# US 2008/0305254 A1 · Method of manufacturing optical element, and optical element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305254 A1
- Document ID: US20080305254A1
- Status: Published application
- Kind: A1
- Application number: 12/130,073
- Filed: 2008-05-30
- Published: 2008-12-11
- Earliest claimed: 2007-06-06
- Assignees: Canon Kabushiki Kaisha
- Inventors: Hiroyuki Tanaka; Masayuki Yamada; Yoshinori Kotani
- Web page: https://patentgrep.com/patent/US20080305254A1

## CPC

- C03C 1/008: {for the production of films or coatings}
- C03C 17/007: {containing a dispersed phase, e.g. particles, fibres or flakes, in a continuous phase}
- C03C 17/3417: {all coatings being oxide coatings}
- C08J 7/043: Improving the adhesiveness of the coatings per se, e.g. forming primers (adhesives in the form of films or foils characterised by the primer layers between the polymer carriers and the adhesives C09J7/50)
- C08J 7/046: Forming abrasion-resistant coatings; Forming surface-hardening coatings
- C08J 7/06: with compositions not containing macromolecular substances
- G02B 1/113: using inorganic layer materials only
- G02B 1/118: having sub-optical wavelength surface structures designed to provide an enhanced transmittance, e.g. moth-eye structures
- C03C 2217/214: Al2O3
- C03C 2217/425: consisting of a porous layer
- C03C 2217/465: having a specific shape
- C03C 2217/475: Inorganic materials
- C03C 2217/477: Titanium oxide
- C03C 2217/73: Anti-reflective coatings with specific characteristics
- C03C 2217/732: made of a single layer
- C03C 2217/77: Coatings having a rough surface
- C03C 2218/113: by sol-gel processes
- C03C 2218/32: After-treatment
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- Y10T 428/31: Surface property or characteristic of web, sheet or block
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of manufacturing an optical element having a good reflection preventing characteristic is provided in which an irregularity structure having a reflection preventing function can be formed at low temperature. The method includes forming a film on the optical substrate by using a coating liquid containing a metal alkoxide containing at least aluminum, immersing the film in a water-containing liquid, baking the film having been immersed in the water-containing liquid, and subjecting the film having been baked to treatment with warm water to form an aluminum-containing film having a fine irregularity structure.

## Claims

### Claim 1

A method for manufacturing an optical element, the method comprising:
forming a film on an optical substrate by using a coating liquid containing a metal alkoxide containing at least aluminum;
immersing the film in a water-containing liquid;
baking the film having been immersed in the water-containing liquid; and
subjecting the film having been baked to treatment with warm water to form an aluminum-containing film having an irregularity structure.

### Claim 2 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein temperature of the water-containing liquid is not less than 5° C. and not more than 50° C.

### Claim 3 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein the treatment with warm water comprises immersing the film in warm water.

### Claim 4 (depends on 3)

The method for manufacturing an optical element according to claim 3, wherein temperature of the warm water is not less than 60° C. and not more than 100° C.

### Claim 5 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein the treatment with warm water comprises exposing the film to steam.

### Claim 6 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein temperature for baking the film having been immersed in the water-containing liquid is not less than 60° C. and not more than 300° C.

### Claim 7 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein the irregularity structure comprises plate crystals containing aluminum oxide as a main ingredient.

### Claim 8 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein the optical substrate comprises an organic polymer.

### Claim 9 (depends on 1)

The method for manufacturing an optical element according to claim 1, wherein the aluminum-containing film is an aluminum oxide film.

### Claim 10

An optical element comprising an optical substrate and an aluminum oxide film on the optical substrate, wherein the aluminum oxide film has an irregularity structure on its surface, a refractive index n1 of the aluminum oxide film increases from its surface toward a boundary part with the optical substrate, and a refractive index n2 of the aluminum oxide film at the boundary part is in a range of 1.30≦n2≦1.45.