# US 2008/0305604 A1 · Deep trench and fabricating method thereof, trench capacitor and fabricating method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305604 A1
- Document ID: US20080305604A1
- Status: Published application
- Kind: A1
- Application number: 11/943,586
- Filed: 2007-11-21
- Published: 2008-12-11
- Earliest claimed: 2007-06-08
- Assignees: Nanya Technology Corporation
- Inventors: Shian-Jyh Lin
- Web page: https://patentgrep.com/patent/US20080305604A1

## CPC

- H10D 1/712: {being rough surfaces, e.g. using hemispherical grains}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of fabricating a deep trench is provided, by which a trench is formed in the substrate initially. Then, a block layer is formed on the substrate surface of the upper portion of the trench. After that, a pad oxide layer is formed on the substrate surface of the lower portion of the trench. Next, a plurality of hemispherical silicon grains is formed on the substrate and exposes a portion of the pad oxide layer. Then, by using the hemispherical silicon grains as a mask, a portion of the pad oxide layer is removed so as to form a patterned pad oxide layer. Continually, the hemispherical silicon grains and the substrate exposed by the patterned pad oxide layer are removed. Finally, the patterned pad oxide layer is removed.

## Claims

### Claim 1

A trench fabricating method consisting essentially of the steps of:
forming a trench in a substrate to allow the trench to have a lower portion and an upper portion;
forming multiple undulating concaves in an inner surface of the lower portion of the trench of the substrate, wherein the undulating concaves extend away from a center of the trench.

### Claim 2 (depends on 1)

The method as claimed in claim 1 further comprising:
a step of forming an oxidation layer on the inner surface of the lower portion of the trench and a bottom surface of the trench; and
a step of forming a nitrification layer on an inner surface of the upper portion of the trench and on an outer surface of the substrate.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein the oxidation layer forming step is performed by proceeding a thermal oxidation process and the nitrification layer forming step is performed by proceeding a thermal nitrification process.

### Claim 4 (depends on 2)

The method as claimed in claim 2, wherein multiple hemispherical silicon grains are formed on the oxidation layer on the inner surface of the lower portion of the trench as well as on the nitrification layer on the inner surface of the upper portion of the trench and on the outer surface of the substrate.

### Claim 5 (depends on 4)

The method as claimed in claim 4 further comprising a step of removing the oxidation layer which is free of being covered by the hemispherical silicon grains.

### Claim 6 (depends on 5)

The method as claimed in claim 5 further comprising a step of removing a portion of the inner surface of the lower portion of the trench which is free of the hemispherical silicon grains and the oxidation layer.

### Claim 7 (depends on 6)

The method as claimed in claim 6 further comprising a step of removing the oxidation layer which is covered by the hemispheric silicon grains, wherein the hemispherical silicon grains are removed simultaneously during the step of removing the portion of the inner surface of the lower portion of the trench which is free of the hemispherical silicon grains and the oxidation layer.

### Claim 8 (depends on 1)

The method as claimed in claim 1 further comprising:
a step of forming a oxidation layer on the inner surface of the lower portion of the trench and a bottom surface of the trench.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein the oxidation layer forming step is performed by proceeding a thermal oxidation process.

### Claim 10 (depends on 8)

The method as claimed in claim 8, wherein multiple hemispherical silicon grains are formed on the oxidation layer on the inner surface of the lower portion of the trench and on the outer surface of the substrate.

### Claim 11 (depends on 10)

The method as claimed in claim 10 further comprising a step of removing the oxidation layer which is free of being covered by the hemispherical silicon grains.

### Claim 12 (depends on 11)

The method as claimed in claim 11 further comprising a step of removing a portion of the inner surface of the lower portion of the trench which is free of the hemispherical silicon grains and the oxidation layer.

### Claim 13 (depends on 12)

The method as claimed in claim 12 further comprising a step of removing the oxidation layer which is covered by the hemispheric silicon grains, wherein the hemispherical silicon grains are removed simultaneously during the step of removing the portion of the inner surface of the lower portion of the trench which is free of the hemispherical silicon grains and the oxidation layer.