# US 2008/0305601 A1 · Method for forming semiconductor device using multi-functional sacrificial dielectric layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305601 A1
- Document ID: US20080305601A1
- Status: Published application
- Kind: A1
- Application number: 11/758,897
- Filed: 2007-06-06
- Published: 2008-12-11
- Earliest claimed: 2007-06-06
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Jyh-Huei Chen
- Web page: https://patentgrep.com/patent/US20080305601A1

## CPC

- H10P 30/204: {into Group IV semiconductors}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10P 30/208: {of electrically inactive species}
- H10D 64/663: {the additional layers comprising a silicide layer contacting the layer of silicon, e.g. polycide gates}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A composite dielectric layer including a nitride layer over an oxide layer serves the dual function of acting as an SMT (stress memorization technique) film while an annealing operation is carried out and then remains partially intact as it is patterned to further serve as an RPO film during a subsequent silicidation process. The need to form and remove two separate dielectric material layers is obviated. The nitride layer protects the oxide layer to alleviate oxide damage during a pre-silicidation PAI (pre-amorphization implant) process thereby preventing oxide attack during a subsequent HF dip operation and preventing nickel silicide spiking through the attacked oxide layer during silicidation.

## Claims

### Claim 1

A method for forming a semiconductor device, said method comprising;
forming a gate structure over a semiconductor substrate; and
forming a dielectric material over said semiconductor substrate including over said gate structure and maintaining said dielectric material over said semiconductor substrate including over said gate structure during a rapid thermal annealing operation and maintaining said dielectric material over at least portions of said semiconductor substrate and said gate structure during a silicidation operation, while shielding other portions of at least one of said semiconductor substrate and said gate structure during said silicidation operation.

### Claim 2 (depends on 1)

The method as in claim 1, wherein said dielectric material comprises a composite layer of a silicon nitride layer over an oxide layer.

### Claim 3 (depends on 2)

The method as in claim 2, wherein said silicon nitride layer is formed to include a tensile stress and impart a stress upon a channel disposed beneath said gate structure.

### Claim 4 (depends on 1)

The method as in claim 1, wherein said forming a dielectric material comprises forming at least one stressed film, and
said forming a dielectric material and said maintaining said dielectric material over said semiconductor substrate including over said gate structure during a rapid thermal annealing operation comprise stressing a channel disposed beneath said gate structure.

### Claim 5 (depends on 1)

The method as in claim 1, further comprising maintaining said dielectric material over said portions of said gate structure and said semiconductor substrate during a pre-amorphization implant carried out before said silicidation and in which said pre-amorphization implant at least partially amorphizes exposed silicon surfaces in said other portions but does not damage said dielectric material.

### Claim 6 (depends on 5)

The method as in claim 5, wherein said pre-amorphization implant includes an implant energy of at least 15 KeV, a dose of at least 2E13, and includes implanting at least one of argon, gallium, indium, germanium, and thallium,

### Claim 7 (depends on 5)

The method as in claim 5, wherein said dielectric material comprises a composite layer of a silicon nitride layer over an oxide layer and further comprising contacting said substrate with a wet HF solution while maintaining said dielectric material over portions of said gate structure and said semiconductor substrate and prior to said siliciding.

### Claim 8 (depends on 1)

The method as in claim 1, wherein said dielectric material is maintained over said semiconductor substrate but not said gate structure during said silicidation operation and wherein said silicidation operation comprises forming a nickel silicide on exposed portions of said gate structure.

### Claim 9

A method for forming a semiconductor device, said method comprising:
forming a gate structure over a semiconductor substrate;
forming a dielectric composite over said semiconductor substrate including over said gate structure, and maintaining said dielectric composite thereover during rapid thermal annealing;
removing said dielectric composite from first areas to be silicided thereby forming a patterned dielectric composite over second areas not to be silicided;
performing a pre-amorphization implant process with said patterned dielectric composite in place; and
forming silicides in said first areas during a silicidation process with said dielectric composite preventing silicidation in said second areas during said silicidation process,

### Claim 10 (depends on 9)

The method as in claim 9, wherein said pre-amorphization implant includes implanting at least one of argon, gallium, indium, germanium, and thallium.

### Claim 11 (depends on 9)

The method as in claim 9, wherein said pre-amorphization implant includes an implant energy of at least 15 KeV and an implant dose of at least 2E13 and at least partially amorphizes exposed silicon surfaces in said first areas.

### Claim 12 (depends on 9)

The method as in claim 9, wherein said forming a dielectric composite comprises forming at least one stressed film and said forming a dielectric material and said maintaining comprise stressing a channel disposed beneath said gate structure.

### Claim 13 (depends on 9)

The method as in claim 9, wherein said forming a dielectric composite comprises forming a layer of silicon nitride over an oxide layer.

### Claim 14 (depends on 13)

The method as in claim 13, wherein said silicon nitride layer is formed to include a tensile stress and impart a stress upon a channel disposed beneath said gate structure.

### Claim 15 (depends on 13)

The method as in claim 13, wherein said oxide layer is formed by chemical vapor deposit and includes a thickness of at least 50 angstroms and said silicon nitride includes a thickness of at least 300 angstroms.

### Claim 16 (depends on 13)

The method as in claim 13, wherein said removing comprises plasma etching said silicon nitride and terminating said plasma etching using automatic endpointing techniques, and wet etching to remove said oxide layer.

### Claim 17 (depends on 13)

The method as in claim 13, further comprising contacting said substrate with a wet HF solution after said pre-amorphization implant and prior to said forming a silicide and wherein said pre-amorphization implant and said exposing said substrate to said wet HF solution does not attack said oxide layer.

### Claim 18 (depends on 9)

The method as in claim 9, wherein said silicides comprise nickel silicide.

### Claim 19 (depends on 9)

The method as in claim 9, wherein said rapid thermal annealing includes a maximum temperature within the range of 1100-1200° C.

### Claim 20 (depends on 9)

The method as in claim 9, wherein said forming silicides in said first areas with said dielectric composite preventing silicidation in said second areas, comprises forming a metal film over said patterned dielectric composite and said semiconductor substrate including said gate structure, then heating.