# US 2008/0305600 A1 · Method and apparatus for fabricating high tensile stress film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305600 A1
- Document ID: US20080305600A1
- Status: Published application
- Kind: A1
- Application number: 11/758,623
- Filed: 2007-06-05
- Published: 2008-12-11
- Earliest claimed: 2007-06-05
- Assignees: United Microelectronics Corp.
- Inventors: Hsiu-Lien Liao; Neng-Kuo Chen; Teng-Chun Tsai; Yi-Wei Chen
- Web page: https://patentgrep.com/patent/US20080305600A1

## CPC

- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/0223: {having source and drain regions or source and drain extensions self-aligned to sides of the gate}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method and an apparatus for fabricating a high tensile stress film includes providing a substrate, forming a poly stressor on the substrate, and performing an ultra violet rapid thermal process (UVRTP) for curing the poly stressor and adjusting its tensile stress status, thus the poly stressor serves as a high tensile stress film. Due to a combination of energy from photons and heat, the tensile stress status of the high tensile stress film is adjusted in a relatively shorter process period or under a relatively lower temperature.

## Claims

### Claim 1

A method for fabricating a poly stressor, the method comprising:
providing a substrate having at least a transistor formed thereon;
forming a poly stressor on the substrate; and
performing an ultra violet rapid thermal process (UVRTP) for curing the poly stressor and adjusting a tensile stress of the poly stressor.

### Claim 2 (depends on 1)

The method of claim 1, wherein the poly stressor comprises silicon nitride, silicon oxide, or silicon oxynitride.

### Claim 3 (depends on 1)

The method of claim 1, wherein a tensile-stress status of an as-deposition of the poly stressor is lower than 1.5 GPa.

### Claim 4 (depends on 1)

The method of claim 1, wherein the UVRTP is performed at a temperature between 150-800° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the UVRTP is performed for a duration of 0-60 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the UVRTP is performed under a pressure between 3-500 mTorr.

### Claim 7 (depends on 1)

The method of claim 1, wherein an ultra violet light used in the UVRTP has a wavelength in a range of 100-400 nm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the UVRTP further comprises introducing a nitrogen gas.

### Claim 9 (depends on 1)

The method of claim 1, wherein the UVRTP further comprises introducing an inert gas.

### Claim 10 (depends on 1)

The method of claim 1, wherein the step of curing the poly stressor and the step of adjusting the tensile stress of the poly stressor are simultaneously completed in the UVRTP.

### Claim 11 (depends on 1)

The method of claim 1, wherein a tensile-stress status of the high tensile stress film after performing the UVRTP is between 0.5-3.0 GPa.

### Claim 12 (depends on 1)

The method of claim 1, wherein the transistor is an N-channel Metal-Oxide-Semiconductor (NMOS) transistor.

### Claim 13 (depends on 1)

The method of claim 1 further comprises steps of forming the transistor on the substrate:
forming a gate structure on the substrate;
forming a spacer on sidewalls of the gate structure; and
forming a source/drain region in the substrate surrounding the spacers.

### Claim 14 (depends on 13)

The method of claim 13, wherein the poly stressor is formed after forming the source/drain region.

### Claim 15 (depends on 1)

The method of claim 1 further comprising a step of removing the poly stressor after performing the UVRTP.

### Claim 16

A method for fabricating a contact etch stop layer (CESL), the method comprising:
providing a substrate having at least a gate, a spacer and a source/drain region formed thereon;
forming a metal layer on the substrate;
performing a rapid thermal annealing (RTA) process to form intergraded salicide layers on the gate and the source/drain region respectively;
forming a CESL on the substrate; and
performing an ultra violet rapid thermal process (UVRTP) for curing the CESL and adjusting a tensile stress of the CESL.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal layer comprises a metal or an alloy of a metal from a set of metals comprising Co, Ti, Ni, W, Pt, Pd, and Mo.

### Claim 18 (depends on 16)

The method of claim 16, wherein the RTA process is performed at a temperature between 400-600° C.

### Claim 19 (depends on 16)

The method of claim 16, wherein the CESL comprises silicon nitride, silicon oxide, or silicon oxynitride.

### Claim 20 (depends on 16)

The method of claim 16, wherein a tensile-stress status of an as-deposition of the CESL is lower than 1.5 GPa.

### Claim 21 (depends on 16)

The method of claim 16, wherein the UVRTP is performed at a temperature between 150-800° C.

### Claim 22 (depends on 16)

The method of claim 16, wherein the UVRTP is performed for a duration of 0-60 minutes.

### Claim 23 (depends on 16)

The method of claim 16, wherein the UVRTP is performed under a pressure between 3-500 mTorr.

### Claim 24 (depends on 16)

The method of claim 16, wherein an ultra violet light used in the UVRTP has a wavelength in a range of 100-400 nm.

