# US 2008/0305590 A1 · High performance cmos devices and methods for making same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305590 A1
- Document ID: US20080305590A1
- Status: Published application
- Kind: A1
- Application number: 12/191,868
- Filed: 2008-08-14
- Published: 2008-12-11
- Earliest claimed: 2004-11-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chih-Hao Wang; Ta-Wei Wang; Chenming Hu
- Web page: https://patentgrep.com/patent/US20080305590A1

## CPC

- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 30/0218: {having pocket halo regions selectively formed at the sides of the gates}
- H10D 30/022: {having lightly-doped source or drain extensions selectively formed at the sides of the gates}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 62/314: {having vertical doping variations (vertical IGFETs H10D30/63)}
- H10D 64/015: {removing at least parts of gate spacers, e.g. disposable spacers}
- H10D 30/0212: {using self-aligned silicidation}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

An integrated circuit having high performance CMOS devices with good short channel effects may be made by forming a gate structure over a substrate; forming pocket implant regions and source/drain extensions in the substrate; forming spacers along sides of the gate structure; and thermal annealing the substrate when forming the spacers, the thermal annealing performed at an ultra-low temperature. An integrated circuit having high performance CMOS devices with low parasitic junction capacitance may be made by forming a gate structure over a substrate; forming pocket implant regions and source/drain extensions in the substrate; forming spacers along sides of the gate structure; performing a low dosage source/drain implant; and performing a high dosage source/drain implant.

## Claims

### Claim 1

A method of manufacturing an integrated circuit, the method comprising the steps of:
forming a gate structure over a substrate;
forming pocket implant regions and source/drain extensions in the substrate;
forming spacers along sides of the gate structure; and
thermal annealing the substrate when forming the spacers, the thermal annealing performed at an ultra-low temperature.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the gate structure comprises a gate conductor composed of a material selected from the group consisting of poly-Si, poly SiGe, metal, metal oxide, metal nitride, silicide and combinations thereof

### Claim 3 (depends on 1)

The method according to claim 1, wherein the ultra-low temperature is between about 350° C. and about 800° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the thermal annealing step is performed for a time period of between about 5 seconds and about 700 minutes.

### Claim 5

A method of manufacturing an integrated circuit, the method comprising the steps of:
forming a gate structure over a substrate;
forming source/drain extensions in the substrate; and
performing a thermal cycle process for solid phase epitaxy on the substrate.

### Claim 6 (depends on 5)

The method according to claim 5, further comprising the step of thermal annealing the substrate at an ultra-low temperature.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the ultra-low temperature is between about 350° C. and about 800° C.

### Claim 8 (depends on 5)

The method according to claim 5, further comprising the step of forming pocket implant regions in the substrate.

### Claim 9 (depends on 8)

The method according to claim 8, further comprising the step of thermal annealing the substrate at an ultra-low temperature.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the ultra-low temperature is between about 350° C. and about 800° C.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the step of forming pocket implant regions in the substrate is performed prior to the step of forming source/drain implant regions in the substrate.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the thermal annealing step is performed after the step of forming the pocket implant regions and before the step of forming the source/drain extensions.

### Claim 13 (depends on 6)

The method according to claim 6, wherein the thermal annealing step is performed after the step of performing a thermal cycle process for solid phase epitaxy.

### Claim 14

A method of manufacturing an integrated circuit, the method comprising the steps of:
forming a gate structure over a substrate;
forming a super halo-shape pocket implant region in the substrate;
forming thin, off-set spacers along sides of the gate structure; and
forming source/drain extensions in the substrate.

### Claim 15

A method of manufacturing an integrated circuit, the method comprising the steps of:
forming a gate structure over a substrate;
forming pocket implant regions and source/drain extensions in the substrate;
forming spacers along sides of the gate structure;
performing a low dosage source/drain implant; and
performing a high dosage source/drain implant.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the low dosage source/drain implant is performed at a high energy.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the high energy comprises less than 150 kev.

### Claim 18 (depends on 15)

The method according to claim 15, wherein the low dosage source/drain implant is performed with a dopant dosage of less than 1E15 cm−2.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the high dosage source/drain implant is performed with a dopant dosage of greater than 1E14 cm−2.

### Claim 20 (depends on 15)

The method according to claim 15, wherein the high dosage source/drain implant is performed with a dopant dosage of greater than 1E14 cm−2.