# US 2008/0305569 A1 · Semiconductor Device and a Method of Manufacturing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305569 A1
- Document ID: US20080305569A1
- Status: Published application
- Kind: A1
- Application number: 12/174,124
- Filed: 2008-07-16
- Published: 2008-12-11
- Earliest claimed: 1999-03-26
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Masaya Kadono; Shunpei Yamazaki; Yukio Yamauchi; Hidehito Kitakado
- Web page: https://patentgrep.com/patent/US20080305569A1

## CPC

- H10D 86/40: characterised by multiple TFTs
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6715: {characterised by the doping profiles, e.g. having lightly-doped source or drain extensions}
- H10D 86/0221: {comprising manufacture, treatment or patterning of TFT semiconductor bodies}
- H10D 86/0223: {comprising crystallisation of amorphous, microcrystalline or polycrystalline semiconductor materials}
- H10D 86/0231: {using masks, e.g. half-tone masks}
- H10D 86/421: {having a particular composition, shape or crystalline structure of the active layer}
- H10D 86/451: {characterised by the compositions or shapes of the interlayer dielectrics}
- H10D 86/60: wherein the TFTs are in active matrices
- H10K 59/124: Insulating layers formed between TFT elements and OLED elements
- H10K 59/873: {Encapsulations}
- H10K 59/874: {including getter material or desiccant}
- H10W 76/60: Seals
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A reduction in contaminating impurities in a TFT, and a TFT which is reliable, is obtained in a semiconductor device which uses the TFT. By removing contaminating impurities residing in a film interface of the TFT using a solution containing fluorine, a reliable TFT can be obtained.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A method of manufacturing an active matrix display device, comprising steps of:
forming a semiconductor film over a substrate having an insulating surface;
forming a patterned resist mask over said semiconductor film;
patterning said semiconductor film to form at least one semiconductor island;
removing the patterned resist mask located over said semiconductor island;
spinning the substrate after removing the patterned resist mask;
applying an etching solution to a surface of said semiconductor island and scattering the etching solution during said spinning, thereby contaminating impurities are removed from the surface of the semiconductor island by the step of applying the etching solution; and then
forming a gate insulating film over said semiconductor island after the contaminating impurities are removed from the surfaces by the step of applying the etching solution;
forming a gate electrode over said gate insulating film,
forming an insulating film over the gate insulating film and the gate electrode, and
forming a pixel electrode over the insulating film, wherein the pixel electrode is electrically connected to the semiconductor island.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the semiconductor island comprises crystal structure.

### Claim 17 (depends on 15)

The method according to claim 15, wherein said etching solution is selected from the group consisting of hydrofluoric acid, dilute hydrofluoric acid, ammonium fluoride, buffered hydrofluoric acid (BHF), hydrofluoric acid and aqueous hydrogen peroxide (FPM), and a solution mixture including ammonium hydrofluoride (NH4HF2) and ammonium fluoride (NH4F) (LAL500).

### Claim 18 (depends on 15)

The method according to claim 15, wherein the contaminating impurity is at least one element selected from periodic table group 1 elements or periodic table group 2 elements.

### Claim 19 (depends on 15)

The method according to claim 15, wherein the contaminating impurity element is at least one element selected from the group consisting of Na, K, Mg, Ca, and Ba.

### Claim 20 (depends on 15)

The method according to claim 15, wherein the contaminating impurity is removed by an acidic solution containing fluorine.

### Claim 21 (depends on 15)

The method according to claim 15, wherein the active matrix display device is one selected from the group consisting of a liquid crystal display device, an electro-luminescence display device, and an EC display device.

### Claim 22

A method of manufacturing an active matrix display device, comprising steps of:
forming a semiconductor film over a substrate having an insulating surface;
forming a patterned resist mask over said semiconductor film;
patterning said semiconductor film to form at least one semiconductor island;
removing the patterned resist mask located over said semiconductor island;
spinning the substrate after removing the patterned resist mask;
applying an etching solution to a surface of said semiconductor island and scattering the etching solution during said spinning, thereby contaminating impurities are removed from the surface of the semiconductor island by the step of applying the etching solution;
forming a gate insulating film over said semiconductor island after the contaminating impurities are removed from the surface of the semiconductor island;
spinning the substrate having the gate insulating film;
applying an etching solution to a surface of said gate insulating film and scattering the etching solution during said spinning, thereby contaminating impurities are removed from the surface of the gate insulating film by the step of applying the etching solution;
forming a gate electrode over said gate insulating film after the contaminating impurities are removed from the surface of the gate insulating film,
forming an insulating film over the gate insulating film and the gate electrode, and
forming a pixel electrode over the insulating film, wherein the pixel electrode is electrically connected to the semiconductor island.

