# US 2008/0302135 A1 · Method for the Production of Shaped Silica Aquagels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0302135 A1
- Document ID: US20080302135A1
- Status: Published application
- Kind: A1
- Application number: 11/667,977
- Filed: 2005-10-28
- Published: 2008-12-11
- Earliest claimed: 2004-11-27
- Assignees: Degussa AG
- Inventors: Lorenzo Costa; Giulio Boara
- Web page: https://patentgrep.com/patent/US20080302135A1

## CPC

- C03B 19/12: by liquid-phase reaction processes
- C03C 1/006: {to produce glass through wet route}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 2203/22: using colloidal silica sols
- C03C 2203/24: using alkali silicate solutions
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

It has been discovered that aquagels, formed from acid catalized composite sols, survive to conditions of high-tension when they are prepared by a process that hydrolyzes the silicon alkoxides in presence of fumed silica. The aquagel can be used for the production of monoliths of glass.

## Claims

### Claim 1

Method for the production of formed aquagels for the production of monoliths by means of the sol-gel process, comprising the following steps:
a. Dispersing a pyrogenically prepared silicondioxide in water or a water containing solvent, to form an aqueous or water containing dispersion.
b. Adding of an acid in order to reach a pH-value of 2±0.5.
c. Adding of tetraethylorthosilicate (TEOS).
d. Hydrolyzing the tetraethylorthosilicate (TEOS) in order to produce a sol containing the pyrogenically produced oxide of a metal and/or metalloid.
e. Evaporating the liquid from the sol.
f. Adding to the remaining sol an aqueous solution of ammoniumhydroxide in order to reach a pH-value of 4±0.5.
g. Filling the sol into a mould.
h. Gelling the sol to the corresponding aquagels.

### Claim 2 (depends on 1)

Method for the production of glass-monoliths by means of the sol-gel process using the aquagel produced according to claim 1, comprising:
a. Exchanging the solvent by acetone.
b. Extracting the aquagel under supercritical or slightly subcritical conditions in order to get an aerogel.
c. Treating the aerogel thermally for the densification to glass.