# US 2008/0293889 A1 · Nitrile rubbers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0293889 A1
- Document ID: US20080293889A1
- Status: Published application
- Kind: A1
- Application number: 12/030,953
- Filed: 2008-02-14
- Published: 2008-11-27
- Earliest claimed: 2007-05-22
- Assignees: LANXESS Deutschland GmbH
- Inventors: Werner Obrecht
- Web page: https://patentgrep.com/patent/US20080293889A1

## CPC

- C08L 9/02: Copolymers with acrylonitrile
- C08C 1/15: characterised by the coagulants used
- C08C 1/16: in floc form
- C08F 236/12: with nitriles
- C08K 3/16: Halogen-containing compounds
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

An improved polymerization and work-up process makes it possible to produce specific nitrile rubbers which have a specific calcium and chloride content and have a particularly high storage stability.

## Claims

### Claim 1

A nitrile rubber comprising repeating units of at least one α,β-unsaturated nitrile, at least one conjugated diene and optionally one or more further copolymerizable monomers and
(i) has a calcium content of at least 150 ppm, based on the nitrile rubber, and a chlorine content of at least 40 ppm, based on the nitrile rubber, and
(ii) contains 2,2,4,6,6-pentamethylheptane-4-thio and/or 2,4,4,6,6-pentamethylheptane-2-thio and/or 2,3,4,6,6-pentamethylheptane-2-thio and/or 2,3,4,6,6-pentamethylheptane-3-thio end groups.

### Claim 2

The nitrile rubber according to Claim i comprising a calcium content of at least 200 ppm, preferably at least 400 ppm, particularly preferably more than 500 ppm, in particular at least 600 ppm and especially preferably at least 800 ppm, of calcium, based on the nitrile rubber.

### Claim 3 (depends on 1)

The nitrile rubber according to claim 1 which has a storage stability SS of not more than 5 Mooney units, preferably less than 5 Mooney units and particularly preferably not more than 4 Mooney units, with the storage stability SS being given by the formula (I),
SS=MV2−MV1 (I)
where
MV1 is the Mooney viscosity of the nitrile rubber and
MV2 is the Mooney viscosity of the same nitrile rubber after storage at 100° C. for 48 hours.

### Claim 4 (depends on 1)

The nitrile rubber according to claim 1, comprising repeating units of acrylonitrile, 1,3-butadiene and optionally one or more further copolymerizable monomers.

### Claim 5 (depends on 1)

The nitrile rubber according to claim 1 comprising repeating units of one or more α,β-unsaturated monocarboxylic or dicarboxylic acids, their esters or amides, preferably repeating units of an alkyl ester of an α,β-unsaturated carboxylic acid, in particular methyl(meth)acrylate, ethyl(meth)acrylate, propyl(meth)acrylate, n-butyl(meth)acrylate, t-butyl(meth)acrylate, hexyl(meth)acrylate, 2-ethylhexyl(meth)acrylate, octyl(meth)acrylate or lauryl(meth)acrylate.

### Claim 6 (depends on 1)

The nitrile rubber according to claim 1 comprising a Mooney viscosity MV1 (ML (1+4@100° C.)) of from 10 to 150 Mooney units, preferably from 20 to 100 Mooney units.

### Claim 7 (depends on 1)

The nitrile rubber according to claim 1 comprising a glass transition temperature in the range from −70° C. to +10° C., preferably in the range from −60° C. to 0° C.

### Claim 8 (depends on 1)

The nitrile rubber according to claim 1 comprising 2,2,4,6,6-pentamethylheptane-4-thio-, 2,4,4,6,6-pentamethylheptane-2-thio-, 2,3,4,6,6-pentamethyl-heptane-2-thio and 2,3,4,6,6-pentamethylheptane-3-thio end groups.

### Claim 9 (depends on 1)

A process for producing a nitrile rubber according to claim 1 by emulsion polymerization of at least one α,β-unsaturated nitrile, at least one conjugated diene and optionally one or more further copolymerizable monomers, with the latex containing the nitrile rubber which is initially obtained in the polymerization being subjected to coagulation and the coagulated nitrile rubber obtained subsequently being washed, characterized in that
(i) the emulsion polymerization is carried out in the presence of a mixture containing 2,2,4,6,6-pentamethylheptane-4-thiol, 2,4,4,6,6-pentamethylheptane-2-thiol, 2,3,4,6,6-pentamethylheptane-2-thiol and 2,3,4,6,6-pentamethylheptane-3 -thiol,
(ii) the latex containing the nitrile rubber which is obtained after the polymerization is subjected to coagulation using at least one salt selected from the group consisting of aluminium, calcium, magnesium, sodium, potassium and lithium salts,
(iii) either a water-soluble calcium salt is present in the coagulation and/or the washing of the coagulated nitrile rubber is carried out using water containing calcium ions and
(iv) a salt based on a chloride is present either during the emulsion polymerization, during the coagulation or during the subsequent washing of the coagulated nitrile rubber.

