# US 2008/0304997 A1 · Process for Production of a Carboxylic Acid/Diol Mixture Suitable for Use in Polyester Production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0304997 A1
- Document ID: US20080304997A1
- Status: Published application
- Kind: A1
- Application number: 11/547,298
- Filed: 2005-03-11
- Published: 2008-12-11
- Earliest claimed: 2004-04-06
- Assignees: Primometal Co., Ltd.
- Inventors: Kang-Hyung Kim
- Web page: https://patentgrep.com/patent/US20080304997A1

## CPC

- C22C 23/02: with aluminium as the next major constituent
- C22C 23/06: with a rare earth metal as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Disclosed is a wrought magnesium alloy having excellent strength and extrusion or rolling formability, and a method of producing the same. The wrought magnesium alloy comprises 0.1-1.5 at % group IIIa, 1.0-4.0 at % group IIIb, 0.35 at % or less of one selected from the group consisting of groups IIa, IVa, VIIa, IVb, and a mixture thereof, 1.0 at % or less of group IIb, and a balance of Mg and unavoidable impurities and thus has a second phase composite microstructure. The wrought magnesium alloy of the present invention has high strength, toughness, and formability in addition to the electromagnetic wave shield ability of magnesium. Accordingly, the wrought magnesium alloy is a material useful to portable electronic goods, such as notebook personal computers, mobile phones, digital cameras, camcorders, CD players, PDA, or MP3 players, automotive parts, such as engine room hoods, oil pans, or inner panel of door, or structural parts for airplane.

## Claims

### Claim 1

A wrought magnesium alloy having excellent formability and plating properties, which comprises 0.1-1.5 at % group IIIa 1.0-4.0 at % group IIIb, 0.35 at % or less of one selected from the group consisting of groups IIa, IVa, VIIa, IVb, and a mixture thereof, 1.0 at % or less of group IIb, and a balance of Mg and unavoidable impurities and thus has a second phase intermetallic compound.

### Claim 2 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group IIIa includes Sc, Y, and Lanthanides.

### Claim 3 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group IIIb includes Al and B.

### Claim 4 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group IIa includes Ca and Sr.

### Claim 5 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group IVa includes Ti, Zr, and Hf.

### Claim 6 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group VIIa includes Mn.

### Claim 7 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group IVb includes Si and Ge.

### Claim 8 (depends on 1)

The wrought magnesium alloy as set forth in claim 1, wherein the group IIb includes Zn and Cd, and a content of the group IIb is 0.65 at % or less.

### Claim 9

A method of producing a wrought magnesium alloy, comprising:
extruding a magnesium alloy cast billet which comprises 0.1-1.5 at % group IIIa, 1.0-4.0 at % group IIIb, 0.35 at % or less of one selected from the group consisting of groups IIa, IVa, VIIa, IVb, and a mixture thereof 1.0 at % or less of group IIb, and a balance of Mg and unavoidable impurities and thus has a second phase intermetallic compound; and then rolling the magnesium alloy plate.