# US 2008/0305351 A1 · Method For Inhibiting the Crystallization of Boric Acid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305351 A1
- Document ID: US20080305351A1
- Status: Published application
- Kind: A1
- Application number: 10/593,936
- Filed: 2005-03-24
- Published: 2008-12-11
- Earliest claimed: 2004-03-24
- Inventors: David M. Schubert
- Web page: https://patentgrep.com/patent/US20080305351A1

## CPC

- C09K 21/02: Inorganic materials
- D21H 17/65: Acid compounds
- D21H 21/34: Ignifugeants
- D21H 21/36: Biocidal agents, e.g. fungicidal, bactericidal, insecticidal agents
- Y10T 428/31989: Of wood
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for inhibiting the crystallization of boric acid is provided. Boric acid is dissolved in water and a vitrifying agent, such as an amino alcohol or amino acid, to form an aqueous mixture which is then dried to form a vitreous boric acid-containing residue. This mixture, when applied to a surface and allowed to dry on the surface, forms a vitreous boric acid-containing coating which is readily adherent to the surface, or if allowed to penetrate into a porous substrate, deposits a vitreous boric acid-containing residue within the substrate upon drying. The vitreous boric acid-containing residue provides beneficial properties, including for example improved fire retardancy and biocidal protection, to a variety of materials such as cotton batting, cellulose, and wood and paper products and gypsum wallboard.

## Claims

### Claim 1

A method for inhibiting the crystallization of boric acid comprising the steps of dissolving a source of boric acid in water and a vitrifying agent selected from the group consisting of amino alcohols and amino acids to form an aqueous mixture and allowing the aqueous mixture to dry, thereby forming a vitreous boric acid-containing residue.

### Claim 2 (depends on 1)

The method of claim 1 wherein the mole ratio of the vitrifying agent to boric acid is above about 0.25:1 and below about 1:1 and wherein the aqueous mixture is applied to a surface of a substrate before it is allowed to dry, thereby forming a vitreous boric acid-containing residue on and/or in the substrate.

### Claim 3 (depends on 1)

The method of claim 1 wherein the mole ratio of the vitrifying agent to boric acid is in the range of from about 0.3:1 to about 1:1.

### Claim 4 (depends on 1)

The method of claim 1 wherein the vitrifying agent is selected from the group consisting of 2-amino-2-methyl-1-propanol, ethanolamine, tris(hydroxylmethyl)aminomethane, 5-aminopentanol, and lysine.

### Claim 5 (depends on 1)

The method of claim 1 wherein the boric acid-containing residue is a solid.

### Claim 6 (depends on 1)

The method of claim 1 wherein the boric acid-containing residue is a viscous fluid.

### Claim 7 (depends on 1)

The method according to claim 1 wherein the aqueous mixture is applied to cotton batting, wood, wood products, engineered wood, paper, cellulose insulation or gypsum wallboard.

### Claim 8 (depends on 2)

The method according to claim 2 wherein the vitreous boric acid-containing residue forms a coating on the surface of the substrate.

### Claim 9 (depends on 8)

The method according to claim 8 wherein the coating is a hard vitreous boric acid-containing layer.

### Claim 10 (depends on 8)

The method according to claim 8 wherein the coating is a tacky vitreous boric acid-containing layer.

### Claim 11 (depends on 2)

The method according to claim 2 wherein the aqueous mixture penetrates into the substrate and dries within the substrate, thereby depositing a vitreous boric acid-containing residue within the substrate.

### Claim 12

A method for protecting a combustible material against fire comprising the steps of: (a) dissolving a source of boric acid in water and a vitrifying agent selected from the group consisting of amino alcohols and amino acids to form an aqueous mixture; (b) applying the aqueous mixture to a surface of the combustible material; and (c) allowing the aqueous mixture to dry such that a vitreous boric acid-containing residue is deposited on the surface of the combustible material and/or within the combustible material, thereby enhancing the fire retardant nature of the combustible material.

### Claim 13 (depends on 12)

The method according to claim 12 wherein the combustible material is cotton batting.

### Claim 14 (depends on 13)

The method according to claim 13 wherein the cotton batting is heated after the aqueous mixture is applied.

### Claim 15 (depends on 12)

A fire retardant article comprising a combustible material and further comprising a vitreous boric acid-containing residue, prepared according to the method of claim 12.

### Claim 16

A method for protecting wood or lignocellulosic-based products against decay and insect attack comprising the steps of: (a) dissolving a source of boric acid in water and a vitrifying agent selected from the group consisting of amino alcohols and amino acids to form an aqueous mixture; (b) applying the aqueous mixture to the wood or lignocellulosic-based product; (c) allowing the aqueous mixture to penetrate into the wood or lignocellulosic-based product; and (d) allowing the aqueous mixture to dry within the substrate, depositing a vitreous boric acid-containing residue, thereby providing protection against decay and insect attack.

### Claim 17 (depends on 16)

An article comprising wood or lignocellulosic-based material and further comprising a vitreous boric acid-containing residue, prepared according to the method of claim 16.

### Claim 18 (depends on 21)

The composition according to claim 21 wherein the vitrifying agent is 2-amino-2-methyl-1-propanol.

### Claim 19 (depends on 18)

The composition of claim 18 wherein the concentration of boric acid is in the range of about 35% to 57% by weight.

### Claim 20 (depends on 19)

The composition of claim 19 wherein the mole ratio of 2-amino-2-methyl-1-propanol to boric acid is at least about 0.3:1 and the concentration of boric acid is up to about 50% by weight.

### Claim 21

An aqueous composition comprising boric acid, a vitrifying agent and water wherein the vitrifying agent is selected from the group consisting of 2-amino-2-methyl-1-propanol, tris(hydroxylmethyl)aminomethane, 5-aminopentanol, and lysine and the mole ratio of the vitrifying agent to boric acid is above about 0.25:1 and below about 1:1.

### Claim at position 22

22-23. (canceled)