# US 2008/0305607 A1 · Thin film capacitor and fabrication method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305607 A1
- Document ID: US20080305607A1
- Status: Published application
- Kind: A1
- Application number: 12/219,577
- Filed: 2008-07-24
- Published: 2008-12-11
- Earliest claimed: 2006-03-31
- Assignees: Fujitsu Limited
- Inventors: John David Baniecki; Takeshi Shioga; Kazuaki Kurihara
- Web page: https://patentgrep.com/patent/US20080305607A1

## CPC

- H01G 4/085: {Vapour deposited}
- H01G 4/1227: {based on alkaline earth titanates}
- H01G 4/33: Thin- or thick-film capacitors {(thin- or thick-film circuits; capacitors without a potential-jump or surface barrier specially adapted for integrated circuits, details thereof, multistep manufacturing processes therefor)}
- H10B 12/033: {the capacitor extending over the transistor}
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10B 53/30: characterised by the memory core region
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/69394: {the material containing titanium, e.g. TiO2}
- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A thin film capacitor comprising a top electrode, a bottom electrode, and a dielectric film held between the top and bottom electrodes. The dielectric film is composed of at least cations Ba, Sr, and Ti and anion O. The concentration of Sr, Ti, and O ions are uniform along the growth direction of the dielectric film while the concentration of the Ba cation is non-uniform along the growth direction such that a reduced Ba-I region in which the average concentration of perovskite type Ba cations (Ba-I) is less than the average concentration of non-perovskite type Ba cations (Ba-II) exists at or near the boundary between at least one of the top and bottom electrodes, with ratio R=(atm % Ba-I)/[(atm % Ba-I)+(atm % Ba-II)] within a range of 0.1<R<0.2.

## Claims

### Claim 1

A method for fabricating a thin film capacitor comprising steps of:
forming a dielectric film over a bottom electrode, the dielectric film being composed of at least Ba, Sr, Ti, and O at prescribed compositions; and
controlling a deposition condition of a top electrode when forming the top electrode over the dielectric film so as to produce a reduced Ba-I region in the dielectric film, in which region an average concentration of perovskite type Ba cations (Ba-I) is less than an average concentration of non-perovskite type Ba cations (Ba-II), at or near a boundary between the top electrode and the dielectric film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the deposition condition is controlled such that a ratio R=(atm % Ba-I)/[(atm % Ba-I)+(atm % Ba-II)] is within a range of 0.1<R<0.2.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reduced Ba-I region is produced so as to extend to 5.0 nm, and more preferably, to 2.5 nm, from the boundary.

### Claim 4 (depends on 1)

The method of claim 1, further comprising a step of:
annealing the thin film capacitor in a temperature range of 100° C. to 900° C. in an oxygen atmosphere after the top electrode is formed.

### Claim 5

A method for fabricating a semiconductor device comprising the steps of:
forming a transistor on a semiconductor substrate; and
forming a thin film capacitor electrically connected to the transistor, the thin film capacitor including a dielectric film held between a top electrode and a bottom electrode,
wherein during the formation of the thin film capacitor, a reduced Ba-I region is formed in the dielectric film in which an average concentration of perovskite type Ba cations (Ba-I) is less than an average concentration of non-perovskite type Ba cations (Ba-II), at or near a boundary between the top electrode and the dielectric film.

### Claim 6 (depends on 5)

The method of claim 5, the thin film capacitor forming step including a step of:
controlling a deposition condition of the top electrode such that in the reduced Ba-I region a ratio R=(atm % Ba-I)/[(atm % Ba-I)+(atm % Ba-II)] is within a range of 0.1<R<0.2.

### Claim 7 (depends on 5)

The method of claim 5, further comprising a step of:
annealing the thin film capacitor in a temperature range of 100° C. to 900° C. in an oxygen atmosphere.

### Claim 8 (depends on 5)

The method of claim 5, further comprising steps of:
forming a contact plug for electrically connecting the transistor to the thin film capacitor; and
forming an adhesion layer to be located between the contact plug and the thin film capacitor.

### Claim 9 (depends on 2)

The method of claim 2, further comprising a step of:
annealing the thin film capacitor in a temperature range of 100° C. to 900° C. in an oxygen atmosphere after the top electrode is formed.