# US 2008/0304131 A1 · Electrochromic devices and fabrication methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0304131 A1
- Document ID: US20080304131A1
- Status: Published application
- Kind: A1
- Application number: 11/956,238
- Filed: 2007-12-13
- Published: 2008-12-11
- Earliest claimed: 2007-06-07
- Assignees: Soladigm, Inc.
- Inventors: Paul Nguyen
- Web page: https://patentgrep.com/patent/US20080304131A1

## CPC

- G02F 1/1508: {using a solid electrolyte}
- G02F 1/1525: {characterised by a particular ion transporting layer, e.g. electrolyte}
- G02F 2001/1536: {additional, e.g. protective, layer inside the cell}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

An electrochromic device includes a first conductive layer, a single-layer or dual-layer ion conductor layer, and a second conductive layer. The layers are deposited using PVD, CVD, PECVD, atomic layer deposition, pulsed laser deposition, plating, or sol-gel techniques.

## Claims

### Claim 1

A method for forming an electrochromic device, comprising the steps of:
(a) forming a first conductive electrochromic layer;
(b) forming a first ion conductor layer having a thickness between 1 nm and 300 nm over the first conductive layer, wherein the first ion conductor layer is formed using a deposition technique selected from the group consisting of sputtering, evaporation, CVD, PECVD, ALD, pulsed laser deposition, plating, and sol-gel;
(c) forming a second ion conductor layer having a thickness between 1 nm and 300 nm over the first ion conductor layer, wherein the second ion conductor layer is formed from a different material or using a different deposition technique than the first ion conductor layer, wherein the second ion conductor layer is formed using a deposition technique selected from the group consisting of sputtering, evaporation, CVD, PECVD, ALD, pulsed laser deposition, plating, and sol-gel; and
(d) forming a second conductive counter electrode layer over the second ion conductor layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first ion conductor layer includes a first material selected from the group consisting of Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2.

### Claim 3 (depends on 2)

The method of claim 2, wherein the second ion conductor layer includes a second material selected from the group consisting of a commonly used oxide such as Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2, and the second material is different from the first material.

### Claim 4 (depends on 3)

The method of claim 3, wherein the first ion conductor layer and the second ion conductor layer are each formed in selected atmospheres, wherein the selected atmospheres may be the same or different and are selected from the group consisting of water vapor, oxygen, and a mixture of water vapor and oxygen.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first conductive layer is a counter-electrode layer, and the second conductive layer is an electrochromic layer.

### Claim 6 (depends on 1)

The method of claim 1, further comprising the step of forming at least one additional ion conductor layer over the second ion conductor layer before forming the second conductive counter electrode layer, wherein each additional ion conductor layer is formed from a different material or using a different deposition technique than the previously formed ion conductor layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first ion conductor layer has a thickness between 5 mm and 50 nm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second ion conductor layer has a thickness between 5 nm and 50 nm.

### Claim 9 (depends on 1)

The method of claim 1, wherein one of the ion conductor layers is a material that reduces degradation of at least one adjacent layer.

### Claim 10 (depends on 1)

The method of claim 1, further comprising providing ions for conduction through the ion conductor layers, wherein the provided ions include ions selected from the group consisting of hydrogen and lithium ions.

### Claim 11

A method for forming an electrochromic device, comprising the steps of:
(a) forming a first conductive electrochromic layer;
(b) forming a ion conductor layer having a thickness between 1 nm and 300 nm over the first conductive layer, wherein the first ion conductor layer is formed using a deposition technique selected from the group consisting of sputtering, evaporation, CVD, PECVD, ALD, pulsed laser deposition, plating, and sol-gel;
(c) forming a second conductive counter electrode layer over the ion conductor layer; and
(d) providing ions for conduction through the ion conductor layer, wherein the provided ions include ions selected from the group consisting of hydrogen and lithium ions.

### Claim 12 (depends on 11)

The method of claim 11, wherein the ion conductor layer includes a material selected from the group consisting of Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2.

### Claim 13 (depends on 12)

The method of claim 12, wherein the ion conductor layer is formed in a selected atmosphere, wherein the selected atmosphere is selected from the group consisting of water vapor, oxygen, and a mixture of water vapor and oxygen.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first conductive layer is a counter-electrode layer, and the second conductive layer is an electrochromic layer.

