# US 2008/0304307 A1 · Use of a symmetric resistive memory material as a diode to drive symmetric or asymmetric resistive memory

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0304307 A1
- Document ID: US20080304307A1
- Status: Published application
- Kind: A1
- Application number: 11/761,043
- Filed: 2007-06-11
- Published: 2008-12-11
- Earliest claimed: 2007-06-11
- Assignees: International Business Machines Corporation
- Inventors: Kailash Gopalakrishnan
- Web page: https://patentgrep.com/patent/US20080304307A1

## CPC

- G11C 13/003: {Cell access}
- G11C 13/0004: {comprising amorphous/crystalline phase transition cells}
- G11C 13/0007: {comprising metal oxide memory material, e.g. perovskites}
- G11C 13/0011: {comprising conductive bridging RAM [CBRAM] or programming metallization cells [PMCs]}
- G11C 13/0014: {comprising cells based on organic memory material}
- G11C 13/0069: {Writing or programming circuits or methods}
- G11C 2013/0073: {Write using bi-directional cell biasing}
- G11C 2213/32: Material having simple binary metal oxide structure
- G11C 2213/72: Array wherein the access device being a diode
- G11C 2213/76: Array using an access device for each cell which being not a transistor and not a diode
- G11C: STATIC STORES (semiconductor memory devices H10B)

## Abstract

A symmetrically resistive memory material (such as a phase change material) is described for use as a rectifying element for driving symmetric or asymmetric resistive memory elements in a crosspoint memory architecture. The crosspoint architecture has a plurality of electrodes and a plurality of crossbar elements, with each crossbar element being disposed between a first and a second electrode. The crossbar element is made of a symmetric resistive memory element used as a rectifier in series with a symmetric or asymmetric resistive memory element.

## Claims

### Claim at position 1

1-21. (canceled)

### Claim 22

A crosspoint array comprising:
a plurality of bitlines and wordlines; and
a plurality of crossbar elements, each crossbar element disposed between a bitline and a wordline and each crossbar element comprising at least a phase change material used as a rectifier in series with a solid electrolyte used as an asymmetric resistive memory element, said phase change material, in said ON state has a first resistance, RON, and in an OFF state has a second resistance, ROFF, with ROFF/RON≧104, where one or more of said crossbar elements are responsive to the following voltages:
a first set of voltages to transition said phase change material in said crossbar elements from an OFF state to an ON state;
a second set of voltages to read or program said solid electrolyte, and
a third set of voltages to transition said phase change material from an ON state to an OFF state,
wherein said solid electrolyte material includes at least one of the following: germanium sulfide (GexS1−x), germanium selenide (GexSe1−x), germanium telluride (GexTe1−x), silicon sulfide (SixS1−x), silicon selenide (SixSe1−x), silicon telluride (SixTe1−x), arsenic sulfide (AsxS1−x), arsenic selenide (AsxSe1−x), arsenic telluride (AsxTe1−x), lead sulfide (PbxS1−x), lead selenide (PbxSe1−x), lead telluride (PbxTe1−x), cadmium sulfide (CdxS1−x), cadmium selenide (CdxSe1−x), cadmium telluride (CdxTe1−x), zinc sulfide (ZnxS1−x), zinc selenide (ZnxSe1−x), zinc telluride (ZnxTe1−x), silver sulfide (AgxS), silver selenide (AgxSe), copper sulfide (CuxS), copper selenide (CuxSe), tungsten oxide (WOx), copper oxide (CuxO), silver (Ag), copper (Cu), lithium (Li), sodium (Na), and zinc (Zn).

### Claim at position 3

23-24. (canceled)

### Claim 25 (depends on 22)

The crosspoint array of claim 22, wherein said crosspoint array is a three-dimensional array comprised of a plurality of layers, with wordlines and bitlines in each layer running at lithographic pitches, and the effective density of cells is 4F2/n, where 2F is a lithographic pitch and n is the number of layers

### Claim at position 5

26-29. (canceled)

### Claim 30

A method for use with a crosspoint array, said crosspoint array comprising a plurality of bitlines and wordlines and a plurality of crossbar elements, each crossbar element disposed between a bitline and a wordline, each crossbar element comprising at least a phase change material used as a rectifier in series with a solid electrolyte, said method comprising the steps of:
applying a first set of voltages to at least one of said crossbar elements, said first set of voltages transitioning said phase change material in said crossbar elements from an OFF state to an ON state;
applying a second set of voltages to at least one of said crossbar elements, said second set of voltages reading or programming said solid electrolyte,
applying a third set of voltages to at least one of said crossbar elements, said third set of voltages transitioning said phase change material from an ON state to an OFF state,
said phase change material, in said ON state has a first resistance, RON, and in an OFF state has a second resistance, ROFF, with ROFF/RON≧104, and
said solid electrolyte material includes at least one of the following: germanium sulfide (GexS1−x), germanium selenide (GexSe1−x), germanium telluride (GexTe1−x), silicon sulfide (SixS1−x), silicon selenide (SixSe1−x), silicon telluride (SixTe1−x), arsenic sulfide (AsxS1−x), arsenic selenide (AsxSe1−x), arsenic telluride (AsxTe1−x), lead sulfide (PbxS1−x), lead selenide (PbxSe1−x), lead telluride (PbxTe1−x), cadmium sulfide (CdxS1−x), cadmium selenide (CdxSe1−x), cadmium telluride (CdxTe1−x), zinc sulfide (ZnxS1−x), zinc selenide (ZnxSe1−x), zinc telluride (ZnxTe1−x), silver sulfide (AgxS), silver selenide (AgxSe), copper sulfide (CuxS), copper selenide (CuxSe), tungsten oxide (WOx), copper oxide (CuxO), silver (Ag), copper (Cu), lithium (Li), sodium (Na), and zinc (Zn).