### Claim 25 (depends on 16)

The method of claim 16, wherein the UVRTP further comprises introducing a nitrogen gas.

### Claim 26 (depends on 16)

The method of claim 16, wherein the UVRTP further comprises introducing an inert gas.

### Claim 27 (depends on 16)

The method of claim 16, wherein a tensile-stress status of the CESL after performing the UVRTP is between 0.5-3.0 GPa.

### Claim 28 (depends on 16)

The method of claim 16, wherein the RTA process and the UVRTP are performed in-situ or ex-situ.

### Claim 29 (depends on 16)

The method of claim 16, wherein the UVRTP is used to transform the intergraded salicide layers into salicide layers.

### Claim 30

A method for fabricating a high tensile stress film, the method comprising:
providing a substrate having at least a gate, a spacer and a source/drain region formed thereon;
forming a first high tensile stress film on the substrate;
performing a first ultra violet rapid thermal process (UVRTP) for simultaneously curing the first high tensile stress film and adjusting a tensile stress of the first high tensile stress film;
removing the first high tensile stress film;
forming a metal layer on the substrate;
performing a rapid thermal annealing (RTA) process to form intergraded salicide layers on the gate and the source/drain region respectively;
forming a second high tensile stress film on the substrate; and
performing a second UVRTP for curing the second high tensile stress film and adjusting a tensile stress of the second high tensile stress film.

### Claim 31 (depends on 30)

The method of claim 30, wherein the first high tensile stress film and the second high tensile stress film comprise silicon nitride, silicon oxide, or silicon oxynitride.

### Claim 32 (depends on 30)

The method of claim 30, wherein tensile-stress statuses of an as-deposition of the first high tensile stress film and the second high tensile stress film are lower than 1.5 GPa.

### Claim 33 (depends on 30)

The method of claim 30, wherein the first UVRTP and the second UVRTP are performed at a temperature between 150-800° C.

### Claim 34 (depends on 30)

The method of claim 30, wherein the first UVRTP and the second UVRTP are performed for a duration of 0-60 minutes.

### Claim 35 (depends on 30)

The method of claim 30, wherein the first UVRTP and the second UVRTP are performed under a pressure between 3-500 mTorr.

### Claim 36 (depends on 30)

The method of claim 30, wherein an ultraviolet light used in the first UVRTP and the second UVRTP has a wavelength in a range of 100-400 nm.

### Claim 37 (depends on 30)

The method of claim 30, wherein the first UVRTP and the second UVRTP further comprise a step of introducing a nitrogen gas or an inert gas.

### Claim 38 (depends on 30)

The method of claim 30, wherein a tensile-stress status of the first high tensile stress film after performing the first UVRTP is between 0.5-3.0 GPa.

### Claim 39 (depends on 30)

The method of claim 30, wherein the metal layer comprises a metal or an alloy of a metal from a set of metals comprising Co, Ti, Ni, W, Pt, Pd, and Mo.

### Claim 40 (depends on 30)

The method of claim 30, wherein the RTA process is performed at a temperature between 400-600° C.

### Claim 41 (depends on 30)

The method of claim 30, wherein a tensile-stress status of the second high tensile stress film after performing the second UVRTP is between 0.5-3.0 GPa.

### Claim 42 (depends on 30)

The method of claim 30, wherein the second high tensile stress film serves as a contact etch stop layer (CESL).

### Claim 43 (depends on 30)

The method of claim 30, wherein the first UVRTP, the second UVRTP, and the RTA process are performed in-situ or ex-situ.

### Claim 44 (depends on 30)

The method of claim 30, wherein the second UVRTP is used to transform the intergraded salicide layers into salicide layers.

### Claim 45 (depends on 30)

The method of claim 30, wherein the transistor is an N-channel Metal-Oxide-Semiconductor (NMOS) transistor.

### Claim 46

An ultra violet rapid thermal process (UVRTP) apparatus comprising:
a chamber for accommodating a wafer;
a holder positioned in the chamber for holding the wafer; and
an ultra violet light source and heating devices comprising a UV light source and a heating source.

### Claim 47 (depends on 46)

The apparatus of claim 46, wherein the UV light source provides an ultraviolet light having a wavelength between 100-400 nm.

### Claim 48 (depends on 47)

The apparatus of claim 47 further comprising a shutter element for controlling an access of the ultra violet light.

### Claim 49 (depends on 46)

The apparatus of claim 46, wherein the heating source comprises a halogen lamp or a laser source.

### Claim 50 (depends on 46)

The apparatus of claim 46 further comprising a temperature sensor for sensing a temperature of the wafer.

### Claim 51 (depends on 46)

The apparatus of claim 46, wherein the holder comprises a heating function.