### Claim 10 (depends on 9)

The process according to claim 9, wherein the emulsion polymerization is carried out batchwise or continuously in a cascade of stirred vessels.

### Claim 11 (depends on 9)

The process according to claim 9, wherein one or more ageing inhibitors, preferably phenolic ageing inhibitors are added to the latex containing the nitrile rubber before or during coagulation.

### Claim 12 (depends on 9)

The process according to claim 9, wherein sodium chloride, potassium chloride, calcium chloride, magnesium chloride, sodium nitrate, potassium nitrate, sodium sulphate, potassium sulphate, sodium hydrogencarbonate, potassium hydrogencarbonate, sodium carbonate, potassium carbonate, aluminium sulphate, potassium aluminium sulphate (potassium alum), sodium aluminium sulphate (sodium alum), sodium acetate, calcium acetate or calcium formate is used for the coagulation of the latex.

### Claim 13 (depends on 9)

The process according to claim 9, wherein the total amount of the salt or salts used for the coagulation of the latex is 0.5-200 parts by weight, preferably 0.8-80 parts by weight and particularly preferably 1-50 parts by weight, per 100 parts by weight of nitrile rubber.

### Claim 14 (depends on 9)

The process according to claim 9, wherein the latex used for the coagulation has a solids concentration in the range from 1% to 40%, preferably in the range from 5% to 35% and particularly preferably in the range from 15 to 30% by weight.

### Claim 15 (depends on 9)

The process according to claim 9, wherein the coagulation of the latex is carried out at a temperature in the range from 10 to 100° C., particularly preferably in the range from 20 to 90° C.

### Claim 16 (depends on 9)

The process according to claim 9, wherein the washing of the coagulated nitrile rubber is carried out at a temperature in the range from 15 to 90° C., preferably at a temperature in the range from 20 to 80° C.

### Claim 17 (depends on 9)

The process according to claim 9, wherein the obtained nitrile rubber is subsequently subjected either (i) to a metathetic degradation reaction, (ii) a metathetic degradation reaction and a subsequent hydrogenation, or (iii) only a hydrogenation reaction.

### Claim 18 (depends on 17)

An optionally hydrogenated nitrile rubbers obtainable in the process according to claim 17.

### Claim 19 (depends on 1)

A vulcanizable mixture containing at least one nitrile rubber according to claim 1.

### Claim 20 (depends on 18)

A vulcanizable mixture according to claim 18 containing at least one crosslinker and optionally further additives.

### Claim 21 (depends on 19)

A process for producing a vulcanizable mixture according to claim 19 by mixing at least one nitrile rubber comprising repeating units of at least one α,β-unsaturated nitrile, at least one conjugated diene and optionally one or more further copolymerizable monomers and
(i) has a calcium content of at least 150 ppm, based on the nitrile rubber, and a chlorine content of at least 40 ppm, based on the nitrile rubber, and
(ii) contains 2,2,4,6,6-pentamethylheptane-4-thio and/or 2,4,4,6,6-pentamethylheptane-2-thio and/or 2,3,4,6,6-pentamethylheptane-2thio and/or 2 3,4,6,6-pentamethylheptane-3-thio end groups.

### Claim 22 (depends on 18)

A process for producing a vulcanizable mixture according to claim 18 comprising at least one crosslinker and optionally further additives.

### Claim 23 (depends on 1)

A process for producing mouldings based on a nitrile rubber according to claim 1.

### Claim 24 (depends on 19)

A process for producing mouldings based on an optionally hydrogenated nitrile rubbers, wherein a vulcanizable mixture according to claim 19 is vulcanized in a shaping process, preferably using an injection moulding process.

### Claim 25 (depends on 23)

A moulding obtainable by the process according to claim 23.

### Claim 26 (depends on 25)

The moulding according to claim 25, characterized in that it is a seal, a cap, a hose or a diaphragm, in particular an O-ring seal, a flat seal, a corrugated sealing ring, a sealing sleeve, a sealing cap, a dust protection cap, a plug seal, a thermal insulation hose (with or without addition of PVC), an oil cooler hose, an air intake hose, a servo control hose or a pump diaphragm.