# US 2008/0305618 A1 · Method of forming polycrystalline semiconductor film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305618 A1
- Document ID: US20080305618A1
- Status: Published application
- Kind: A1
- Application number: 12/133,635
- Filed: 2008-06-05
- Published: 2008-12-11
- Earliest claimed: 2007-06-07
- Assignees: Advanced LCD Technologies Development Center Co., Ltd.
- Inventors: Daisuke IGA; Yukio TANIGUCHI
- Web page: https://patentgrep.com/patent/US20080305618A1

## CPC

- H10P 14/3808: {using laser beams}
- B23K 26/066: by using masks
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3466: {Crystal orientation}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method of forming a polycrystalline semiconductor film, which includes irradiating an amorphous semiconductor film formed on an insulating substrate with light to convert the amorphous semiconductor into a polycrystalline semiconductor with laterally grown crystal grains, thus forming a polycrystalline semiconductor film, wherein crystal growth in the semiconductor is controlled such that first crystal grains laterally grow in the first direction along a X-axis from the first group of initial nuclei, the second crystal grains laterally grow in the second direction opposite to the first direction along the X-axis from the second group of initial nuclei arranged apart from the first group of initial nuclei along the X-axis, and the first crystal grains collide against the second crystal grains at different points in time along a Y-axis.

## Claims

### Claim 1

A method of forming a polycrystalline semiconductor film, which comprises irradiating an amorphous semiconductor film formed on an insulating substrate with light to convert the amorphous semiconductor into a laterally grown polycrystalline semiconductor, thus forming a polycrystalline semiconductor film,
wherein crystal growth in the amorphous semiconductor is controlled such that, on an X-axis and a Y-axis which are set with respect to a surface of the amorphous semiconductor film and which are orthogonal to each other, first crystal grains laterally grow in the first direction along the X-axis from the first group of initial nuclei, the second crystal grains laterally grow in the second direction opposite to the first direction along the X-axis from the second group of initial nuclei arranged apart from the first group of initial nuclei along the X-axis, and the first crystal grains collide against the second crystal grains at different points in time along the Y-axis.

### Claim 2 (depends on 1)

The method according to claim 1, wherein controlling the crystal growth of semiconductor film such that the first crystal grains collide against the second crystal grains at the different points in time along the Y-axis is performed by controlling the crystal growth such that the first crystal grains laterally grow in the first direction along the X-axis from the first group of initial nuclei on the first straight line extending along the Y-axis, the second crystal grains laterally grow in the second direction opposite to the first direction along the X-axis from the second group of initial nuclei arranged on the second straight line extending along the Y-axis and apart from the first straight line, and growing speeds of the first and second crystal grains vary along the Y-axis.

### Claim 3 (depends on 1)

The method according to claim 1, wherein controlling the crystal growth in the amorphous semiconductor film such that the first crystal grains collide against the second crystal grains at the different points in time along the Y-axis is performed by controlling the crystal growth such that the first crystal grains laterally grow in the first direction along the X-axis from the first group of initial nuclei arranged at positions in the X-axis direction which vary along the Y-axis, and the second crystal laterally grow in the second direction opposite to the first direction from the second group of initial nuclei.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the first crystal grains and the second crystal grains grow laterally along the X-axis and collide against one another, and after the collision, the crystal growth in an area in which the collision occurs earlier than in an adjacent area along the Y-axis progresses to the adjacent area along the Y-axis in which the crystal growth has not started yet, and a plurality of isolated nodules are finally formed.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the light with which the amorphous semiconductor is irradiated, exhibits an intensity distribution varying in V shape along the X-axis and having a gradient increasing and decreasing along the Y-axis.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the light exhibiting the intensity distribution varying in V shape along the X-axis and having a gradient of cyclic increase and decrease along the Y-axis is formed by a light modulating element.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the light modulating element has a basic pattern in which elongate band-like areas containing a plurality of unit areas arranged along the Y-axis and extending along the Y-axis are repeatedly arranged along the X-axis, and in each of the band-like areas, a ratio of the first area having the first phase value to the second area having the second phase value varies with the unit area along the X-axis, and a change rate of an occupied area rate of the first area in each unit area increases and decreases in the Y-axis for each band-like area.

