# US 2008/0308198 A1 · Austenitic Stainless Steel, Manufacturing Method for the Same, and Structure Using the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0308198 A1
- Document ID: US20080308198A1
- Status: Published application
- Kind: A1
- Application number: 10/585,885
- Filed: 2005-01-13
- Published: 2008-12-18
- Earliest claimed: 2004-01-13
- Assignees: Mitsubishi Heavy Industries, Ltd.; The Tokyo Electric Power Company, Incorporated
- Inventors: Yasuhiro Sakaguchi; Toshihiko Iwamura; Hiroshi Kanasaki; Hidehito Mimaki; Masaki Taneike; Shunichi Suzuki; Kenrou Takamori; Suguru Ooki; Naoki Anahara; Naoki Hiranuma; Toshio Yonezawa
- Web page: https://patentgrep.com/patent/US20080308198A1

## CPC

- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/02: Hardening by precipitation
- C21D 7/02: by cold working
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/44: with molybdenum or tungsten
- C21D 6/004: {containing Cr and Ni}
- C21D 2211/001: Austenite
- Y10S 376/90: Particular material or material shapes for fission reactors
- Y10T 428/13: Hollow or container type article [e.g., tube, vase, etc.]
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

There are provided an austenitic stainless steel having high stress corrosion crack resistance, characterized by containing, in percent by weight, 0.030% or less C, 0.1% or less Si, 2.0% or less Mn, 0.03% or less P, 0.002% or less S, 11 to 26% Ni, 17 to 30% Cr, 3% or less Mo, and 0.01% or less N, the balance substantially being Fe and unavoidable impurities; a manufacturing method for an austenitic stainless steel, characterized in that a billet consisting of the said austenitic stainless steel is subjected to solution heat treatment at a temperature of 1000 to 1150° C.; and a pipe and a in-furnace structure for a nuclear reactor to which the said austenitic stainless steel is applied.

## Claims

### Claim 1

An austenitic stainless steel having high stress corrosion crack resistance, characterized by containing, in percent by weight,
0.030% or less C,
0.1% or less Si,
2.0% or less Mn,
0.03% or less P,
0.002% or less S,
11 to 26% Ni,
17 to 30% Cr,
3% or less Mo, and
0.01% or less N,
the balance substantially being Fe and unavoidable impurities.

### Claim 2

An austenitic stainless steel having high stress corrosion crack resistance, characterized by containing, in percent by weight,
0.030% or less C,
0.1% or less Si,
2.0% or less Mn,
0.03% or less P,
0.002% or less S,
11 to 26% Ni,
17 to 30% Cr,
3% or less Mo,
0.01% or less N,
0.001% or less Ca,
0.001% or less Mg, and
0.004% or less O,
the balance substantially being Fe and unavoidable impurities.

### Claim 3

An austenitic stainless steel having high stress corrosion crack resistance, characterized by containing, in percent by weight,
0.030% or less C,
0.1% or less Si,
2.0% or less Mn,
0.03% or less P,
0.002% or less S,
11 to 26% Ni,
17 to 30% Cr,
3% or less Mo,
0.01% or less N,
0.001% or less Ca,
0.001% or less Mg,
0.004% or less O, and
0.01% or less of any one of Zr, B and Hf,
the balance substantially being Fe and unavoidable impurities.

### Claim 4 (depends on 1, 2, 3)

The austenitic stainless steel having high stress corrosion crack resistance according to any one of claims 1 to 3, characterized in that
(Cr equivalent)−(Ni equivalent) is in the range of −5% to +7%.

### Claim 5 (depends on 1, 2, 3)

The austenitic stainless steel having high stress corrosion crack resistance according to any one of claims 1 to 3, characterized in that
Cr equivalent/Ni equivalent is 0.7 to 1.4.

### Claim 6 (depends on 1, 2, 3)

The austenitic stainless steel having high stress corrosion crack resistance according to any one of claims 1 to 3, characterized in that
stacking fault energy (SFE) calculated by the following equation (1):
SFE(mJ/m2)=25.7+6.2×Ni+410×C−0.9×Cr−77×N−13×Si-1.2×Mn (1)
is 100 (mJ/m2) or higher.

### Claim 7 (depends on 1, 2, 3)

A manufacturing method for a stainless steel, characterized in that
a billet consisting of the austenitic stainless steel according to any one of claims 1 to 3 is subjected to solution heat treatment at a temperature of 1000 to 1150° C.

### Claim 8 (depends on 1, 2, 3)

A manufacturing method for a stainless steel, characterized in that
a billet consisting of the austenitic stainless steel according to any one of claims 1 to 3 is subjected to solution heat treatment at a temperature of 1000 to 1150° C., thereafter being subjected to cold working of 10 to 30%, and is then subjected to intergranular carbide precipitation treatment at a temperature of 600 to 800° C. for 1 to 50 hours.

### Claim 9 (depends on 1, 2, 3)

A structure in a nuclear reactor, characterized by being formed of the austenitic stainless steel according to any one of claims 1 to 3.

### Claim 10 (depends on 1, 2, 3)

A pipe for a nuclear reactor, characterized by being formed of the austenitic stainless steel according to any one of claims 1 to 3.

### Claim 11 (depends on 7)

A structure in a nuclear reactor, characterized by being formed of the stainless steel obtained by the manufacturing method according to claim 7.

### Claim 12 (depends on 7)

A pipe for a nuclear reactor, characterized by being formed of the stainless steel obtained by the manufacturing method according to claim 7.

### Claim 13 (depends on 8)

A structure in a nuclear reactor, characterized by being formed of the stainless steel obtained by the manufacturing method according to claim 8.

### Claim 14 (depends on 8)

A pipe for a nuclear reactor, characterized by being formed of the stainless steel obtained by the manufacturing method according to claim 8.