# US 2008/0305566 A1 · Silicon Nanocrystal Embedded Silicon Oxide Electroluminescence Device with a Mid-Bandgap Transition Layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305566 A1
- Document ID: US20080305566A1
- Status: Published application
- Kind: A1
- Application number: 12/197,045
- Filed: 2008-08-22
- Published: 2008-12-11
- Earliest claimed: 2004-03-15
- Assignees: Sharp Laboratories of America, Inc.
- Inventors: Jiandong Huang; Pooran Chandra Joshi; Hao Zhang; Apostolos T. Voutsas
- Web page: https://patentgrep.com/patent/US20080305566A1

## CPC

- C23C 16/30: Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C 16/24: Deposition of silicon only
- C23C 16/401: {containing silicon}
- C23C 16/505: using radio frequency discharges
- C23C 16/56: After-treatment
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3461: {Nanoparticles}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method is provided for forming a silicon (Si) nanocrystal embedded Si oxide electroluminescence (EL) device with a mid-bandgap transition layer. The method provides a highly doped Si bottom electrode, and forms a mid-bandgap electrically insulating dielectric film overlying the electrode. A Si nanocrystal embedded SiOx film layer is formed overlying the mid-bandgap electrically insulating dielectric film, where X is less than 2, and a transparent top electrode overlies the Si nanocrystal embedded SiOx film layer. The bandgap of the mid-bandgap dielectric film is about half that of the bandgap of the Si nanocrystal embedded SiOx film. In one aspect, the Si nanocrystal embedded SiOx film has a bandgap (Eg) of about 10 electronvolts (eV) and mid-bandgap electrically insulating dielectric film has a bandgap of about 5 eV. By dividing the high-energy tunneling processes into two lower energy tunneling steps, potential damage due to high power hot electrons is reduced.

## Claims

### Claim 1

A method for forming a silicon (Si) nanocrystal embedded Si oxide electroluminescence (EL) device with a mid-bandgap transition layer, the method comprising:
providing a highly doped Si bottom electrode;
forming a mid-bandgap electrically insulating dielectric film overlying the Si bottom electrode;
forming a Si nanocrystal embedded SiOx film overlying the mid-bandgap electrically insulating dielectric film, where X is less than 2;
forming a transparent top electrode overlying the Si nanocrystal embedded SiOx film; and,
where the bandgap of the mid-bandgap electrically insulating dielectric film is about half that of the bandgap of the Si nanocrystal embedded SiOx film.

### Claim 2 (depends on 1)

The method of claim 1 wherein forming the Si nanocrystal embedded SiOx film includes forming a Si nanocrystal embedded SiOx film having a bandgap (Eg) of about 10 electronvolts (eV); and,
wherein forming the mid-bandgap electrically insulating dielectric film includes forming a mid-bandgap electrically insulating dielectric film having a bandgap of about 5 eV.

### Claim 3 (depends on 2)

The method of claim 2 wherein forming the mid-bandgap electrically insulating dielectric film includes forming a silicon nitride (SiNy) film, having a bandgap of about 5 eV, where Y is about 4/3.

### Claim 4 (depends on 3)

The method of claim 3 wherein forming the SiNy film includes forming a SiNy film having a thickness in a range of 1 to 30 nanometers (nm).

### Claim 5 (depends on 1)

The method of claim 1 wherein forming the Si nanocrystal embedded SiOx film includes depositing the film using a high density plasma-enhanced chemical vapor deposition (HDPECVD) process.

### Claim 6 (depends on 5)

The method of claim 5 wherein forming the Si nanocrystal embedded SiOx film using the HDPECVD process includes:
subsequent to depositing a SiOx film layer, annealing; and,
in response, embedding Si nanocrystals in the SiOx film layer.

