# US 2008/0305355 A1 · Plastic electronic component package

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305355 A1
- Document ID: US20080305355A1
- Status: Published application
- Kind: A1
- Application number: 12/220,543
- Filed: 2008-07-25
- Published: 2008-12-11
- Earliest claimed: 2006-12-12
- Assignees: Quantum Leap Packaging, Inc.
- Inventors: Michael A. Zimmerman; Keith Smith; Jacob Shverdin
- Web page: https://patentgrep.com/patent/US20080305355A1

## CPC

- H10F 39/804: {Containers or encapsulations}
- H10F 39/011: {Manufacture or treatment of image sensors covered by group H10F39/12}
- H10W 70/479: {on or in insulating or insulated package substrates, interposers, or redistribution layers}
- H10W 74/127: {characterised by arrangements for sealing or adhesion}
- H10W 76/60: Seals
- H10H 20/8506: {Containers}
- H10W 72/581: {Auxiliary members, e.g. flow barriers}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 90/754: {between a chip and a stacked insulating package substrate, interposer or RDL}
- Y10T 428/12569: Synthetic resin
- Y10T 428/12618: Plural oxides
- Y10T 428/31678: Of metal
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A plastic package for an image sensor or other electronic component which comprises a plastic body, preferably of LCP material, molded around a leadframe and defining a cavity in which the image sensor is to be disposed. A lid assembly is provided having a transparent glass lid retained in a plastic lid frame which is weldable or otherwise bondable to the plastic body of the package to enclose the image sensor mounted in the cavity. The leadframe is usually composed of copper or a copper alloy, or a ferrous alloy having a copper coating. An interfacial layer is formed on the surfaces of the leadframe at least in those portions which are in contact with the plastic body which serves to provide substantially improved adhesion between the leadframe and the plastic material to achieve a hermetic bond between the metal and plastic materials. The interfacial layer is composed of a cuprous oxide base layer formed on a surface of the leadframe, and a cupric oxide layer formed on the cuprous oxide layer. The cupric oxide outer layer has an acicular structure which provides an interlocking mechanism for adhesion to the plastic material molded thereto in forming the package.

## Claims

### Claim 1

A hermetic seal between a metal element and a plastic element comprising:
an intermediate layer between the metal element and the plastic element, the intermediate layer having:
a layer of a first oxide formed on a surface of the metal element; and
a layer of a second oxide formed on the layer of a first oxide, the second oxide layer having an acicular structure bondable to the plastic element.

### Claim 2 (depends on 1)

The hermetic seal of claim 1 wherein:
the first oxide is an oxide of the metal material of the metal element; and
the second oxide is a different oxide form of the first oxide.

### Claim 3 (depends on 2)

The hermetic seal of claim 2 wherein:
the metal element has a copper surface at least in the area bondable to the plastic element;
the first oxide is cuprous oxide and the second oxide is cupric oxide.

### Claim 4

For use in fabricating a hermetic seal between a high temperature plastic part molded to a copper part, the copper part comprising:
a first layer of cuprous oxide formed on the surfaces of the copper part at least at the portions to be molded to the high temperature plastic part; and
a second layer of cupric oxide formed on the first layer of cuprous oxide and having an acicular structure bondable to the high temperature plastic part.

### Claim 5

A method of fabricating a component having a metal part and a plastic part, the method comprising the steps of:
providing a metal part;
providing on at least a portion of the surfaces of the metal part an interfacial layer of oxide material; and
molding a high temperature thermoplastic part around the portion of the metal part having the interfacial layer.

### Claim 6 (depends on 5)

The method of claim 5 wherein the thermoplastic part is an LCP material containing hydroquinine (HQ), teraphalic acid, isophalic acid, 2,6 naphalene, dicarboxyclic acid, 4-hydrobenzoic acid (HBA), bisphenol or biphenol (BP), and hydroxynaphthoic acid;
and filler particles of at least one of the group consisting of talc, glass fiber, milled glass and flake glass.

### Claim 7 (depends on 6)

The method of claim 6 wherein the filler particles are in the range of 10-50% by weight.

### Claim 8 (depends on 7)

The method of claim 7 wherein at least some of the filler particles have a particle size in the range of about 50-350 microns.

### Claim 9 (depends on 5)

The method of claim 5 wherein the step of providing an interfacial layer includes providing a first oxide on at least a portion of the surfaces of the metal part, and providing a second oxide on the first oxide.

### Claim 10 (depends on 9)

The method of claim 9 wherein the step of providing the interfacial layer includes providing the interfacial layer on the entire surface of the metal part;
and further including the step of removing the exposed portions of the interfacial layer from the metal part after molding the high temperature thermoplastic part.

### Claim 11 (depends on 5)

The method of claim 5 wherein the metal part is copper and wherein the interfacial layer is copper oxide material.

### Claim 12 (depends on 5)

The method of claim 5 wherein the step of molding comprises injection molding the high temperature thermoplastic part.

### Claim 13 (depends on 5)

The method of claim 5 wherein the thermoplastic part is an LCP material.

### Claim 14

A component having a metal part and a plastic part comprising:
a high temperature plastic part molded to a metal part; and
a metal part having on at least a portion of the surfaces thereof which are molded to the plastic part an interfacial layer of material effective to improve the adhesion of the high temperature plastic frame to the metal leadframe.

### Claim 15 (depends on 14)

The component of claim 14 wherein the metal part is composed of copper;
and wherein an interfacial layer is formed on at least the surfaces of the metal part in contact with the plastic part, the interfacial layer composed of a cuprous oxide layer formed on the surface of the metal part and a cupric oxide layer formed on the surface of the cuprous oxide layer.

### Claim 16 (depends on 14)

The component of claim 14 wherein the interfacial layer has:
a first layer formed on a surface of the metal part; and
a second layer formed on a surface of the first layer, the second layer having a surface bonded to the high temperature plastic part.

### Claim 17 (depends on 16)

The component of claim 16 wherein the metal part has a copper surface;
the interfacial layer has a first layer of cuprous oxide formed on the copper surface of the metal part; and
a layer of cupric oxide formed on a surface of the cuprous layer, the cupric layer having an acicular structure bonded to the high temperature plastic part.

### Claim 18 (depends on 14)

The component of claim 14 wherein the plastic part is a high temperature LCP material.

### Claim 19 (depends on 14)

The component of claim 14 wherein the LCP material has a melting temperature greater than about 300° C.

### Claim 20 (depends on 14)

The component of claim 14 wherein the LCP material has a melting temperature greater than about 200° C.

### Claim 21 (depends on 14)

The component of claim 14 wherein the LCP material contains filler particles to provide a CTE compatible with that of the metal part.

### Claim 22 (depends on 21)

The component of claim 21 wherein the CTE of the LCP material is in the range of about 6-25 ppm/° C.

### Claim 23 (depends on 21)

The component of claim 21 wherein the filler particles are of nano size.

### Claim 24 (depends on 21)

The component of claim 21 wherein the filler particles are in the range of about 10-17% by weight.

### Claim 25 (depends on 14)

The component of claim 14 wherein the metal part is copper.

### Claim 26 (depends on 14)

The component of claim 14 wherein the metal part is a copper alloy.

### Claim 27 (depends on 14)

The component of claim 14 wherein the metal part is a ferrous metal having copper su.