# US 2008/0305284 A1 · Inkjet Recording Element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305284 A1
- Document ID: US20080305284A1
- Status: Published application
- Kind: A1
- Application number: 11/570,898
- Filed: 2005-06-13
- Published: 2008-12-11
- Earliest claimed: 2004-07-08
- Inventors: Olivier J. Poncelet
- Web page: https://patentgrep.com/patent/US20080305284A1

## CPC

- B41M 5/5218: {characterised by inorganic additives, e.g. pigments, clays}
- C01B 33/26: Aluminium-containing silicates {, i.e. silico-aluminates}
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

The present invention relates to an inkjet recording element having good stability to light and ozone over time. Said recording element comprises a support and at least one ink-receiving layer, said ink-receiving layer comprising at least one hydrosoluble binder and at least one fibrous aluminosilicate polymer obtainable a preparation method consisting in a controlled hydrolysis of aluminum halide and silicon alcoxide, and in a heat treatment in the presence of silanol groups for sufficient time to form the fibrous aluminosilicate polymer.

## Claims

### Claim 1

1) An inkjet recording element, comprising a support and at least one ink-receiving layer, wherein said ink-receiving layer comprises at least one hydrosoluble binder and one polymeric inorganic material based on silicon and aluminum comprising more than 80 moles % of a fibrous aluminosilicate of formula AlxSiyOz in which the ratio x:y is between 1 and 3, and z is between 2 and 6.

### Claim 2 (depends on 1)

2) The recording element according to claim 1, wherein said polymeric inorganic material is obtainable by a preparation method that comprises the following steps:
a) treating a mixed aluminum and silicon alcoxide, or a mixed aluminum and silicon precursor, with an aqueous alkali, whilst maintaining the pH between 4 and 6.5, the aluminum concentration being maintained between 5.104 and 1 mol/l and the Al/Si molar ratio being maintained between 1 and 3;
b) heating the mixture obtained in step a) at a temperature below the boiling point of water, in the presence of silanol groups for sufficient time to obtain a complete reaction of forming the polymeric inorganic material; and
c) material the byproducts formed during steps a) and b) are eliminated from the reaction medium.

### Claim 3 (depends on 1)

3) The recording element according to claim 1, wherein part of the silicon is replaced by a metal selected from the group consisting of titanium, zirconium and tin.

### Claim 4 (depends on 1)

4) The recording element according to claim 1, wherein the alkali of step a) to prepare the aluminosilicate polymer is selected from the group consisting of sodium and potassium hydroxide.

### Claim 5 (depends on 1)

5) The recording element according to claim 1, wherein the amount of silanol groups used in step b) corresponds to a ratio between aluminum atoms and silanol groups of less than 2.25.1010.

### Claim 6 (depends on 5)

6) The recording element according to claim 5, wherein the amount of silanol groups used in step b) corresponds to a ratio between aluminum atoms and silanol groups of less than 1.0.1010.

### Claim 7 (depends on 1)

7) The recording element according to claim 1, wherein the Al/Si molar ratio is between 1.5 and 2.5.

### Claim 8 (depends on 1)

8) The recording element according to claim 1, wherein in step a) the pH is maintained at between 4.5 and 5.5.

### Claim 9 (depends on 1)

9) The recording element according to claim 1, wherein in step b) the heating is at a temperature between about 70° C. and 98° C.

### Claim 10 (depends on 1)

10) The recording element according to claim 1, wherein the mixed aluminum and silicon precursor is the product of the hydrolysis (i) of one compound selected from the group consisting of aluminum salts, aluminum alcoxides and aluminum halogenoalcoxides and (ii) at least one compound selected from the group consisting of silicon alcoxides and chloroalcoxides.

### Claim 11 (depends on 10)

11) The recording element according to claim 10, wherein said mixed aluminum and silicon precursor is the product of the hydrolysis (i) of an aluminum halide and (ii) a silicon alcoxide.

### Claim 12 (depends on 11)

12) The recording element according to claim 11, wherein said silicon alcoxide is tetramethyl orthosilicate or tetraethyl orthosilicate.

### Claim 13 (depends on 1)

13) The recording element according to claim 1, wherein said ink-receiving layer comprises between 5 percent and 95 percent by weight of said polymeric inorganic material compared with the total weight of the dry receiving layer.

### Claim 14 (depends on 1)

14) The recording element according to claim 1, wherein said hydrosoluble binder is gelatin or polyvinyl alcohol.

### Claim 15

15) The use of a polymeric inorganic material based on silicon and aluminum comprising more than 80 moles % of a fibrous aluminosilicate of formula AlxSiyOz in which the ratio x:y is between 1 and 3, and z is between 2 and 6 as receiving agent in an ink-receiving layer of an inkjet recording element, said ink-receiving layer comprising at least one hydrosoluble binder.