# US 2008/0305567 A1 · Nitride-based light emitting device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305567 A1
- Document ID: US20080305567A1
- Status: Published application
- Kind: A1
- Application number: 12/192,360
- Filed: 2008-08-15
- Published: 2008-12-11
- Earliest claimed: 2005-08-09
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: June O. Song
- Web page: https://patentgrep.com/patent/US20080305567A1

## CPC

- H10H 20/833: Transparent materials
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A light emitting device according to an exemplary embodiment of the present invention includes: an n-type cladding layer; a p-type cladding layer; an active layer interposed between the n-type cladding layer and the p-type cladding layer; and an ohmic contact layer contacting the p-type cladding layer or the n-type cladding layer and comprising a first film that comprises a transparent conductive zinc oxide having a one-dimensional nano structure, wherein the one-dimensional nano structure is at least one selected from a nano-column, a nano rod, and a nano wire.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A method of manufacturing a light emitting device, the method comprising:
forming an n-type cladding layer, an active layer, and a p-type cladding layer on a substrate;
forming a transparent conductive zinc oxide film of an ohmic contact layer, the zinc oxide film having a nano structure; and
heat treating the zinc oxide film.

### Claim 12 (depends on 11)

The method of claim 11, wherein the formation of the zinc oxide film comprising:
depositing a two-dimensional thin film of zinc oxide; and
etching and re-growing the two-dimensional thin film under an atmosphere including a hydrogen gas.

### Claim 13 (depends on 11)

The method of claim 11, wherein the zinc oxide film comprises at least one of aluminum (Al), chromium (Cr), silicon (Si), germanium (Ge), indium (In), lithium (Li), gallium (Ga), magnesium (Mg), zinc (Zn), beryllium (Be), molybdenum (Mo), vanadium (V), copper (Cu), iridium (Ir), rhodium (Rh), ruthenium (Ru), tungsten (W), cobalt (Co), nickel (Ni), manganese (Mn), titanium (Ti), tantalum (Ta), cadmium (Cd), lanthanum (La), and oxides thereof.

### Claim 14 (depends on 11)

The method of claim 11, further comprising:
forming an ohmic interlayer under the zinc oxide film,
wherein the ohmic interlayer comprises at least one of metals including Ni, Pd, Pt, Rh, Zn, In, Sn, Ag, Au, Cd, Mg, Be, Mo, V, Cu, Ti, Ir, Ru, W, Co, Mn, and La, transparent conductive oxides including ITO, SnO2, ZnO, In2O3, Ga2O3, RhO2, NiO, CoO, PdO, PtO, CuAlO2, CdO, and CuGaO2, and transparent conductive nitrides including TiN, TaN, and SiNx.

### Claim 15 (depends on 14)

The method of claim 14, further comprising:
performing heat treatment after the formation of the ohmic interlayer and before the formation of the zinc oxide film.

### Claim 16 (depends on 15)

The method of claim 15, wherein the heat treatment before the formation of the zinc oxide film is performed at a temperature equal to or lower than about 800° C. and under a vacuum or under an atmosphere of oxygen (O2), nitrogen (N2), argon (Ar), hydrogen (H2), or air.

### Claim 17 (depends on 11)

The method of claim 11, further comprising:
performing plasma treatment on the zinc oxide film by using ions of such as oxygen (O2), nitrogen (N2), hydrogen (H2), or argon (Ar) at a temperature equal to or lower than about 800° C.