# US 2008/0305274 A1 · Process for coating metal sheets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305274 A1
- Document ID: US20080305274A1
- Status: Published application
- Kind: A1
- Application number: 12/228,580
- Filed: 2008-08-14
- Published: 2008-12-11
- Earliest claimed: 2000-05-08
- Inventors: Georg Gros
- Web page: https://patentgrep.com/patent/US20080305274A1

## CPC

- C09D 133/062: {Copolymers with monomers not covered by C09D133/06}
- B05D 3/067: {Curing or cross-linking the coating}
- C08L 67/07: having terminal carbon-to-carbon unsaturated bonds
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method for coating sheet metals such as coils with a chromate-free, water-dilutable, organic, UV-curing anti-corrosive coating, and for curing the coating by irradiation with UV light. According to the method a dispersion or emulsion is provided as the UV-curing coating agent for forming the anti-corrosive coating that substantially consists of 25 to 80 wt.-% binder, 1 to 8 wt.-% photoinitiators, 0 to 5 wt. % additive, 20 to 70 wt. % water, and optionally a pigment. The coating agent is applied on the sheet metal, preferably in an inline method, dried to form a film and cured by UV light.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A method for coating a metal surface comprising the steps of:
applying a chromate-free, water-thinnable, organic UV-hardening corrosion-protection coating to the metal surface; and
curing the applied coating by irradiation with UV light to form a cured coating on said metal surface, wherein said coating is formed from a composition that is a dispersion or emulsion and comprises
from 25 to 80 wt. % of a binder calculated as total solids content of the composition;
from 1 to 8 wt. % of a photoinitiator;
at least some and up to 5 wt. % of at least one additive selected from the group consisting of a silane, a polydimethylsiloxane and a wax;
at least some and up to 70 wt. % water;
optionally an organic solvent; and
from 0.1 to 60 wt. % of a pigment;
wherein said binder comprises a base resin and from 1 to 15 wt. % measured as weight of the solids content of the composition of an elasticizing resin, wherein the total weight of the binder includes the weight of the elasticizing resin;
wherein said base resin is selected from the group consisting of an aqueous polyacrylate dispersion, an aqueous polyacrylate emulsion, an unsaturated acrylic ester resin, an urethane acrylic resin or any combination thereof, wherein the base resin is not an elasticizing resin;
wherein the elasticizing resin comprises at least one unsaturated aliphatic urethaneacrylate;
wherein said pigment has a mean particle diameter in the range from 0.001 to 10 μm; wherein said coating does not contain reactive thinners and the cured coating has a thickness of from 0.1 to 12 microns.

### Claim 14 (depends on 13)

A method according to claim 13, said binder comprises a resin selected from the group consisting of a polyacrylate resin and a urethane acrylic resin.

### Claim 15 (depends on 13)

A method according to claim 13, wherein said photoinitiator is selected from the group consisting of benzoin ether, benzoin isopropyl ether, benzil dimethyl ketal, 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-2-methyl-1-phenyl-1-propanone, benzophenones and 2,4,6-trimethylbenzoyldiphenylphosphine oxide.

### Claim 16 (depends on 13)

A method according to claim 13, wherein an elasticizing resin formed from an unsaturated aliphatic urethane acrylate prepolymer is added to the mixture as an additive.

### Claim 17 (depends on 13)

A method according to claim 13, wherein an emulsifier for the binder is added as an additive.

### Claim 18 (depends on 13)

A method according to claim 13, wherein at least two different pigments are added to the mixture.

### Claim 19 (depends on 13)

A method according to claim 13, wherein the corrosion-protection coating has a dry-film thickness in the range from 0.3 to 12 microns.

### Claim 20 (depends on 13)

A method according to claim 13, wherein the metal surface coated with the coating is dried at temperatures in the range from 50 to 100° C.

### Claim 21 (depends on 13)

A method according to claim 13, wherein the UV light is generated with mercury vapor lamps radiating in the range from 180 to 500 nm.

### Claim 22 (depends on 13)

A method according to claim 13, wherein the metal surface with the cured corrosion-protection coating is at least one of worked, cut or punched.

### Claim 23 (depends on 22)

A method according to claim 22, wherein the worked, cut or punched metal surface is joined to another structural element by clinching, bonding, welding or at least one further joining method.

### Claim 24 (depends on 19)

A method according to claim 19, wherein the dry-film thickness is from 0.5 to 8 microns.