### Claim 23 (depends on 22)

The method according to claim 22, wherein the semiconductor island comprises crystal structure.

### Claim 24 (depends on 22)

The method according to claim 22, wherein said etching solution is selected from the group consisting of hydrofluoric acid, dilute hydrofluoric acid, ammonium fluoride, buffered hydrofluoric acid (BHF), hydrofluoric acid and aqueous hydrogen peroxide (FPM), and a solution mixture including ammonium hydrofluoride (NH4HF2) and ammonium fluoride (NH4F) (LAL500).

### Claim 25 (depends on 22)

The method according to claim 22, wherein the contaminating impurity is at least one element selected from periodic table group 1 elements or periodic table group 2 elements.

### Claim 26 (depends on 22)

The method according to claim 22, wherein the contaminating impurity element is at least one element selected from the group consisting of Na, K, Mg, Ca, and Ba.

### Claim 27 (depends on 22)

The method according to claim 22, wherein the contaminating impurity is removed by an acidic solution containing fluorine.

### Claim 28 (depends on 22)

The method according to claim 22, wherein the active matrix display device is one selected from the group consisting of a liquid crystal display device, an electro-luminescence display device, and an EC display device.

### Claim 29

A method of manufacturing an active matrix display device, comprising steps of:
forming a gate wiring over a substrate having an insulating surface;
spinning the substrate;
applying an etching solution to surfaces of said substrate and said gate wiring and scattering the etching solution during said spinning, thereby contaminating impurities are removed from the surface of the wiring and the insulating surface by the step of applying the etching solution; and then
forming a gate insulating film and a semiconductor film over said gate wiring after the contaminating impurities are removed from the surfaces.

### Claim 30 (depends on 29)

The method according to claim 29, wherein said etching solution is selected from the group consisting of hydrofluoric acid, dilute hydrofluoric acid, ammonium fluoride, buffered hydrofluoric acid (BHF), hydrofluoric acid and aqueous hydrogen peroxide (FPM), and a solution mixture including ammonium hydrofluoride (NH4HF2) and ammonium fluoride (NH4F) (LAL500).

### Claim 31 (depends on 29)

The method according to claim 29, wherein the contaminating impurity is at least one element selected from periodic table group 1 elements or periodic table group 2 elements.

### Claim 32 (depends on 29)

The method according to claim 29, wherein the contaminating impurity element is at least one element selected from the group consisting of Na, K, Mg, Ca, and Ba.

### Claim 33 (depends on 29)

The method according to claim 29, wherein the contaminating impurity is removed by an acidic solution containing fluorine.

### Claim 34 (depends on 29)

The method according to claim 29, wherein the active matrix display device is one selected from the group consisting of a liquid crystal display device, an electro-luminescence display device, and an EC display device.

### Claim 35

A method of manufacturing an active matrix display device, comprising steps of:
forming a gate wiring over a substrate having an insulating surface;
spinning the substrate;
applying an etching solution to surfaces of said substrate and said gate wiring and scattering the etching solution during said spinning, thereby contaminating impurities are removed from the surface of the wiring and the insulating surface by the step of applying the etching solution; and then
forming a gate insulating film and a semiconductor film over said gate wiring, continuously after the contaminating impurities are removed from the surfaces.

### Claim 36 (depends on 35)

The method according to claim 35, wherein said etching solution is selected from the group consisting of hydrofluoric acid, dilute hydrofluoric acid, ammonium fluoride, buffered hydrofluoric acid (BHF), hydrofluoric acid and aqueous hydrogen peroxide (FPM), and a solution mixture including ammonium hydrofluoride (NH4HF2) and ammonium fluoride (NH4F) (LAL500).

### Claim 37 (depends on 35)

The method according to claim 35, wherein the contaminating impurity is at least one element selected from periodic table group 1 elements or periodic table group 2 elements.

### Claim 38 (depends on 35)

The method according to claim 35, wherein the contaminating impurity element is at least one element selected from the group consisting of Na, K, Mg, Ca, and Ba.

### Claim 39 (depends on 35)

The method according to claim 35, wherein the contaminating impurity is removed by an acidic solution containing fluorine.

### Claim 40 (depends on 35)

The method according to claim 35, wherein the active matrix display device is one selected from the group consisting of a liquid crystal display device, an electro-luminescence display device, and an EC display device.