# US 2008/0305392 A1 · Surface treated steel sheet for battery case, battery case and battery using the case

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305392 A1
- Document ID: US20080305392A1
- Status: Published application
- Kind: A1
- Application number: 12/190,917
- Filed: 2008-08-13
- Published: 2008-12-11
- Earliest claimed: 2002-04-22
- Assignees: Toyo Kohan Co., Ltd.; Browdy and Neimark, P.L.L.C.
- Inventors: Hitoshi OHMURA; Tatsuo Tomomori; Yoshitaka Honda
- Web page: https://patentgrep.com/patent/US20080305392A1

## CPC

- C23C 10/28: using solids, e.g. powders, pastes
- C23C 12/02: Diffusion in one step
- C23C 18/00: Chemical coating by decomposition of either liquid compounds or solutions of the coating forming compounds, without leaving reaction products of surface material in the coating; Contact plating
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- C25D 5/50: by heat-treatment
- H01M 50/119: Metals
- H01M 50/124: having a layered structure
- H01M 50/1245: {characterised by the external coating on the casing}
- H01M 50/128: with two or more layers of only inorganic material
- H01M 50/133: Thickness
- Y02E 60/10: Energy storage using batteries
- Y10T 428/12937: Co- or Ni-base component next to Fe-base component
- Y10T 428/12944: Ni-base component
- Y10T 428/12951: Fe-base component
- Y10T 428/12972: Containing 0.01-1.7% carbon [i.e., steel]
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A surface treated steel sheet for a battery case, which has a diffusion layer of a nickel-phosphorus alloy or a nickel-cobalt-phosphorus alloy formed on the outermost layer of the inside surface of a plated steel sheet for a battery case; a battery case which is produced through forming the surface-treated steel sheet having a diffusion layer of a nickel-phosphorus alloy or a nickel-cobalt-phosphorus alloy by the deep drawing method, the DI forming or the DTR forming: and a battery using the battery case. The battery case can be used for producing a battery excellent in battery characteristics.

## Claims

### Claim 1

A surface treated steel sheet for a battery case in which a diffusion layer of a nickel-phosphorus alloy is formed at a surface on the inner side of the battery case.

### Claim 2 (depends on 1)

The surface treated steel sheet for a battery case of claim 1 in which an iron-nickel diffusion layer is formed as a lower layer and said diffusion layer of a nickel-phosphorus alloy is formed as an upper layer at the surface on the inner side, and an iron-nickel diffusion layer is formed as a lower layer and a nickel layer is formed as an upper layer at the surface on the outer side of the battery case.

### Claim 3 (depends on 1)

The surface treated steel sheet for a battery case of claim 1 in which an iron-nickel diffusion layer is formed as a lower layer, a nickel layer is formed as an intermediate layer and said diffusion layer of a nickel-phosphorus alloy is formed as an upper layer at the surface on the inner side, and an iron-nickel diffusion layer is formed as a lower layer and a nickel layer is formed as an upper layer at the surface on the outer side of the battery case.

### Claim 4 (depends on 1)

The surface treated steel sheet for a battery case according to claim 1, wherein the diffusion layer of the nickel-phosphorus alloy contains Ni3P.

### Claim 5 (depends on 1)

The surface treated steel sheet for a battery case according to claim 1, wherein the thickness of the nickel-phosphorus alloy is within a range from 0.1 to 2 μm.

### Claim 6 (depends on 1)

The surface treated steel sheet for a battery case according to claim 1, wherein the phosphorus content in the nickel-phosphorus alloy is within a range from 1 to 12% by weight.

### Claim 7 (depends on 1)

The surface treated steel sheet for a battery case of claim 1 in which an iron-nickel diffusion layer is formed as a lower layer and said diffusion layer of a nickel-cobalt-phosphorus alloy is formed as an upper layer at the surface on the inner side, and an iron-nickel diffusion layer is formed as a lower layer and a nickel layer is formed as an upper layer at the surface on the outer side of a battery case.

### Claim 8 (depends on 1)

The surface treated steel sheet for a battery case of claim 1 in which an iron-nickel diffusion layer is formed as a lower layer, a nickel layer is formed as an intermediate layer, and said diffusion layer of a nickel-cobalt-phosphorus alloy is formed as an upper layer at the surface an the inner side, and an iron-nickel diffusion layer is formed as a lower layer and a nickel layer is formed as an upper layer at the surface on the outer side of the battery case.

### Claim 9

A battery case in which a diffusion layer of a nickel-phosphorus alloy is formed on the inner side.

### Claim 10 (depends on 9)

The battery case of claim 9 in which an iron-nickel diffusion layer is formed as a lower layer and said nickel-phosphorus alloy layer is formed as an upper layer on the inner side and an iron-nickel diffusion layer is formed as a lower layer and a nickel layer is formed as an upper layer on the outer side.

### Claim 11 (depends on 9)

The battery case of claim 9 in which an iron-nickel diffusion layer is formed as a lower layer, a nickel layer is formed as an intermediate layer and said nickel-phosphorus alloy layer is formed as an upper layer on the inner side and an iron-nickel diffusion layer is formed as a lower layer and a nickel layer is formed as an upper layer on the outer.

### Claim 12 (depends on 9)

The surface treated steel sheet for a battery case according to claim 9, wherein the diffusion layer of the nickel-phosphorus alloy contains Ni3P.

### Claim 13 (depends on 9)

The surface treated steel sheet for a battery case according to a claim 9, wherein the phosphorus content in the nickel-phosphorus alloy is within a range from 1 to 12% by weight.

### Claim 14 (depends on 9)

The battery case according to claim 9, which is obtained by a drawing forming method, DI forming method or DTR forming method.

### Claim 15 (depends on 9)

The battery using a battery case according to claim 9 and filling a positive electrode active substance and a negative electrode active substance to the inside of the battery case.