# US 2008/0305560 A1 · Method for eliminating defects from semiconductor materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305560 A1
- Document ID: US20080305560A1
- Status: Published application
- Kind: A1
- Application number: 11/810,561
- Filed: 2007-06-06
- Published: 2008-12-11
- Earliest claimed: 2007-06-06
- Assignees: OPC Laser Systems LLC
- Inventors: Joseph Reid Henrichs
- Web page: https://patentgrep.com/patent/US20080305560A1

## CPC

- H10P 95/408: {of Group III-V semiconductors, e.g. to render them semi-insulating}
- H10P 14/3414: {being group IIIA-VIA materials}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10P 95/904: {of Group III-V semiconductors}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Using a helium cryostat, the temperature for a substrate wafer(s) is reduced to 2.2 Kelvin over a period of twenty-four hours. Next, a soak segment will hold the temperature of the substrate wafer at 2.2 Kelvins for a period of ninety-six hours. At these low temperatures, alloys such as GaAs, InP, and GaP will form dipole molecular moments, which will re-align along lines of internal magnetic force as molecular bonds condense. Next the substrate wafer's temperature is ramped up to room temperature over a period of twenty-four hours. Next, the temperature of the substrate wafer is ramped up to assure that the temperature gradients made to occur within the wafer are kept low. Typically, a temper ramp up temperature will range between 300° F. to 1100° F. and depends upon the single crystal material used to construct the substrate wafer. Next, the substrate wafer undergoes a temper hold segment, which assures that the entire substrate wafer has had the benefit of the tempering temperature. A typical temper hold segment is around 3 hours and depends upon the material, thickness, and diameter size of the substrate wafer.

## Claims

### Claim 1

A method of cryogenically treating substrate wafers constructed from material taken from columns III-V of the periodic table, comprising:
(a) lowering the temperature of a substrate wafer to cryogenic levels,
(b) holding said temperature of said wafer at said cryogenic levels,
(c) bringing the temperature of said wafer back up to room temperature,
(d) elevating the temperature of said wafer to above ambient,
(e) holding said temperature of said wafer for a period,
(f) returning the temperature of said wafer to said room temperature,
whereby the cryogenic treatment of said substrate wafers provides for the elimination of point, dislocation, vacancy, and other crystallographic defects from said substrate wafers.