# US 2009/0014103 A1 · Aluminum alloy sheet for lithographic printing plate and method of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0014103 A1
- Document ID: US20090014103A1
- Status: Published application
- Kind: A1
- Application number: 12/157,869
- Filed: 2008-06-13
- Published: 2009-01-15
- Earliest claimed: 2007-07-10
- Assignees: FUJIFILM Corporation; Sumitomo Light Metal Industries, Ltd.
- Inventors: Akio Uesugi; Atsushi Matsuura; Hiroshi Ougi; Atsushi Hibino
- Web page: https://patentgrep.com/patent/US20090014103A1

## CPC

- C22F 1/04: of aluminium or alloys based thereon
- B41N 1/083: {made of aluminium or aluminium alloys or having such surface layers (B41N1/086 takes precedence)}
- C22C 21/00: Alloys based on aluminium
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B41N: PRINTING PLATES OR FOILS (photosensitive material G03); MATERIALS FOR SURFACES USED IN PRINTING MACHINES FOR PRINTING, INKING, DAMPING, OR THE LIKE; PREPARING SUCH SURFACES FOR USE AND CONSERVING THEM
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An aluminum alloy sheet for a lithographic printing plate is obtained by homogenizing an ingot of an aluminum alloy at 500 to 610° C. for one hour or more, the aluminum alloy containing 0.03 to 0.15% of Si, 0.2 to 0.6% of Fe, 0.005 to 0.05% of Ti, and 2 to 30 ppm of Pb, with the balance being aluminum and unavoidable impurities, subjecting the homogenized product to rough hot rolling, a start temperature of the rough hot rolling being 430 to 500° C. and a finish temperature of the rough hot rolling being 400° C. or more, holding the product subjected to rough hot rolling for 60 to 300 seconds after the completion of the rough hot rolling to recrystallize the surface of the product, and subjecting the resulting product to finish hot rolling that is finished at 320 to 370° C. The aluminum alloy sheet has an average recrystallized grain diameter of 50 μm or less in a surface area in a direction perpendicular to a rolling direction, and has a Pb concentration 100 to 400 times an average Pb concentration in a surface area up to a depth of 0.2 μm from the surface of the aluminum alloy sheet.

## Claims

### Claim 1

An aluminum alloy sheet for a lithographic printing plate comprising 0.03 to 0.15% (mass %; hereinafter the same) of Si, 0.2 to 0.6% of Fe, 0.005 to 0.05% of Ti, and 2 to 30 ppm of Pb, with the balance being aluminum and unavoidable impurities, the aluminum alloy sheet having an average recrystallized grain diameter of 50 μm or less in a surface area in a direction perpendicular to a rolling direction, and having a Pb concentration 100 to 400 times an average Pb concentration in a surface area up to a depth of 0.2 μm from the surface of the aluminum alloy sheet.

### Claim 2 (depends on 1)

The aluminum alloy sheet according to claim 1, further comprising 0.05% or less of Cu.

### Claim 3 (depends on 1)

The aluminum alloy sheet according to claim 1, further comprising less than 0.05% of Mg.

### Claim 4 (depends on 1)

The aluminum alloy sheet according to claim 1, wherein the number of precipitates having a particle diameter (circle equivalent diameter; hereinafter the same) of 1 to 10 μm and the number of precipitates having a particle diameter of more than 10 μm distributed in a matrix are 4000 to 10,000 per square millimeter (mm2) and 100 or less per square millimeter (mm2) respectively.

### Claim 5 (depends on 1)

A method of producing an aluminum alloy sheet for a lithographic printing plate comprising homogenizing an ingot of the aluminum alloy according to claim 1 at 500 to 610° C. for one hour or more, subjecting the homogenized product to rough hot rolling, a start temperature of the rough hot rolling being 430 to 500° C. and a finish temperature of the rough hot rolling being 400° C. or more, holding the product subjected to the rough hot rolling for 60 to 300 seconds after completion of the rough hot rolling to recrystallize the surface of the product, subjecting the resulting product to finish hot rolling that is finished at 330° C. or more, and cold-rolling the resulting product at a reduction ratio of 80% or more.

### Claim 6 (depends on 2)

The aluminum alloy sheet according to claim 2, further comprising less than 0.05% of Mg.

### Claim 7 (depends on 2)

The aluminum alloy sheet according to claim 2, wherein the number of precipitates having a particle diameter of 1 to 10 μm and the number of precipitates having a particle diameter of more than 10 μm distributed in a matrix are 4000 to 10,000 per square millimeter (mm2) and 100 or less per square millimeter (mm2), respectively.

### Claim 8 (depends on 3)

The aluminum alloy sheet according to claim 3, wherein the number of precipitates having a particle diameter of 1 to 10 μm and the number of precipitates having a particle diameter of more than 10 μm distributed in a matrix are 4000 to 10,000 per square millimeter (mm2) and 100 or less per square millimeter (mm2), respectively.

### Claim 9 (depends on 6)

The aluminum alloy sheet according to claim 6, wherein the number of precipitates having a particle diameter of 1 to 10 μm and the number of precipitates having a particle diameter of more than 10 μm distributed in a matrix are 4000 to 10,000 per square millimeter (mm2) and 100 or less per square millimeter (mm2), respectively.

### Claim 10

A method of producing an aluminum alloy sheet for a lithographic printing plate comprising homogenizing an ingot of the aluminum alloy comprising 0.03 to 0.15% of Si, 0.2 to 0.6% of Fe, 0.005 to 0.05% of Ti, and 2 to 30 ppm of Pb, with the balance being aluminum and unavoidable impurities at 500 to 610° C. for one hour or more, subjecting the homogenized product to rough hot rolling, a start temperature of the rough hot rolling being 430 to 500° C. and a finish temperature of the rough hot rolling being 400° C. or more, holding the product subjected to the rough hot rolling for 60 to 300 seconds after completion of the rough hot rolling to recrystallize the surface of the product, subjecting the resulting product to finish hot rolling that is finished at 330° C. or more, and cold-rolling the resulting product at a reduction ratio of 80% or more.

### Claim 11 (depends on 9)

The method of producing an aluminum alloy sheet according to claim 9, the aluminum alloy further comprising 0.05% or less of Cu.

### Claim 12 (depends on 9)

The method of producing an aluminum alloy sheet according to claim 9, the aluminum alloy further comprising less than 0.05% of Mg.

### Claim 13 (depends on 9)

The method of producing an aluminum alloy sheet according to claim 9, the aluminum alloy further comprising 0.05% or less of Cu and less than 0.05% of Mg.