# US 2008/0305447 A1 · Time-delayed activation of zeolite heating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305447 A1
- Document ID: US20080305447A1
- Status: Published application
- Kind: A1
- Application number: 12/123,740
- Filed: 2008-05-20
- Published: 2008-12-11
- Earliest claimed: 2007-06-06
- Assignees: Honeywell International Inc.
- Inventors: MARK R. WHEELER; Milton E. McDonnell; Maria M. Higuera; Michael Jablon; Richard B. Heath; Lee R. Mores
- Web page: https://patentgrep.com/patent/US20080305447A1

## CPC

- A61K 8/26: Aluminium; Compounds thereof
- A61K 8/60: Sugars; Derivatives thereof
- A61Q 19/10: Washing or bathing preparations
- A61K 2800/242: Exothermic; Self-heating; Heating sensation
- A61K 2800/412: Microsized, i.e. having sizes between 0.1 and 100 microns
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61Q: SPECIFIC USE OF COSMETICS OR SIMILAR TOILETRY PREPARATIONS

## Abstract

The invention relates to zeolite particles which are at least partially coated with a coating that is capable of delaying the release of heat from the zeolite particles upon contact with water over time. The coating effectively at least partially blocks the pore structure of the zeolite particle from contact with water, thereby delaying contact between water and the zeolite, and prolonging the warming effect caused by such contact.

## Claims

### Claim 1

A time-delayed heat-release coated zeolite particle comprising a zeolite particle at least partially coated with a coating comprising a mixture of:
a) at least one water-soluble component which is at least partially soluble in water at temperatures of from about 15° C. to about 25° C.; and
b) at least one water-insoluble component which is substantially insoluble in water at temperatures of from about 15° C. to about 25° C.;
wherein the coating has a melting temperature of from about 45° C. to about 120° C., and wherein the coating is capable of dissolving in water at temperatures of from about 15° C. and 25° C. in an amount sufficient to at least partially expose the zeolite particle to the water.

### Claim 2 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1, wherein the zeolite particle is coated such that the coating becomes at least partially dissolved at a time of from about 1 minute to about 60 minutes upon contact with water.

### Claim 3 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the coating composition is thermally stable at temperatures of up to about 130° C.

### Claim 4 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the zeolite particle comprises a 3A zeolite, a 4A zeolite, a 5A zeolite or combinations thereof.

### Claim 5 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the water-soluble component comprises sucrose, glucose, fructose, amylose, amylopectin, polyethylene glycol, taurates, glutamates, fatty esters of ethylene glycol, mono- and/or divalent salts of an alkali or alkaline earth metal and a halide or nonmetal oxide, di- or tri-block copolymers of ethylene oxide and propylene oxide, or combinations thereof.

### Claim 6 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the water-soluble component comprises sucrose.

### Claim 7 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the water-insoluble component comprises a saccharide ester, an esterified polyol, a wax, or combinations thereof.

### Claim 8 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the water-insoluble component comprises sucrose octyl stearate.

### Claim 9 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the zeolite particle is substantially entirely coated with the coating composition.

### Claim 10 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the zeolite particle is less than entirely coated with the coating composition.

### Claim 11 (depends on 1)

The time-delayed heat-release coated zeolite particle of claim 1 wherein the coating composition has a thickness of from about 0.1 μm to about 10 μm.

### Claim 12 (depends on 1)

A carrier composition which comprises a plurality of time-delayed heat-release coated zeolite particles of claim 1.

### Claim 13 (depends on 12)

The carrier composition of claim 12, which comprises an anhydrous, fluid, cosmetically acceptable carrier composition

### Claim 14 (depends on 13)

The carrier composition of claim 13, which comprises a self-heating facial cleanser composition.

### Claim 15

A process for heating a fluid composition which comprises:
I) providing a fluid composition which comprises a plurality of time-delayed heat-release coated zeolite particles, each comprising a zeolite particle at least partially coated with a coating comprising a mixture of:
a) at least one water-soluble component which is at least partially soluble in water at temperatures of from about 15° C. to about 25° C.; and
b) at least one water-insoluble component which is substantially insoluble in water at temperatures of from about 15° C. to about 25° C.;
wherein the coating has a melting temperature of from about 45° C. to about 120° C., and wherein the coating is capable of dissolving in water at temperatures of from about 15° C. and 25° C. in an amount sufficient to at least partially expose the zeolite particle to the water; and
II) contacting the fluid composition with water to thereby at least partially dissolve the coatings of the time-delayed heat-release coated zeolite particles, thus exposing the zeolite particles to the water such that the zeolite particles generate heat.

