# US 2008/0306291 A1 · Start-up of high selectivity catalysts in olefin oxide plants

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0306291 A1
- Document ID: US20080306291A1
- Status: Published application
- Kind: A1
- Application number: 12/116,653
- Filed: 2008-05-07
- Published: 2008-12-11
- Earliest claimed: 2007-05-11
- Assignees: SD Lizenzverwertungsgesellschaft mbH & Co. KG
- Inventors: Barry Jay Billig; James Mann; Norma Beatriz Castagnola; Christian Gueckel; Andrzej Rokicki
- Web page: https://patentgrep.com/patent/US20080306291A1

## CPC

- C07D 301/10: with catalysts containing silver or gold
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)

## Abstract

A method to achieve a controlled start-up temperature of an expoxidation process which exceeds the maximum achievable temperature of the epoxidation reactor relative to using an external heat source. The method of the present invention employs an oxidation reaction within the reactor to bring the temperature of the reactor to a temperature that is suitable for conditioning a high selectivity catalyst. The method of the present invention includes first bringing a reactor including a high selectivity catalyst to a first temperature using the external heat source to the reactor, while staying within the reactor design limitations and maintaining a gas flow to the reactor that is within 25 to 100% of the design rates. Once the reactor has achieved the first temperature, at least an olefin, e.g., ethylene, and then oxygen are introduced to the reactor feed gas. The olefin and oxygen concentrations are adjusted to have a heat of reaction that will allow raising the reactor gas flow to 100% of design and then have sufficient heat of reaction to raise the reactor temperature to a second temperature which is greater than the first temperature and greater than the temperature of the reactor achievable by the external heat source.

## Claims

### Claim 1

A method to achieve a controlled start-up temperature of an epoxidation process comprising:
bringing a reactor including a high selectivity catalyst to a first temperature by an external heat source of the reactor, while staying within reactor design limitations and maintaining a gas flow to the reactor that is within 25 to 100% of design rates; and
subsequently introducing at least an olefin and then oxygen to the feed gas to cause a heat of reaction within said reactor to raise the first temperature to a second temperature which is greater than the first temperature.

### Claim 2 (depends on 1)

The method of claim 1 wherein the second temperature within the reactor is controlled by adjusting the feed rate of at least one of said olefin, oxygen, CO2 and/or moderator.

### Claim 3 (depends on 1)

The method of claim 1 further comprising controlling the concentration level of oxygen at the reactor outlet.

### Claim 4 (depends on 3)

The method of claim 3 wherein said adjusting is achieved by changing the flow of one of the olefin, oxygen, carbon dioxide and/or moderator in said gas feed.

### Claim 5 (depends on 4)

The method of claim 4 wherein said oxygen flow is adjusted utilizing an oxygen mixing station.

### Claim 6 (depends on 1)

The method of claim 1 wherein the second temperature exceeds the maximum reactor coolant temperature.

### Claim 7 (depends on 1)

The method of claim 1 wherein said high selectivity catalyst includes silver in an amount up to 45% by weight.

### Claim 8 (depends on 7)

The method of claim 7 wherein said silver is supported on a solid refractory support having a surface area of at most 20 m2/gm.

### Claim 9 (depends on 8)

The method of claim 8 wherein said solid refractory support is alpha alumina.

### Claim 10 (depends on 7)

The method of claim 7 further comprising a promoting amount of rhenium.

### Claim 11 (depends on 10)

The method of claim 10 wherein said promoting amount of rhenium is from about 0.01 wt. % to about 1 wt. %.

### Claim 12 (depends on 10)

The method of claim 10 further comprising a promoting amount of at least one alkali metal.

### Claim 13 (depends on 12)

The method of claim 12 wherein said at least one alkali metal is a combination of lithium and cesium.

### Claim 14 (depends on 7)

The method of claim 7 further comprising a promoting amount of at least one transition metal selected from Mo, W, Cr, Ti, Hf, Zr, V, Ta and Nb.

### Claim 15 (depends on 1)

The method of claim 1 wherein said high selectivity catalyst is a calcined catalyst.

### Claim 16 (depends on 7)

The method of claim 7 further comprising a promoting amount of sulfur.

### Claim 17 (depends on 1)

The method of claim 1 wherein said first temperature is from about 180° C. to about 250° C.

### Claim 18

The method of claim I wherein said second temperature is from about 240° C. to about 290° C.