### Claim 7 (depends on 6)

The method of claim 6 wherein depositing the Si nanocrystal embedded SiOx film includes:
introducing silane (SiH4) in a range of about 20 to 40 standard cubic centimeters (SCCM);
introducing N2O in a range of about 15 to 35 SCCM;
supplying power to a top electrode at a frequency in a range of 13.56 to 300 megahertz (MHz), and a power density in a range of about 1 to 20 watts per square centimeter (W/cm2); and,
supplying power to a bottom electrode at a frequency in a range of 50 kilohertz to 13.56 MHz, and a power density in a range of about 1 to 5 W/cm2.

### Claim 8 (depends on 7)

The method of claim 7 wherein annealing the Si insulating film includes annealing:
for a duration in a range of about 10 to 120 minutes; and,
at a temperature in a range of about 500 to 1100° C.

### Claim 9 (depends on 7)

The method of claim 7 wherein forming the Si nanocrystal embedded SiOx film includes forming a Si nanocrystal embedded SiOx film having emission wavelength in a range of 600 to 1100 nm with a spectral width of about 150 nm (Full Width at Half Magnitude), responsive to ratio of SiH4 and N2O in the HDPECVD deposition process.

### Claim 10 (depends on 5)

The method of claim 5 wherein depositing the Si nanocrystal embedded SiOx film using the HDPECVD process includes using a plasma concentration of greater than 1×1011 cm−3, with an electron temperature of less than 10 eV.

### Claim 11 (depends on 1)

The method of claim 1 wherein forming the Si nanocrystal embedded SiOx film includes forming the Si nanocrystal embedded SiOx film with Si nanocrystals having a diameter in a range of about 2 to 10 nm.

### Claim 12 (depends on 1)

The method of claim 1 wherein forming the Si nanocrystal embedded SiOx film includes forming the SiOx film with a thickness is a range of 20 to 300 nm.

### Claim 13 (depends on 3)

The method of claim 3 wherein forming the SiNy film includes depositing the SiNy film using a PECVD process.

### Claim 14

A method for operating a silicon (Si) nanocrystal embedded Si oxide electroluminescence (EL) device with a mid-bandgap transition layer, the method comprising:
providing an EL device with a highly doped Si bottom electrode, a mid-bandgap electrically insulating dielectric film overlying the Si bottom electrode, a Si nanocrystal embedded SiOx film overlying the mid-bandgap electrically insulating dielectric film, where X is less than 2, and a transparent top electrode overlying the Si nanocrystal embedded SiOx film, and wherein the mid-bandgap electrically insulating dielectric film has a bandgap of about half that of the Si nanocrystal embedded SiOx film;
biasing with EL device with a voltage of less than 10 volts; and,
generating a surface emission power of greater than 0.03 watts per square meter (W/m2).

### Claim 15 (depends on 14)

The method of claim 14 wherein the EL device has an emission wavelength in a range of 600 to 1100 nm with a spectral width of about 150 nm (Full Width at Half Magnitude).

### Claim 16 (depends on 14)

The method of claim 14 wherein providing the EL device includes providing an EL device with a mid-bandgap electrically insulating dielectric film having a bandgap (Eg) of about 5 electronvolts (eV) and a Si nanocrystal embedded SiOx film having a bandgap of about 10 eV.

### Claim 17 (depends on 16)

The method of claim 16 wherein providing the EL device includes providing an EL device with a silicon nitride (SiNy) mid-bandgap electrically insulating dielectric film having a bandgap of about 5 eV, where Y is about 4/3.

### Claim 18 (depends on 17)

The method of claim 17 wherein providing the EL device with the SiNy mid-bandgap electrically insulating dielectric film includes providing an EL device with a SiNy film having a thickness in a range of 1 to 30 nanometers (nm).

### Claim 19 (depends on 14)

The method of claim 14 wherein providing the EL device includes providing an EL device with a Si nanocrystal embedded SiOx film having Si nanocrystals with a diameter in a range of about 2 to 10 nm.

### Claim 20 (depends on 14)

The method of claim 14 wherein providing the EL device includes providing an EL device with a Si nanocrystal embedded SiOx film having a thickness is a range of 20 to 300 nm.