# US 2008/0306209 A1 · Production of a Water-Absorbing Resin to Which a Particulate Additive is Admixed

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0306209 A1
- Document ID: US20080306209A1
- Status: Published application
- Kind: A1
- Application number: 12/158,502
- Filed: 2006-12-28
- Published: 2008-12-11
- Earliest claimed: 2005-12-29
- Assignees: BASF SE
- Inventors: Uwe Stueven; Rudiger Funk; Matthias Weismantel; Thomas Daniel; Annemarie Hillebrecht; Dominicus van Esbroeck; Karl J. Possemiers
- Web page: https://patentgrep.com/patent/US20080306209A1

## CPC

- C08F 2/44: Polymerisation in the presence of compounding ingredients, e.g. plasticisers, dyestuffs, fillers
- C08F 220/06: Acrylic acid; Methacrylic acid; Metal salts or ammonium salts thereof
- C08F 222/102: {of dialcohols, e.g. ethylene glycol di(meth)acrylate or 1,4-butanediol dimethacrylate}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The invention relates to a process for producing a water-absorbing resin by polymerization of a reaction mixture comprising at least one hydrophilic monomer and, if appropriate, at least one crosslinker in a reactor, which comprises admixing the reaction mixture with at least one first portion of a particulate additive before the reaction mixture has reached a residence time of 40% of the overall residence time in the reactor and with at least one second portion of a particulate additive when the reaction mixture has reached a residence time of 45% or more of the overall residence time in the reactor, the additive being selected from water-absorbing resin powders, fillers and mixtures thereof, the total solids content of monomer and additive being in the range from 30% to 60% by weight, the amount of additive being in the range from 5% to 50% by weight, based on the monomers, and the weight ratio of the first portion to the second portion of the additive being in the range from 10:1 to 1:5. The resin powder is recycled fine-sized material for example. Not only the residual monomer content, specifically the residual crosslinker content, but also the level of extractables in the water-absorbing resin are reduced by the method of addition described. A high fraction of additives can be incorporated without the properties of the water-absorbing resin obtained being adversely affected. The additives enter a sufficiently firm bond with the resin, so that no excessive dusting occurs on exposure to mechanical stress.

## Claims

### Claim 1

A process for producing a water-absorbing resin by polymerization of a reaction mixture comprising at least one hydrophilic monomer and, if optionally, at least one crosslinker in a reactor, which comprises admixing the reaction mixture with at least one first portion of a particulate additive before a reaction mixture has reached a residence time of 40% of the overall residence time in the reactor and with at least one second portion of a particulate additive when the reaction mixture has reached a residence time of 45% or more of the overall residence time in the reactor, the additive being selected from the group consisting of water-absorbing resin powders, fillers, and mixtures thereof, a total solids content of monomer and additive being in the range from 30% to 60% by weight, an amount of additive being in the range from 5% to 50% by weight, based on the monomers, and a weight ratio of the first portion to the second portion of the additive being in the range from 10:1 to 1:5.

### Claim 2 (depends on 1)

The process according to claim 1 wherein the first portion of the additive is admixed when the reaction mixture has reached a residence time of up to 30% of the overall residence time in the reactor.

### Claim 3 (depends on 1)

The process according to claim 1 wherein the second portion of the additive is admixed when the reaction mixture has reached a residence time in the range from 50% to 99% of the overall residence time in the reactor.

### Claim 4 (depends on 1)

The process according to claim 1 wherein an aqueous solution of monomer is fed to an input end of a continuous operated reactor having at least two axially parallel rotating shafts, in which the reaction mixture is transported from the input end of the reactor to its output end as the polymerization progresses, and the first and second portions of the additive are admixed at two locations of the reactor which are spaced apart in the direction of transport of the monomer solution.

### Claim 5 (depends on 1)

The process according to claim 1 wherein the resin powder has a weight average particle size of less than 200 μm.

### Claim 6 (depends on 1)

The process according to claim 1 wherein the resin powder has a moisture content in the range from 0.1% to 10% by weight.

### Claim 7 (depends on 1)

The process according to claim 1 wherein the resin powder comprises a non-surface-postcrosslinked hydrogel, a surface-postcrosslinked hydrogel, or a mixture thereof.

### Claim 8 (depends on 1)

The process according claim 1 wherein the amount of additive is in the range from 15% to 40% by weight, based on the monomers.

### Claim 9 (depends on 1)

The process according to claim 1 wherein the weight ratio of the first portion to the second portion of the additive is in the range from 5:1 to 1:1.

### Claim 10 (depends on 1)

The process according to claim 1 wherein the fillers are inorganic particles.

### Claim 11 (depends on 10)

The process according to claim 10 wherein the inorganic particles are selected from clay minerals, polysilicas, zeolites, activated carbon, water-insoluble metal phosphates, metal oxides, metal carbonates, and mixtures thereof.

### Claim 12 (depends on 1)

The process according to claim 1 wherein the fillers are organic particles.

### Claim 13 (depends on 1)

The process according to claim 1 wherein the fillers have an average particle size in the range from 10 to 500 μm.

### Claim 14 (depends on 1)

The process according to claim 1 wherein the first portion of the additive comprises resin powder only and the second portion of the additive comprises a mixture of resin powder and fillers.

### Claim 15 (depends on 1)

The process according to claim 1 wherein the reaction mixture comprises 0.01% to 5% by weight of a crosslinker, based on the hydrophilic monomer.

### Claim 16 (depends on 1)

The process according to claim 1 wherein the hydrophilic monomer comprises partially neutralized acrylic acid.