### Claim 25 (depends on 19)

A method according to claim 19, wherein the dry film thickness is form 0.8 to 6 microns.

### Claim 26

A method comprising coating a metal surface with a chromate-free, water-thinnable, organic UV-hardening corrosion-protection coating and for curing the coating by irradiation with UV light, comprising applying a composition that is a dispersion or emulsion that is a UV-hardening coating agent for forming the corrosion-protection coating that comprises
from 25 to 80 wt. % of a binder calculated as total solids content of the composition, wherein the binder comprises a base resin and an elasticizing resin; wherein the base resin is selected from the group consisting of an aqueous polyacrylate dispersion, an aqueous polyacrylate emulsion, an unsaturated acrylic ester resin, a urethane acrylic resin or any combination thereof;
wherein the elasticizing resin comprises from 1 to 15 wt. % of the composition;
wherein at least some and up to 100 wt. % of the elastizing resin is at least an unsaturated aliphatic urethaneacrylate of up to 15 wt. % by weight of the composition;
wherein the base resin is not an elasticizing resin;
1 to 8 wt. % of a photoinitiator;
at least some and up to 5 wt. % of an additive selected from the group consisting of a silane, a dimethylsiloxane and a wax additives,
optionally an organic solvent; and at least some and up to 70 wt. % water;
at least one pigment; and
wherein said pigment content is added in the range from 0.1 to 60% by weight and wherein the pigment content is calculated in addition to the sum of said binder, said photoinitiator, said additive, said water and said optional organic solvent equals 100% by weight, wherein said pigment has a mean particle diameter in the range from 0.001 to 10 μm, wherein the aqueous dispersion or emulsion is without an addition of reactive thinners and wherein the coating agent is applied in a layer to the metal surface, dried to a film and hardened by means of UV light, in a thickness from 0.1 to 12 micrometers.

### Claim 27 (depends on 13)

The method of claim 13, wherein the metal surface is on a metal sheet.

### Claim 28 (depends on 26)

The method of claim 26, wherein the metal surface is on a metal sheet.

### Claim 29 (depends on 13)

The method of claim 13, wherein the metal surface is from a coiled metal.

### Claim 30 (depends on 26)

The method of claim 26, wherein the metal surface is from a coiled metal.

### Claim 31 (depends on 26)

The method of claim 26, wherein an in-line method is employed.

### Claim 32 (depends on 13)

The method of claim 13, wherein the cured coating has a thickness of 12 microns.

### Claim 33 (depends on 13)

The method of claim 13, wherein said additive is a silane.

### Claim 34 (depends on 13)

The method of claim 13, wherein said additive is a dimethylsiloxane.

### Claim 35 (depends on 13)

The method of claim 13, wherein said additive is a wax.

### Claim 36

A method comprising applying to a metal surface a chromate-free composition that is dispersion or emulsion comprising
25-80% by weight of a binder by total solids content of the chromate-free composition;
1 to 8 wt. % of a photoinitiator;
a lubricating agent;
at least some and up to 70% water; and
from 0.1 to 60 wt. % of a pigment,
wherein the binder comprises a base resin and an elasticizing resin, wherein the elasticizing resin is from 1 to 15% by weight of the composition,
wherein the base resin is an aqueous polyacrylate dispersion or emulsion, an unsaturated acrylic ester resin, a urethane acrylic resin or a combination thereof,
wherein the elasticizing resin comprises an amount of at least one unsaturated aliphatic urethaneacrylate,
wherein the pigment content is calculated in addition to the sum of the weight of said binder, said photoinitiator, and said lubricating agent equals 100% by weight and said pigment has a mean particle diameter of from 0.001 to 10 microns, and curing the applied composition by irradiation with UV light to form a cured coating on said metal surface, wherein said cured coating has a thickness from 0.1 to 12 micrometers, wherein the total weight of the binder includes the weight of the elasticizing resin; and wherein the base resin is not an elasticizing resin;

### Claim 37 (depends on 36)

The method of claim 36, wherein said dispersion or emulsion comprises a silane.

### Claim 38 (depends on 36)

The method of claim 36, wherein said dispersion or emulsion comprises a dimethylsiloxane.

### Claim 39 (depends on 36)

The method of claim 36, wherein said dispersion or emulsion comprises a wax.

