# US 2008/0302999 A1 · Negative Active Material for Rechargeable Lithium Battery, Method of Preparing Same and Rechargeable Lithium Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0302999 A1
- Document ID: US20080302999A1
- Status: Published application
- Kind: A1
- Application number: 12/182,998
- Filed: 2008-07-30
- Published: 2008-12-11
- Earliest claimed: 2003-08-22
- Assignees: Samsung SDI Co., Ltd.
- Inventors: Keiko Matsubara; Akira Takamuku; Toshiaki Tsuno; Sung-Soo Kim
- Web page: https://patentgrep.com/patent/US20080302999A1

## CPC

- H01M 10/052: Li-accumulators
- C04B 35/58085: {based on silicides}
- C04B 35/62615: {High energy or reactive ball milling}
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- C04B 35/62685: {characterised by the order of addition of constituents or additives}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/38: of elements or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- C04B 2235/405: Iron group metals
- C04B 2235/408: Noble metals
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y10T 29/49108: Electric battery cell making
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Disclosed is a negative active material for a rechargeable lithium battery comprising a Si phase, a SiM phase and at least one of a X phase and a SiX phase, wherein each of phases has a crystal grain size of 100 nm and 500 nm. The element M is at least one selected from the group consisting of Ni, Co, B, Cr, Cu, Fe, Mn, Ti, and Y, the element X is at least one selected from the group consisting of Ag, Cu, and Au. However, where M is Cu, X is not Cu.

## Claims

### Claim 1

A method of preparing a negative active material for a rechargeable lithium battery comprising:
first alloying Si and element M by a mechanical alloying process to provide a SiM alloy, wherein M is selected from the group consisting of Ni, Co, B, Cr, Cu, Fe, Mn, Ti, Y and combinations thereof;
first heating the SiM alloy at a first temperature; adding a powder of element X to the heated SiM alloy wherein X is selected from the group consisting of Ag, Cu, Au and combinations thereof, provided that if M is Cu, X is not Cu;
second alloying the combined SiM alloy and element X by a mechanical alloying process to provide a SiMX alloy; and
second heating the SiMX alloy at a second temperature lower than the first temperature; wherein the negative active material comprises a Si phase, a SiM phase and at least one of an X phase and a SiX phase, wherein each of the phases has a crystal grain size between 100 nm and 500 nm.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first heating is carried out at temperature between (Tm-100)° C. to (Tm-20)° C. where Tm is the melting point of the SiM alloy phase.