# US 2008/0292878 A1 · Polyimide film with improved adhesion, process for its fabrication and laminated body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0292878 A1
- Document ID: US20080292878A1
- Status: Published application
- Kind: A1
- Application number: 12/164,203
- Filed: 2008-06-30
- Published: 2008-11-27
- Earliest claimed: 2004-12-27
- Assignees: Ube Industries, Ltd.
- Inventors: Takashi Kino; Masafumi Kohda; Masato Murakami; Hiroaki Yamaguchi
- Web page: https://patentgrep.com/patent/US20080292878A1

## CPC

- H05K 1/0346: {containing N}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 15/08: of synthetic resin
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 27/16: specially treated, e.g. irradiated
- B32B 27/281: {comprising polyimides}
- B32B 27/34: comprising polyamides
- C08L 79/04: Polycondensates having nitrogen-containing heterocyclic rings in the main chain; Polyhydrazides; Polyamide acids or similar polyimide precursors
- C09J 179/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- B32B 2274/00: Thermoplastic elastomer material
- B32B 2307/306: Resistant to heat
- B32B 2307/5825: Tear resistant
- B32B 2439/00: Containers; Receptacles
- B32B 2457/00: Electrical equipment
- H05K 2201/0154: Polyimide
- H05K 2203/124: Heterocyclic organic compounds, e.g. azole, furan
- Y10T 428/265: 1 mil or less
- Y10T 428/266: of base or substrate
- Y10T 428/31681: Next to polyester, polyamide or polyimide [e.g., alkyd, glue, or nylon, etc.]
- Y10T 428/31721: Of polyimide
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A laminated body obtained by forming a metal-deposited layer onto one or both adhesion-improved sides of a polyimide film with improved adhesion obtained by coating and spraying an organic polar solvent solution containing a polybenzimidazole onto one or both sides of a self-supporting film prepared by casting and drying a dope, which is an organic polar solvent solution of a polyimide precursor which may contain an imidization catalyst, onto a support and then heat treating the film to form a multilayer polyimide film of a base polyimide layer and one or two polybenzimidazole layers, by vapor deposition or sputtering, and then plating with metal to form a metal layer onto the metal-deposited layer.

## Claims

### Claim 1

A laminated body obtained by forming a metal-deposited layer onto one or both adhesion-improved sides of a polyimide film with improved adhesion obtained by coating and spraying an organic polar solvent solution containing a polybenzimidazole onto one or both sides of a self-supporting film prepared by casting and drying a dope, which is an organic polar solvent solution of a polyimide precursor which may contain an imidization catalyst, onto a support and then heat treating the film to form a multilayer polyimide film of a base polyimide layer and one or two polybenzimidazole layers, by vapor deposition or sputtering, and then plating with metal to form a metal layer onto the metal-deposited layer.

### Claim 2 (depends on 1)

The laminated body according to claim 1, wherein the thickness of the polybenzimidazole layer is 0.01-3.0 μm.

### Claim 3 (depends on 1)

The laminated body according to claim 1, wherein the polyimide precursor is produced from 3,3′,4,4′-biphenyltetracarboxylic dianhydride (s-BPDA), para-phenylenediamine (PPD) and 4,4′-diaminodiphenylether (DADE) and has a PPD/DADE molar ratio between 100/0 and 85/15, is produced from s-BPDA, pyromellitic dianhydride, PPD and DADE and has a PPD/DADE molar ratio between 90/10 and 10/90, is produced from pyromellitic dianhydride, PPD and DADE and has a PPD/DADE molar ratio between 90/10 and 10/90, or is produced from 3,3′,4,4′-benzophenonetetracarboxylic dianhydride (BTDA), pyromellitic dianhydride, PPD and DADE and has a PPD/DADE molar ratio between 20/80 and 90/10 in the acid dianhydride and a PPD/DADE molar ratio between 30/70 and 90/10 in the diamine.

### Claim 4 (depends on 1)

The laminated body according to claim 1, wherein tile thickness of the metal-deposited film obtained by sputtering is between 10 nm and 1 μm.

### Claim 5 (depends on 1)

The laminated body according to claim 1, wherein the metal-deposited film has a structure with two or more layers comprising an underlying layer and a surface deposited metal layer, the underlying layer being composed of one member selected from chromium, titanium, palladium, zinc, molybdenum, nickel, cobalt, zirconium arid iron and the surface deposited metal layer being composed of copper.

### Claim 6 (depends on 1)

The laminated body according to claim 1, wherein the material for the metal plating layer formed on the metal-deposited layer is copper, copper alloy or silver.

### Claim 7 (depends on 1)

The laminated body according to claim 1, wherein the metal plating layer is formed by an electroless plating or electroplating method.

### Claim 8 (depends on 1)

The laminated body according to claim 1, wherein the organic polar solvent solution of a polyimide precursor has a polymer concentration of 8-25 wt % and is heated at 100-180° C. for 5-60 minutes to prepare the self-supporting film.

### Claim 9 (depends on 1)

The laminated body according to claim 1, wherein the organic polar solvent solution containing a polybenzimidazole has a polymer concentration of 0.1-10 wt %.

### Claim 10 (depends on 1)

The laminated body according to claim 1, wherein the self-supporting film onto which the organic polar solvent solution containing a polybenzimidazole has been coated or sprayed is heat treated at a temperature above the glass transition temperature Of the polyimide arid no higher than 500° C.

### Claim 11 (depends on 1)

The laminated body according to claim 1, wherein the base polyimide layer has a thickness of 10-100 μm, the multilayer polyimide film has a tensile strength of 30-100 kg/mm2, an elastic modulus of 600-1200 kg/mm2, an elongation of 30-100%, a water absorption (after 24 hours immersed in water at 23° C.) of no greater than 1.5% and a thermal expansion coefficient (23-300° C., both TD and MD) of 0.5-2.5×10−5 cm/cm/° C.

### Claim 12

A process for producing a laminated body whereby a metal-deposited layer is formed onto one or both adhesion-improved sides of a polyimide film with improved adhesion obtained by coating and spraying an organic polar solvent solution containing a polybenzimidazole onto one or both sides of a self-supporting film prepared by casting and drying a dope, which is an organic polar solvent solution of a polyimide precursor which may contain an imidization catalyst, onto a support and then heat treating the film to form a multilayer polyimide film of a base polyimide layer and one or two polybenzimidazole layers, by vapor deposition or sputtering, and then metal is plated to form a metal layer onto the metal-deposited layer.
