# US 2008/0304207 A1 · Low temperature double-layer capacitors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0304207 A1
- Document ID: US20080304207A1
- Status: Published application
- Kind: A1
- Application number: 12/134,128
- Filed: 2008-06-05
- Published: 2008-12-11
- Earliest claimed: 2007-06-05
- Assignees: California Institute of Technology
- Inventors: Erik J. Brandon; Marshall C. Smart; William C. West
- Web page: https://patentgrep.com/patent/US20080304207A1

## CPC

- H01G 11/60: characterised by the solvent
- H01G 11/64: characterised by additives
- H01G 11/84: Processes for the manufacture of hybrid or EDL capacitors, or components thereof
- H01G 11/62: characterised by the solute, e.g. salts, anions or cations therein
- Y02E 60/13: Energy storage using capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Double-layer capacitors capable of operating at extremely low temperatures (e.g., as low as −75° C.) are disclosed. Electrolyte solutions combining a base solvent (e.g., acetonitrile) and a cosolvent are employed to lower the melting point of the base electrolyte. Example cosolvents include methyl formate, ethyl acetate, methyl acetate, propionitrile, butyronitrile, and 1,3-dioxolane. An optimized concentration (e.g., 0.10 M to 0.75 M) of salt, such as tetraethylammonium tetrafluoroborate, is disolved into the electrolyte solution. In some cases (e.g., 1,3-dioxolane cosolvent) additives, such as 2% by volume triethylamine, may be included in the solvent mixture to prevent polymerization of the solution. Conventional device form factors and structural elements (e.g., porous carbon electrodes and a polyethylene separator) may be employed.

## Claims

### Claim 1

An apparatus, comprising:
a first porous electrode for conducting a charge;
a second porous electrode for conducting an opposing charge;
an electrolyte solution soaking the first electrode and the second electrode to enable formation of an electrical double-layer at interfaces of both the first porous electrode and the second porous electrode with the electrolyte solution and thereby exhibit a dielectric interaction between charged surfaces of the first porous electrode and the second porous electrode and ions of the electrolyte solution; and
a separator disposed between the first porous electrode and the second porous electrode, the separator allowing for conduction of the ions while electrically insulating the first porous electrode and the second porous electrode;
wherein the electrolyte solution comprises a salt dissolved into at least a base solvent and a second solvent for reducing a melting point of the base solvent.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein the base solvent comprises acetonitrile (AN) and the second solvent comprises a cosolvent selected from the group consisting of an organic carbonate, ether, an ester, a formate or a substituted nitrile.

### Claim 3 (depends on 1)

The apparatus of claim 1, wherein the salt comprises a molarity concentration of substantially 0.10 M to substantially 0.75 M in the electrolyte solution.

### Claim 4 (depends on 1)

The apparatus of claim 1, wherein the base solvent and the second solvent are each selected from the cosolvents consisting of acetonitrile (AN), methyl formate (MF), ethyl acetate (EA), methyl acetate (MA), propionitrile (PN), butyronitrile (BN), and 1,3-dioxolane (DX).

### Claim 5 (depends on 1)

The apparatus of claim 1, wherein the second solvent comprises 1,3-dioxolane (DX) and the electrolyte solution further comprises triethylamine (TEA).

### Claim 6 (depends on 1)

The apparatus of claim 1, wherein the electrolyte solution comprises substantially a 30% to a 70% base solvent volume.

### Claim 7 (depends on 1)

The apparatus of claim 1, wherein the salt comprises tetraethylammonium tetrafluoroborate (TEATFB).

### Claim 8 (depends on 1)

The apparatus of claim 1, wherein at least one of the first porous electrode and the second porous electrode comprise a carbon material.

### Claim 9 (depends on 1)

The apparatus of claim 1, wherein the separator comprises polyethylene.

### Claim 10

A method of producing a double-layer capacitor, comprising:
disposing a first porous electrode for conducting a charge and a second porous electrode for conducting an opposing charge in a case;
preparing an electrolyte solution comprising a salt dissolved into at least a base solvent and a second solvent for reducing a melting point of the base solvent;
disposing a separator between the first porous electrode and the second porous electrode, the separator allowing for conduction of ions while electrically insulating the first porous electrode and the second porous electrode; and
soaking the first electrode and the second electrode with the electrolyte solution in the case to enable formation of an electrical double-layer at interfaces of both the first porous electrode and the second porous electrode with the electrolyte solution and thereby exhibit a dielectric interaction between charged surfaces of the first porous electrode and the second porous electrode and the ions of the electrolyte solution.

### Claim 11 (depends on 10)

The method of claim 10, wherein the base solvent comprises acetonitrile (AN) and the second solvent comprises a cosolvent selected from the group consisting of an organic carbonate, ether, an ester, a formate or a substituted nitrile.

### Claim 12 (depends on 10)

The method of claim 10, wherein the salt comprises a molarity concentration of substantially 0.10 M to substantially 0.75 M in the electrolyte solution.

### Claim 13 (depends on 10)

The method of claim 10, wherein the base solvent and the second solvent are each selected from the cosolvents consisting of acetonitrile (AN), methyl formate (MF), ethyl acetate (EA), methyl acetate (MA), propionitrile (PN), butyronitrile (BN), and 1,3-dioxolane (DX).

### Claim 14 (depends on 10)

The method of claim 10, wherein the second solvent comprises 1,3-dioxolane (DX) and the electrolyte solution further comprises triethylamine (TEA).

### Claim 15 (depends on 10)

The method of claim 10, wherein the electrolyte solution comprises substantially a 30% to a 70% base solvent volume.

### Claim 16 (depends on 10)

The method of claim 10, wherein the salt comprises tetraethylammonium tetrafluoroborate (TEATFB).

### Claim 17 (depends on 10)

The method of claim 10, wherein at least one of the first porous electrode and the second porous electrode comprise a carbon material.

### Claim 18 (depends on 10)

The method of claim 10, wherein the separator comprises polyethylene.

### Claim 19

An apparatus, comprising:
a first porous electrode means for conducting a charge;
a second porous electrode means for conducting an opposing charge;
an electrolyte solution means for soaking the first electrode means and the second electrode means to enable formation of an electrical double-layer at interfaces of both the first porous electrode means and the second porous electrode means with the electrolyte solution means and thereby exhibit a dielectric interaction between charged surfaces of the first porous electrode means and the second porous electrode means and ions of the electrolyte solution means; and
a separator means disposed between the first porous electrode means and the second porous electrode means, the separator means for allowing conduction of the ions while electrically insulating the first porous electrode means and the second porous electrode means;
wherein the electrolyte solution means comprises a salt dissolved into at least a base solvent and a second solvent means for reducing a melting point of the base solvent.

### Claim 20 (depends on 19)

The apparatus of claim 19, wherein the salt comprises a molarity concentration of substantially 0.10 M to substantially 0.75 M in the electrolyte solution.

### Claim 21 (depends on 19)

The apparatus of claim 19, wherein the electrolyte solution means comprises substantially a 30% to a 70% base solvent volume.