# US 2008/0305023 A1 · Process for selective oxidation of carbon monoxide in a hydrogen containing stream

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0305023 A1
- Document ID: US20080305023A1
- Status: Published application
- Kind: A1
- Application number: 12/195,105
- Filed: 2008-08-20
- Published: 2008-12-11
- Earliest claimed: 2006-07-18
- Assignees: ConocoPhillips Company
- Inventors: M. Bruce WELCH; Roland SCHMIDT; Jianhua YAO; Glenn W. DODWELL; Robert W. MORTON; Jason J. GISLASON; James B. Kimble; David E. SIMON; Marvin M. JOHNSON
- Web page: https://patentgrep.com/patent/US20080305023A1

## CPC

- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 23/8906: {Iron and noble metals}
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0205: {in several steps}
- B01J 37/20: Sulfiding
- C01B 3/583: {the reaction being the selective oxidation of carbon monoxide}
- B01J 21/04: Alumina
- C01B 2203/044: Selective oxidation of carbon monoxide
- C01B 2203/047: the impurity being carbon monoxide
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of making a composition, said method comprising, spraying a substance comprising platinum and iron into or onto an alumina-containing compound is disclosed. The resulting composition can then be used in a process for oxidizing carbon monoxide with free oxygen.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A process for oxidizing carbon monoxide with free oxygen to carbon dioxide comprises:
contacting a feed stream comprising carbon monoxide, hydrogen, and oxygen with a composition in a contacting zone under contacting conditions for a period of time so as to produce a product stream comprising less carbon monoxide than said feed stream,
wherein said composition is prepared by a method comprising the steps of:
a) incorporating a hydrocarbon into the pores of an alumina-containing compound such that at least half of the pore volume of said alumina-containing compound contains said hydrocarbon;
b) spraying a substance comprising platinum and iron into or onto said alumina-containing compound to form a sprayed support;
c) contacting said sprayed support with a sulfide selected from the group consisting of hydrogen sulfide and an alkyl-sulfide to form a sulfided support;
d) calcining said sulfided support to form a calcined support;
e) contacting said calcined support with steam to form a steamed support; and
f) reducing said steamed support to form said composition.

### Claim 14 (depends on 13)

A process in accordance with claim 13 wherein at least a portion of the platinum of said composition is in a reduced valence state.

### Claim 15 (depends on 13)

A process in accordance with claim 13 wherein prior to said oxidizing, said composition is reduced under reducing conditions which include a temperature in the range of from about 20° C. to about 650° C.

### Claim 16 (depends on 13)

A process in accordance with claim 13, wherein prior to said oxidizing, said composition is reduced under reducing conditions, which include a temperature in the range of from 100° C. to 500° C.

### Claim 17 (depends on 13)

A process in accordance with claim 13 wherein said contacting conditions include a temperature in the range of from about room temperature to about 100° C.

### Claim 18 (depends on 13)

A process in accordance with claim 13 wherein said contacting conditions include a temperature in the range of from about 65° C. to about 90° C.

### Claim 19 (depends on 13)

A process in accordance with claim 13 wherein said contacting conditions include a temperature in the range of 70° C. to 85° C.