### Claim 15 (depends on 11)

The method of claim 11, wherein the ion conductor layer has a thickness between 5 nm and 50 mm.

### Claim 16

An electrochromic device, comprising:
(a) a first conductive electrochromic layer;
(b) a first ion conductor layer having a thickness between 1 nm and 300 nm formed over the first conductive layer;
(c) a second ion conductor layer having a thickness between 1 nm and 300 nm formed over the first ion conductor layer, wherein the second ion conductor is formed from a different material or using a different deposition technique than the first ion conductor layer; and
(d) a second conductive counter electrode layer formed over the second ion conductor layer.

### Claim 17 (depends on 16)

The electrochromic device of claim 16, wherein the first ion conductor layer includes a first material selected from the group consisting of Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2.

### Claim 18 (depends on 17)

The electrochromic device of claim 17, wherein second ion conductor layer includes a second material selected from the group consisting of Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2.

### Claim 19 (depends on 17)

The electrochromic device of claim 17, wherein the first ion conductor layer includes a plurality of sublayers of the first material, and adjacent sublayers of the first material are formed using different processing or deposition conditions.

### Claim 20 (depends on 19)

The electrochromic device of claim 19, wherein the sublayers are formed using different atmospheres.

### Claim 21 (depends on 20)

The electrochromic device of claim 20, wherein the different atmospheres are selected from the group consisting of water vapor, oxygen, and a mixture of water vapor and oxygen.

### Claim 22 (depends on 18)

The electrochromic device of claim 18, wherein the second ion conductor layer includes a plurality of sublayers of the second material, and adjacent sublayers of the second material are formed using different processing or deposition conditions.

### Claim 23 (depends on 19)

The electrochromic device of claim 19, wherein the second ion conductor layer includes a second material selected from the group consisting of Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2, the second material is different from the first material, the second conductor layer includes a plurality of sublayers of the second material, and adjacent sublayers of the second material are formed using different processing or deposition conditions.

### Claim 24 (depends on 16)

The electrochromic device of claim 16, further comprising at least one additional ion conductor layer between the second ion conductor layer and the second conductive counter electrode layer, wherein each additional ion conductor layer is formed from a different material or using a different deposition technique than the previously formed ion conductor layer.

### Claim 25 (depends on 16)

The electrochromic device of claim 16, wherein the first ion conductor layer has a thickness between 5 nm and 50 nm.

### Claim 26 (depends on 16)

The electrochromic device of claim 16, wherein the second ion conductor layer has a thickness between 5 nm and 50 nm.

### Claim 27 (depends on 16)

The electrochromic device of claim 16, wherein one of the ion conductor layers is a material that reduces degradation of at least one adjacent layer.

### Claim 28

An electrochromic device, comprising:
(a) a first conductive electrochromic layer;
(b) an ion conductor layer having a thickness between 1 nm and 300 nm formed over the first conductive layer; and
(c) a second conductive counter electrode layer formed over the ion conductor layer; and
(d) providing ions for conduction through the ion conductor layer, wherein the provided ions include ions selected from the group consisting of hydrogen and lithium ions.

### Claim 29 (depends on 28)

The electrochromic device of claim 28, wherein the ion conductor layer includes a material selected from the group consisting of Ta2O5, SiO2, Al2O3, Nb2O3, ZrO2, Li—Nb—O, Li—Ta—O, Li—Al—O, Li—P—O—N, Li—Ti—Al—P—O, Li—Si—Al—O, Li—Zn—Ge—O, Li—Si—P—O, Li—Zr—P—O, Li—La—Ti—O, B2O3, H3BO3, HBO2, H2B4O7, Bi2O3, Mg3(PO4)2.22H2O, MgHPO4.3H2O, KAISO4.12H2O, NaH2P2O7.6H2O, CsHSO4, CsH2PO4, KH2PO4, KHSO4, and K3H(SO4)2.

### Claim 30 (depends on 28)

The method of claim 28, wherein the ion conductor layer has a thickness between 5 nm and 50 nm.

### Claim 31 (depends on 1)

The method of claim 1, wherein the first ion conductor layer includes a first material selected from the group consisting of hygroscopic materials and solid acids.