### Claim 8

A method of manufacturing a thin-film semiconductor device, which comprises:
forming an amorphous semiconductor film on an insulating substrate;
irradiating the amorphous semiconductor film with light to convert the amorphous semiconductor into a polycrystalline semiconductor with laterally grown crystal grains, thus forming a polycrystalline semiconductor film; and
forming a plurality of thin-film transistors each having the polycrystalline semiconductor film as an active layer,
wherein during forming the polycrystalline semiconductor film, crystal growth in the semiconductor is controlled such that, on an X-axis and a Y-axis which are set with respect to a surface of the amorphous semiconductor film and which are orthogonal to each other, first crystal grains laterally grow in the first direction along the X-axis from the first group of initial nuclei, the second crystal grains laterally grow in the second direction opposite to the first direction along the X-axis from the second group of initial nuclei arranged apart from the first group of initial nuclei along the X-axis, and the first crystal grains collide against the second crystal grains at different points in time along the Y-axis.

### Claim 9 (depends on 8)

The method according to claim 8, wherein controlling the crystal growth in the semiconductor film such that the first crystal grains collide against the second crystal grains at the different points in time along the Y-axis is performed by controlling the crystal growth such that the first crystal grains in the second direction grow in the first direction along the X-axis from the first group of initial nuclei on the first straight line extending along the Y-axis, the second crystal grains laterally grow in the second direction opposite to the first direction along the X-axis from the second group of initial nuclei arranged on the second straight line extending along the Y-axis and apart from the first straight line, and growing speeds of the first and the second crystal grains vary along the Y-axis.

### Claim 10 (depends on 8)

The method according to claim 8, wherein controlling the crystal growth in the amorphous semiconductor film such that the first crystal grains collide against the second crystal grains at the different points in time along the Y-axis is performed by controlling the crystal growth such that the first crystal grains laterally grow in the first direction along the X-axis from the first group of initial nuclei arranged at positions in the X-axis direction which vary along the Y-axis, and the second crystal grains laterally grow in the second direction opposite to the first direction from the second group of initial nuclei.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the first crystal grains and the second crystal grains grow laterally along the X-axis and collide against one another, and after the collision, the crystal growth in an area in which the collision occurs earlier than in an adjacent area along the Y-axis progresses to the adjacent area along the Y-axis in which the crystal growth has not started yet, and a plurality of isolated dot-like nodules are finally formed.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the forming the plurality of thin-film transistors each having the polycrystalline semiconductor film as the active layer includes patterning the polycrystalline semiconductor film to form a plurality of island-like polycrystalline semiconductor films, and forming the thin-film transistor on each of the plurality of island-like polycrystalline semiconductor films.

### Claim 13 (depends on 8)

The method according to claim 8, wherein light with which the amorphous semiconductor is irradiated, exhibits an intensity distribution varying in V shape along the X-axis and having a gradient increasing and decreasing along the Y-axis.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the light exhibiting the intensity distribution varying in V shape along the X-axis and having the gradient increasing and decreasing along the Y-axis is formed by a light modulating element.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the light modulating element has a basic pattern in which elongate band-like areas containing a plurality of unit areas arranged along the Y-axis and extending along the Y-axis are repeatedly arranged along the X-axis, and in each of the band-like areas, a ratio of the first area having the first phase value to the second area having the second phase value varies with the unit area along the X-axis, and a change rate of an occupied area rate of the first area in each unit area increases and decreases in the Y-axis for each band-like area.

### Claim 16 (depends on 11)

The method according to claim 11, wherein a sum of size Φ of each of the dot-like nodules and an interval S between the adjacent dot-like projections is smaller than a minimum design rule Dm between the plurality of thin-film transistors.