# US 2008/0302452 A1 · Process for Manufacturing Cold-Formed Precision Steel Pipes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0302452 A1
- Document ID: US20080302452A1
- Status: Published application
- Kind: A1
- Application number: 12/067,756
- Filed: 2006-08-18
- Published: 2008-12-11
- Earliest claimed: 2005-09-21
- Assignees: Mhp Mannesmann Prazisrohr GmbH
- Inventors: Josef Siekmeyer; Wolfgang Mussmann; Lothar See; Sven Herzing
- Web page: https://patentgrep.com/patent/US20080302452A1

## CPC

- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The invention relates to a process for manufacturing cold-formed, in particular cold-drawn, precision steel pipes for application in particular as pressure-operated cylinder pipes with optimum addition of one or several alloying elements as well as impurities caused by melting. A seamless, hot-formed pipe blank or welded pipe blank made from a hot strip with defined starting condition is hereby drawn in one pass or in several passes into a finished pipe, and the pipe undergoes a heat treatment before the finishing pass.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A process for manufacturing a precision steel pipe having the following chemical composition (in weight-%):
C =
0.05-0.25
Si =
0.15-1.0
Mn =
1.0-3.5
Al =
0.020-0.060
V
max. 0.20
N
max 0.150
S
max 0.030
and impurities caused by melting, said process comprising the steps of:
drawing a pipe blank with defined starting condition in at least one pass;
subjecting the pipe blank to a heat treatment; and
subjecting the pipe blank to a finishing drawing step to produce a finished pipe.

### Claim 12 (depends on 11)

The process of claim 11, wherein the pipe blank is a seamless, hot-formed pipe blank.

### Claim 13 (depends on 11)

The process of claim 11, wherein the pipe blank is welded pipe blank made from a hot strip.

### Claim 14 (depends on 11)

The process of claim 11, further comprising the step of adding at least one alloying element selected from the group consisting of Cr, Mo, Ni, W, Ti, and Nb.

### Claim 15 (depends on 11)

The process of claim 11, further comprising the step of adding alloying elements in a following composition (in weight-%):
Cr
max. 0.80
Mo
max. 0.65
Ni
max. 0.90
W
max. 0.90
Ti
max. 0.20
Nb
max. 0.20

### Claim 16 (depends on 11)

The process of claim 11, wherein the heat treatment comprises the step of heating the pipe blank to a temperature of in a range of 910-940° C., cooling the pipe blank, and exposing the pipe blank to a tempering treatment.

### Claim 17 (depends on 16)

The process of claim 16, wherein the cooling step comprises accelerated cooling.

### Claim 18 (depends on 17)

The process of claim 17, wherein the accelerated cooling step comprises quenching.

### Claim 19 (depends on 11)

The process of claim 11, wherein the quenching step is implemented by means of a water shower.

### Claim 20 (depends on 16)

The process of claim 16, wherein the cooling step comprises exposure to static air.

### Claim 21 (depends on 16)

The process of claim 16, wherein the tempering treatment is carried out at a temperature range of 540 to 720° C.

### Claim 22 (depends on 11)

The process of claim 11, further comprising the step of subjecting the finished pipe to a final annealing.

### Claim 23 (depends on 22)

The process of claim 22, wherein the final annealing step is carried out at a temperature range of 500 to 700° C.