# US 2008/0302859 A1 · Method of reflow soldering a printed circuit board wherein an electroconductive coating material is used

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0302859 A1
- Document ID: US20080302859A1
- Status: Published application
- Kind: A1
- Application number: 12/133,521
- Filed: 2008-06-05
- Published: 2008-12-11
- Earliest claimed: 2007-06-08
- Assignees: SMK Corporation
- Inventors: Nobuo Kasagi; Kenichi Hashimoto
- Web page: https://patentgrep.com/patent/US20080302859A1

## CPC

- B23K 1/008: Soldering within a furnace (B23K1/012 takes precedence)
- B23K 1/20: Preliminary treatment of work or areas to be soldered, e.g. in respect of a galvanic coating
- B23K 3/0646: {Solder baths}
- H05K 3/3494: Heating processes for reflow soldering
- H05K 1/095: {for polymer thick films, i.e. having a permanent organic polymeric binder}
- H05K 3/3485: Application of solder paste, slurry or powder (using printing techniques to form the desired conductive pattern of the printed circuit by applying conductive material H05K3/12)
- H05K 2203/086: Using an inert gas
- H05K 2203/111: Preheating, e.g. before soldering
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A reflow soldering method for use with circuit patterns and land patterns formed by an electoconductive coating material. Reflow soldering is performed in an air atmosphere within a range of 150°-190° C. and with a preheating time set within a range of 60±30 sec. Alternatively, preheating is performed in a nitrogen atmosphere.

## Claims

### Claim 1

A method of reflow soldering a printed circuit board, wherein an electroconductive coating material is used, comprising the steps of:
screen printing a circuit pattern on an insulator board with an electroconductive coating material;
printing a land part of the circuit pattern with cream solder;
mounting a component on the land part; and
reflowing the cream solder;
wherein,
the temperature of preheating, which activates the flux, is set within a range of 150°-190° C. and the preheating time is set within a range of 60±30 sec.

### Claim 2

A method of reflow soldering a printed circuit board, wherein an electroconductive coating material is used, comprising the steps of:
screen printing a circuit pattern on an insulator board with an electroconductive coating material;
printing a land part of the circuit pattern with cream solder;
mounting a component on the land part; and
reflowing the cream solder;
wherein,
preheating, which activates a flux, is performed in a nitrogen atmosphere.

### Claim 3 (depends on 2)

The method of claim 2, wherein the nitrogen atmosphere has an oxygen concentration that is less than 4,000 ppm.