# US 2008/0305634 A1 · Metal Film Separation Prevention Structure in Metal Film Forming Device, and Semiconductor Device Manufacturing Method Using Said Structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305634 A1
- Document ID: US20080305634A1
- Status: Published application
- Kind: A1
- Application number: 12/122,794
- Filed: 2008-05-19
- Published: 2008-12-11
- Earliest claimed: 2007-05-23
- Assignees: Texas Instruments Incorporated
- Inventors: Toshifumi Igarashi
- Web page: https://patentgrep.com/patent/US20080305634A1

## CPC

- C23C 16/4404: {Coatings or surface treatment on the inside of the reaction chamber or on parts thereof}
- C23C 4/01: Selective coating, e.g. pattern coating, without pre-treatment of the material to be coated
- C23C 14/564: {Means for minimising impurities in the coating chamber such as dust, moisture, residual gases}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The object of this invention is to prevent unwanted separation of a deposited metal film from a member, such as an anti-adhesion plate, in the chamber of a metal film forming device. In a sputtering device, metal particles sputtered from the surface of a target 12 in a chamber 10 are not only dispersed or scattered toward a semiconductor wafer 22 on the front of the target, but also adhere to shield member 30 to form a deposited metal film 40. Shield member 30 is made of stainless steel, for example, a plasma spray film made of aluminum or an aluminum alloy is formed on its anti-adhesion surface (inner wall surface), and the surface of the plasma spray film is suitably roughened.

## Claims

### Claim 1

A metal film separation prevention structure in a metal film forming device with which a metal thin-film is formed on a treated substrate in a chamber at reduced pressure,
which is a metal film forming device wherein, in order to prevent or curb separation of the deposited metal film from a specified member where the aforementioned metal is deposited by adhering around the aforementioned substrate when a metal film is formed against the aforementioned substrate in the aforementioned chamber, a plasma spray film made of aluminum or an aluminum alloy is formed on the surface of the aforementioned member, and the surface of the aforementioned plasma spray film is roughened.

### Claim 2 (depends on 1)

The metal film separation prevention structure described in claim 1 wherein the surface roughness of the aforementioned plasma spray film is in the range of 65 μm≦Rz≦130 μm, as the ten-point height of irregularities Rz.

### Claim 3 (depends on 2)

The metal film separation prevention structure described in claim 2 wherein the surface roughness of the aforementioned plasma spray film is in the range of 100 μm≦Rz≦130 μm, as the ten-point height of irregularities Rz.

### Claim 4 (depends on 1)

The metal film separation prevention structure described in claim 1 wherein the mean spacing of concavities and convexities in the surface of the aforementioned plasma spray film is in the range of 200 μm-400 μm.

### Claim 5 (depends on 1)

The metal film separation prevention structure described in claim 1 wherein the mean thickness of the aforementioned plasma spray film is 200 μm or more.

### Claim 6 (depends on 1)

The metal film separation prevention structure described in claim 1 wherein the aforementioned metal is a refractory metal or a nitride of a refractory metal.

### Claim 7 (depends on 1)

The metal film separation prevention structure described in claim 1 wherein the aforementioned member includes an anti-adhesion plate to prevent adherence of a deposited film of the aforementioned metal to the inner walls of the aforementioned chamber.

### Claim 8 (depends on 1)

The metal film separation prevention structure described in claim 1 wherein the aforementioned metal film forming device is a sputtering device that forms a metal thin-film on the aforementioned substrate with sputtering.

### Claim 9

A semiconductor device manufacturing method that includes a process to apply metal film formation processing to a semiconductor wafer in a chamber provided with a metal film anti-adhesion member,
which is a semiconductor device manufacturing method having:
a process wherein a semiconductor wafer is introduced into a chamber,
a process to apply metal film formation processing to the aforementioned semiconductor wafer,
a process to remove the metal film anti-adhesion member in the chamber,
a process to wash the removed anti-adhesion member,
a process to install the washed anti-adhesion member in the aforementioned chamber,
a process to introduce a semiconductor wafer into a chamber,
and a process to apply metal film formation processing to the aforementioned semiconductor wafer,
and wherein a plasma spray film made of aluminum or an aluminum alloy is formed on the surface of the aforementioned anti-adhesion member, and the surface roughness of the aforementioned plasma spray film is in the range 65 μm≦Rz≦130 μm, as the ten-point height of irregularities Rz.