### Claim 16 (depends on 15)

The process of claim 15 wherein the fluid composition comprises an anhydrous, cosmetically acceptable carrier composition.

### Claim 17 (depends on 16)

The process of claim 16 wherein the fluid composition comprises a self-heating facial cleanser composition.

### Claim 18

A process for forming time-delayed heat-release coated zeolite particles comprising:
I) forming a coating composition for coating zeolite particles, which comprises a mixture of:
a) at least one water-soluble component which is at least partially soluble in water at temperatures of from about 15° C. to about 25° C.; and
b) at least one water-insoluble component which is substantially insoluble in water at temperatures of from about 15° C. to about 25° C.;
II) heating the coating composition during or after step I, thereby forming a molten coating composition;
III) coating zeolite particles with the molten coating composition; and
IV) cooling the molten coating composition to thereby form time-delayed heat-release coated zeolite particles having a coating, which coating has a melting temperature of from about 45° C. to about 120° C., and which coating is capable of dissolving in water at temperatures of from about 15° C. and 25° C. in an amount sufficient for the zeolite particles to be at least partially exposed to the water.

### Claim 19 (depends on 18)

The process of claim 18 wherein steps I and II are conducted simultaneously.

### Claim 20 (depends on 18)

The process of claim 18 wherein steps I, II, and III are conducted simultaneously.

### Claim 21 (depends on 18)

The process of claim 18 wherein the coating of step III comprises dipping the zeolite particles into the molten coating composition.

### Claim 22 (depends on 18)

The process of claim 18 wherein the coating of step III comprises spray coating the molten coating composition onto the zeolite particles.

### Claim 23 (depends on 18)

The process of claim 18 wherein the coating of step III is conducted in a fluidized bed reactor.

### Claim 24 (depends on 18)

The process of claim 18 wherein step III comprises combining the molten coating composition with zeolite particles, thereby forming a fluid zeolite composite; and wherein step IV comprises cooling the fluid zeolite composite to thereby form a zeolite composite, followed by a separating of the zeolite composite into time-delayed heat-release coated zeolite particles.

### Claim 25 (depends on 18)

The process of claim 18 wherein the zeolite composite is separated by grinding.

### Claim 26

A time-delayed heat-release coated zeolite particle comprising a zeolite particle partially coated with a water-insoluble coating, which coating comprises: a water-insoluble component comprising a crystalline or semicrystalline material having a glass transition temperature of about 40° C. or greater, and a melting point of about 150° C. or lower.

### Claim 27 (depends on 26)

The time-delayed heat-release coated zeolite particle of claim 26 wherein the water-insoluble component comprises a saccharide ester, an esterified polyol, a wax, or combinations thereof.

### Claim 28 (depends on 26)

The time-delayed heat-release coated zeolite particle of claim 26 wherein the water-insoluble coating comprises sucrose octyl stearate.

### Claim 29

A process for heating a fluid composition which comprises:
I) providing a fluid composition which comprises a plurality of time-delayed heat-release coated zeolite particles, each comprising a zeolite particle partially coated with a water-insoluble coating which comprises a water-insoluble component comprising a crystalline or semicrystalline material having a glass transition temperature of about 40° C. or greater, and a melting point of about 150° C. or lower; and
II) contacting the fluid composition with water to thereby partially expose the zeolite particles to the water such that the zeolite particles generate heat.

### Claim 30

A process for forming time-delayed heat-release coated zeolite particles comprising:
I) forming a water-insoluble coating composition for coating zeolite particles, which comprises a water-insoluble component comprising a crystalline or semicrystalline material having a glass transition temperature of about 40° C. or greater, and a melting point of about 150° C. or lower;
II) heating the coating composition during or after step I, thereby forming a molten water-insoluble coating composition;
III) coating zeolite particles with the molten water-insoluble coating composition; and
IV) cooling the molten coating composition to thereby form time-delayed heat-release coated zeolite particles having a water-insoluble coating, which coating is sufficient to partially expose the zeolite particles to water.