# US 2008/0302453 A1 · Shaped Steel Excellent in Fire Resistance and Producing Method Therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0302453 A1
- Document ID: US20080302453A1
- Status: Published application
- Kind: A1
- Application number: 11/658,348
- Filed: 2005-07-26
- Published: 2008-12-11
- Earliest claimed: 2004-07-28
- Assignees: Nippon Steel Corporation
- Inventors: Suguru Yoshida; Kazuhiko Eda; Hiroshi Kita
- Web page: https://patentgrep.com/patent/US20080302453A1

## CPC

- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A shaped steel, such as H-shaped steel, excellent in fire resistance, where a flange portion has 50% or more of a ratio of strength, 80% or less of yield ratio, and 100 J or more of impact strength of Charpy impact test at 0° C., wherein the ratio of strength=(proof stress of 0.2% at 600° C.)/(yield strength at room temperature), and a producing method thereof are provided. The shaped steel comprises in mass percent (%): C: 0.03-0.15; Mo: 0.1-0.6; V≦0.35; and N: 0.002-0.012, and the balance being iron and residual impurities, wherein (x) a mol fraction of precipitate of alloy carbides and alloy carbonitrides at 600° C. is 0.3% or more, and (y) the ratio of the mol fraction of precipitate of alloy carbides and alloy carbonitrides at 300° C. to the mol fraction of precipitate of alloy carbides and alloy carbonitrides at 600° C. is 2.0 or less.

## Claims

### Claim 1

A shaped steel, comprising in mass percent (%):
C: 0.03-0.15;
Mo: 0.1-0.6;
V≦0.35; and
N: 0.002-0.012,
and the balance being iron and residual impurities, wherein
(x) a mol fraction of precipitate of alloy carbides and alloy carbonitrides at 600° C. is 0.3% or more, and
(y) a ratio of the mol fraction of precipitate of alloy carbides and alloy carbonitrides at 300° C. to the mol fraction of precipitate of alloy carbides and alloy carbonitrides at 600° C. is 2.0 or less.

### Claim 2 (depends on 1)

The shaped steel according to claim 1, further comprising:
Si: 0.05-0.50;
Mn: 0.4-2.0; and
Al≦0.01,
wherein the amount of V ranges from 0.04 to 0.35 in mass %, a flange portion of the shaped steel has 50% or more of a ratio of strength, 80% or less of yield ratio, and 100 J or more of impact strength of Charpy impact test at 0° C., wherein the ratio of strength=(proof stress of 0.2% at 600° C.)/(yield strength at room temperature).

### Claim 3 (depends on 1, 2)

The shaped steel according to claim 1 or 2, further comprising one or more of following elements in mass percent (%):
Ti: 0.005-0.020;
Nb≦0.06%;
Cr≦0.7;
Ni≦1.0; and
Cu≦1.0.
wherein the content of V ranges from more than 0.20 to 0.35 in mass %.

### Claim 4 (depends on 1)

A method for producing a shaped steel according to claim 1 by hot rolling after reheating a casted steel, comprising steps of:
(a) reheating the casted steel to 1100-1300° C.;
(b) hot rolling the casted steel to form the shaped steel; and
(c) after terminating the hot rolling, naturally cooling or rapidly cooling then naturally cooling the shaped steel.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the step of hot rolling includes water-cooling the shaped steel at least once to 700° C. or less as measured at the surface of a flange portion of the shaped steel and then rolling in the heat returning process.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the step of rapid cooling is performed at an average cooling rate of 0.5 to 5.0° C./s.