm.

### Claim 58 (depends on 54)

The casting mold of claim 54, wherein the partially or fully sintered particles have an average particle size of less than about 10 μm.

### Claim 59 (depends on 54)

The casting mold of claim 54, wherein the partially or fully sintered particles have an average particle size of less than about 1 μm.

### Claim 60 (depends on 54)

The casting mold of claim 54, wherein the partially or fully sintered particles have an average particle size of less than about 100 nm.

### Claim 61 (depends on 54)

The casting mold of claim 54, wherein the partially or fully sintered particles have an average particle size of less than about 10 nm.

### Claim 62 (depends on 54)

The casting mold of claim 54, wherein the salt residue is selected from the group consisting of sodium chloride, potassium chloride, rubidium chloride, cesium chloride, zinc chloride, and potassium carbonate.

### Claim 63

A casting mold, produced by:
immersing at least a first portion of a template in a first slurry, the first slurry comprising
a plurality of colloidal particles; and
a sufficient quantity of salt to impart an effective charge to the colloidal particles;
applying a voltage to the template, thereby causing the charged colloidal particles to be deposited on the template to form a green shell about at least the first portion of the template; and
sintering the green shell to form the casting mold having greater mechanical integrity than the green shell.

### Claim 64 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles comprise a material selected from the group consisting of silica, glass, alumina, silicon nitride, silicon carbide, yttria, zirconia, and oxides and nitrides of aluminum and titanium.

### Claim 65 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles have an average particle size of less than about 75 μm.

### Claim 66 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles have an average particle size of less than about 40 μm.

### Claim 67 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles have an average particle size of less than about 10 μm.

### Claim 68 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles have an average particle size of less than about 1 μm.

### Claim 69 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles have an average particle size of less than about 100 nm.

### Claim 70 (depends on 63)

The casting mold of claim 63, wherein the colloidal particles have an average particle size of less than about 10 nm.

### Claim 71 (depends on 63)

The casting mold of claim 63, wherein the salt is selected from the group consisting of sodium chloride, potassium chloride, rubidium chloride, cesium chloride, zinc chloride, and potassium carbonate.

### Claim 72 (depends on 63)

The casting mold of claim 63, wherein the salt is a metal salt.

### Claim 73 (depends on 72)

The casting mold of claim 72, wherein the salt is a halide or a carbonate.

### Claim 74 (depends on 63)

The casting mold of claim 63, wherein the salt is an alkyl halide.

### Claim 75 (depends on 63)

The casting mold of claim 63, wherein the green shell has a pore fraction not greater than 40% by volume.

### Claim 76 (depends on 63)

The casting mold of claim 63, wherein the green shell has a pore fraction not greater than 30% by volume.

### Claim 77 (depends on 63)

The casting mold of claim 63, wherein the green shell comprises a plurality of layers of particles, and wherein adjacent layers of particles differ in size distribution or in composition.

### Claim 78 (depends on 63)

The casting mold of claim 63, further produced by, before sintering the green shell:
immersing the template in a second slurry comprising a plurality of colloidal particles; and
allowing the slurry to dry, thereby causing the colloidal particles to be deposited on a second portion of the template and the green shell to form a second green shell.