# US 2008/0305647 A1 · Method for Manufacturing a Semiconductor Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305647 A1
- Document ID: US20080305647A1
- Status: Published application
- Kind: A1
- Application number: 11/547,691
- Filed: 2006-08-28
- Published: 2008-12-11
- Earliest claimed: 2005-09-29
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Daisuke Matsushita; Koichi Muraoka; Koichi Kato; Yasushi Nakasaki; Yuichiro Mitani
- Web page: https://patentgrep.com/patent/US20080305647A1

## CPC

- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/24: Nitriding
- C23C 8/80: After-treatment
- H10B 41/30: characterised by the memory core region
- H10B 43/30: characterised by the memory core region
- H10B 69/00: Erasable-and-programmable ROM [EPROM] devices not provided for in groups H10B41/00 - H10B63/00, e.g. ultraviolet erasable-and-programmable ROM [UVEPROM] devices
- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- H10D 64/01352: {with sacrificial oxide}
- H10D 64/685: {being perpendicular to the channel plane}
- H10P 14/6316: {Formation by nitridation, e.g. nitridation of the substrate}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10D 62/314: {having vertical doping variations (vertical IGFETs H10D30/63)}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/212: {Through-implantation}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

It is made possible to restrain generation of defects at the time of insulating film formation. A method for manufacturing a semiconductor device, includes: placing a semiconductor substrate into an atmosphere, thereby forming a nitride film on a surface of the semiconductor substrate, the atmosphere containing a first nitriding gas nitriding the surface of the semiconductor substrate and a first diluent gas not actually reacting with the semiconductor substrate, the ratio of the sum of the partial pressure of the first diluent gas and the partial pressure of the first nitriding gas to the partial pressure of the first nitriding gas being 5 or higher, and the total pressure of the atmosphere being 40 Torr or lower.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, comprising:
placing a semiconductor substrate into an atmosphere, thereby forming a nitride film on a surface of the semiconductor substrate, the atmosphere containing a first nitriding gas nitriding the surface of the semiconductor substrate and a first diluent gas not actually reacting with the semiconductor substrate, the ratio of the sum of the partial pressure of the first diluent gas and the partial pressure of the first nitriding gas to the partial pressure of the first nitriding gas being 5 or higher, and the total pressure of the atmosphere being 3 Torr or higher but 40 Torr or lower.

### Claim 2

The method for manufacturing a semiconductor device according to 1, wherein the first nitriding gas is one of NH3 gas, radical N* gas, and N2* gas.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the total pressure of the atmosphere is 30 Torr or lower.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the first diluent gas contains N2 gas.

### Claim 5 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the first diluent gas contains a component having natural vibration energy similar to atomic vibration energy at the interface between the semiconductor substrate and the nitride film.

### Claim 6 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, further comprising:
performing heat treatment for the semiconductor substrate placed in an atmosphere of a gas not actually reacting with the semiconductor substrate, after the nitride film is formed on the surface of the semiconductor substrate.

### Claim 7 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6, wherein the gas not actually reacting with the semiconductor substrate is N2 gas or He gas.

### Claim 8 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein, in the atmosphere for forming the nitride film,
the ratio of the sum of the partial pressure of the first dilution gas and the partial pressure of the first nitriding gas to the partial pressure of the first nitriding gas is 10000 or lower.

### Claim 9 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the nitride film is formed at a temperature of 700° C. or more but 850° C. or less.

### Claim 10

A method for manufacturing a semiconductor device, comprising:
placing a semiconductor substrate into a first atmosphere, thereby forming a nitride film on a surface of the semiconductor substrate, the first atmosphere containing a first nitriding gas nitriding the surface of the semiconductor substrate and a first diluent gas not actually reacting with the semiconductor substrate during production, the ratio of the sum of the partial pressure of the first diluent gas and the partial pressure of the first nitriding gas to the partial pressure of the first nitriding gas being 5 or higher, and the total pressure of the first atmosphere being 3 Torr or higher but 40 Torr or lower; and
placing the semiconductor substrate having the nitride film formed on the surface thereof into a second atmosphere containing a radical second nitriding gas, thereby forming a nitride layer between the semiconductor substrate and the nitride film.

### Claim 11 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10, wherein a film thickness of the nitride film is 4 Å or more but 1 nm or less.

### Claim 12

The method for manufacturing a semiconductor device according to 10, wherein the second nitriding gas is N* gas or N2* gas.

### Claim 13

A method for manufacturing a semiconductor device, comprising:
placing a semiconductor substrate into a first atmosphere, thereby forming a nitride film on a surface of the semiconductor substrate, the first atmosphere containing a first nitriding gas nitriding the surface of the semiconductor substrate and a first diluent gas not actually reacting with the semiconductor substrate during production, the ratio of the sum of the partial pressure of the first diluent gas and the partial pressure of the first nitriding gas to the partial pressure of the first nitriding gas being 5 or higher, and the total pressure of the first atmosphere being 3 Torr or higher but 40 Torr or lower; and
placing the semiconductor substrate having the nitride film formed on the surface thereof into a second atmosphere, thereby forming a first oxynitride layer between the semiconductor substrate and the nitride film, and a second oxynitride layer on a surface of the nitride film, the second atmosphere containing an oxidizing gas and a second dilution gas not actually reacting with the semiconductor substrate during production.

### Claim 14 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, wherein the oxidizing gas is one of O2 gas, N2O gas, NO gas, and O* gas.

### Claim 15 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, wherein the second diluent gas is N2 gas.

### Claim 16 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, further comprising:
performing first heat treatment for the semiconductor substrate having the nitride film formed on the surface thereof, the semiconductor substrate being placed into a third atmosphere containing a gas not actually reacting with the semiconductor substrate, the first heat treatment being performed between the formation of the nitride film and the formation of the first oxynitride layer.

### Claim 17 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, wherein the formation of the first and second oxynitride layers is carried out at a temperature of 800° C. or more but 950° C. or less.

### Claim 18 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, further comprising:
performing second heat treatment for the semiconductor substrate placed into a fourth atmosphere containing a gas not actually reacting with the semiconductor substrate, the second heat treatment being performed after the formation of the first and second oxynitride layers.

### Claim 19 (depends on 18)

The method for manufacturing a semiconductor device according to claim 18, wherein the gas not actually reacting with the semiconductor substrate is N2 gas or He gas.

### Claim 20 (depends on 18)

The method for manufacturing a semiconductor device according to claim 18, further comprising:
introducing nitrogen into the second oxynitride film before the second heat treatment after the formation of the first and second oxynitride layers.

### Claim 21 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the nitride film is included in a tunnel insulating film of a floating-gate non-volatile memory.

### Claim 22 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the nitride film is included in a tunnel insulating film of a MONOS non-volatile memory.

### Claim 23 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the nitride film is included in a gate insulating film of a MISFET.