# US 2008/0306188 A1 · Novel UV inhibitors and stabilizers, derived from a biomass feedstock source, for thermoplastic and thermosetting resins

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0306188 A1
- Document ID: US20080306188A1
- Status: Published application
- Kind: A1
- Application number: 11/983,157
- Filed: 2007-11-07
- Published: 2008-12-11
- Earliest claimed: 2007-06-06
- Assignees: Impact Composite Technology, Ltd.
- Inventors: Richard William Tock; Daniel W. A'Hern
- Web page: https://patentgrep.com/patent/US20080306188A1

## CPC

- C08J 5/045: {with vegetable or animal fibrous material}
- C08J 5/10: characterised by the additives used in the polymer mixture
- Y10T 428/24438: Artificial wood or leather grain surface
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates in general to biomass derived compositions and methods of applying such biomass derived compositions to protect polymeric materials from degradation due to ultraviolet (“UV”) radiation or light and weathering. More particularly, the invention relates to the use of cotton gin waste to protect polymeric composites from degradation due to UV radiation and weathering. One embodiment of the present invention includes dusting the surface of liquid polymeric materials with a cotton gin waste powder to protect the polymeric material from UV radiation induced damage.

## Claims

### Claim 1

A method for manufacturing polymeric materials at least partially protected against UV damage, the method comprising the steps of:
(a) mixing a polymeric resin and a reinforcement fiber to form a polymeric mixture;
(b) applying a powdered natural biomass material containing UV absorbents and antioxidants to an external surface of the polymeric mixture prior to the solidification of the polymeric mixture; and
(c) allowing the polymeric mixture to polymerize to form a solid polymeric material having an external layer of the natural biomass material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the natural biomass material is a cotton gin waste.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reinforcement fiber is a cotton gin waste.

### Claim 4 (depends on 3)

The method of claim 3, wherein the polymeric mixture comprises from about 7.5% by weight to about 10.0% by weight of the cotton gin waste.

### Claim 5 (depends on 1)

The method of claim 1, further comprising the steps of: extracting a mixture of UV absorbents and antioxidants from a powdered cotton gin waste with a liquid monomer and adding the liquid monomer extract to the polymeric resin.

### Claim 6 (depends on 5)

The method of claim 5, wherein the liquid monomer extract contains at least one derivative of phthalic acid.

### Claim 7 (depends on 1)

The method of claim 1, further comprising the steps of: extracting a mixture of UV absorbents and antioxidants from a powdered cotton gin waste with a liquid monomer and adsorbing the liquid monomer extract to the reinforcement fiber.

### Claim 8 (depends on 7)

The method of claim 7, wherein the liquid monomer extract contains at least one derivative of phthalic acid.

### Claim 9 (depends on 1)

The method of claim 1, wherein a sufficient quantity of the powdered natural biomass material is applied to the external surface of the liquid polymeric mixture to provide the polymeric material with a wood like appearance.

### Claim 10

A method for manufacturing thermoplastic products at least partially protected from UV damage whenever the products are exposed to UV radiation, the method comprising the steps of:
(a) blending a polymeric resin, a reinforcement fiber, and a powdered natural biomass material containing UV absorbents and antioxidants to form a liquid polymeric mixture;
(b) introducing the liquid polymeric mixture into a mold having a desired shape;
(c) solidifying the molded polymeric mixture; and
(d) removing the solidified polymeric mixture from the mold.

### Claim 11 (depends on 10)

The method of claim 10, wherein the powdered natural biomass material is a cotton gin waste.

### Claim 12 (depends on 11)

The method of claim 11, wherein the polymeric mixture comprises from about 7.5% by weight to about 10.0% by weight of the cotton gin waste.

### Claim 13

A method for manufacturing thermoset plastic products at least partially protected from UV damage whenever the products are exposed to UV radiation, the method comprising the steps of:
(a) mixing a polymeric resin and a reinforcement fiber to form a polymeric mixture;
(b) applying a cotton gin waste to an external surface of the polymeric mixture prior to the solidification of the polymeric mixture, wherein the cotton gin waste contains a mixture of UV absorbers and antioxidants; and
(c) allowing the polymeric mixture to polymerize to form a solid polymeric material having an external layer containing the cotton gin waste.

### Claim 14 (depends on 13)

The method of claim 13, wherein a portion of the reinforcement fiber in the polymeric mixture is a finely ground cotton gin waste comminuted by passage through an 80 mesh or greater screen.

### Claim 15 (depends on 14)

The method of claim 14, wherein the polymeric mixture comprises from about 7.5% by weight to about 10.0% by weight of the cotton gin waste.

### Claim 16 (depends on 13)

The method of claim 13, further comprising the steps of: extracting a mixture of UV absorbents and antioxidants from a powdered cotton gin waste with a liquid monomer and adding the liquid monomer extract to the polymeric resin.

### Claim 17 (depends on 16)

The method of claim 16, wherein the liquid monomer extract contains at least one derivative of phthalic acid.

### Claim 18 (depends on 13)

The method of claim 13, further comprising the steps of: extracting a mixture of UV absorbents and antioxidants from a powdered cotton gin waste with a liquid monomer and adsorbing the liquid monomer extract to the reinforcement fiber.

### Claim 19

A thermoset plastic product comprising an external surface having a wood like appearance, wherein the wood like appearance is derived from an external layer of a cotton gin waste.

### Claim 20 (depends on 19)

The thermoset plastic product of claim 19, wherein the external layer of the cotton gin waste makes up about 1% to about 10% of the weight of the plastic product.

### Claim 21

A thermoset plastic composite containing at least two layers of polymerized materials, the composite comprising a first layer of polymerized material containing a cotton gin waste extract including at least one phthalic acid derivative; and an external layer containing cotton gin waste, wherein the external layer has a wood like appearance.