### Claim 40

A method for coating a metal surface comprising the steps of:
applying a chromate-free composition that is, water-thinnable, organic UV-hardening corrosion-protection coating to the metal surface; and
curing the coating by irradiation with UV light to form a cured coating on said metal surface, wherein said coating is a dispersion or emulsion comprising
from 25 to 80 wt. % of a binder calculated as total solids content of the composition;
from 1 to 8 wt. % of a photoinitiator;
at least some and up to 5 wt. % of at least one additive selected from the group consisting of a silane, a dimethylsiloxane and a wax;
at least some and up to 70 wt. % water;
optionally an organic solvent;
from 0.1 to 60 wt. % of a pigment; and
wherein the binder comprises a base resin and an elasticizing resin, wherein the base resin is selected from the group consisting of an aqueous polyacrylate dispersion, an aqueous polyacrylate emulsion, an unsaturated acrylic ester resin, a urethane acrylic resin or any combination thereof,
wherein the elasticizing resin is present as from 1 to 15 wt. % of the composition;
wherein at least some and up to 100 wt. % of the elastizing resin is at least one unsaturated aliphatic urethaneacrylate;
wherein the pigment content is calculated in addition to the sum of the weight of said binder, said photoinitiator, said additive, said water and said optional organic solvent equals 100% by weight and said pigment has a mean particle diameter in the range from 0.001 to 10 μm; wherein said coating does not contain reactive thinners and has a thickness of from 0.1 to 12 micrometers, and wherein the total weight of the binder includes the weight of the elasticizing resin.

### Claim 41

A method comprising coating a metal surface with a chromate-free, water-thinnable, organic UV-hardening corrosion-protection coating and for curing the coating by irradiation with UV light, comprising applying a dispersion or emulsion as UV-hardening coating agent for forming the corrosion-protection coating that comprises
25 to 80 wt. % by solids content of the coating of a binder
1 to 8 wt. % of a photoinitiator,
at least some and up to 5 wt. % of an additive selected from the group consisting of a silane, a dimethylsiloxane and a wax additives,
optionally an organic solvent; and at least some and up to 70 wt. % water;
at least one pigment; and
wherein the binder comprises a base resin and an elasticizing resin, where the base resin is selected from the group consisting of an aqueous polyacrylate dispersion, an aqueous polyacrylate emulsion, an unsaturated acrylic ester resin, a urethane acrylic resin or any combination thereof, wherein the elasticizing resin comprises at least some and up to 15 wt. % of the composition of the elasticizing resin as a portion of the binder, wherein at least some and up to 100 wt. % of the elastizing resin is at least an unsaturated aliphatic urethaneacrylate;
wherein the binder comprises polyester acrylate, styrene acrylate or urethane acrylate,
wherein said pigment content is added in the range from 0.1 to 60% by weight and wherein the pigment content is calculated in addition to the sum of said binder, said photoinitiator, said additive, said water and said optional organic solvent equals 100% by weight, wherein said pigment has a mean particle diameter in the range from 0.001 to 10 μm, wherein the aqueous dispersion or emulsion is without an addition of reactive thinners and wherein the coating agent is applied in a layer to the metal surface, dried to a film and hardened by means of UV light, in a thickness from 0.1 to 20 micrometers.

### Claim 42

A method comprising; applying to a metal surface a chromate-free composition that is a dispersion or emulsion comprising
25-80% by weight of a binder based on a solids content of the dispersion or emulsion;
1 to 8 wt. % of a photoinitiator;
at least one lubricating agent;
at least some and up to 70% water; and
from 0.1 to 60 wt. % of a pigment;
wherein the binder comprises a base resin that is an aqueous polyacrylate dispersion or emulsion, an unsaturated acrylic ester resin, a urethane acrylic resin, or a combination thereof and an elasticizing resin, wherein the elasticizing resin comprises from at least some to 100% by weight of at least one unsaturated aliphatic urethaneacrylate;
wherein the pigment content is calculated in addition to the sum of the weight of said binder, said photoinitiator, and said lubricating agent equals 100% by weight and said pigment has a mean particle diameter of from 0.001 to 10 microns, and curing the applied composition by irradiation with UV light to form a cured coating on said metal surface the cured coating having a thickness of from 0.1 to 12 microns,
wherein the base resin is not an elasticizing resin; and
wherein the total weight of the binder includes the weight of the elasticizing resin.