# US 2008/0292874 A1 · Sintered power semiconductor substrate and method of producing the substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0292874 A1
- Document ID: US20080292874A1
- Status: Published application
- Kind: A1
- Application number: 12/152,022
- Filed: 2008-05-12
- Published: 2008-11-27
- Earliest claimed: 2007-05-12
- Assignees: Semikron Elektronik GmbH & Co. KG
- Inventors: Christian GOBL; Heiko BRAML; Ulrich HERMANN
- Web page: https://patentgrep.com/patent/US20080292874A1

## CPC

- H05K 3/38: Improvement of the adhesion between the insulating substrate and the metal
- C04B 35/645: Pressure sintering
- C04B 37/021: {in a direct manner, e.g. direct copper bonding [DCB]}
- C04B 37/026: {consisting of metals or metal salts}
- H10W 40/255: {having a laminate or multilayered structure, e.g. direct bond copper [DBC] ceramic substrates}
- H10W 70/098: {Applying pastes or inks, e.g. screen printing (H10W70/095 takes precedence)}
- C04B 2237/124: based on copper
- C04B 2237/125: based on noble metals, e.g. silver
- C04B 2237/343: Alumina or aluminates
- C04B 2237/366: Aluminium nitride
- C04B 2237/368: Silicon nitride
- C04B 2237/407: Copper
- C04B 2237/408: Noble metals, e.g. palladium, platina or silver
- C04B 2237/704: of one or more of the ceramic layers or articles
- C04B 2237/706: of one or more of the metallic layers or articles
- C04B 2237/72: Forming laminates or joined articles comprising at least two interlayers directly next to each other
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H05K 2201/0355: Metal foils
- H10W 72/07141: {Means for applying energy, e.g. ovens or lasers}
- Y10T 428/264: Up to 3 mils
- Y10T 428/31678: Of metal
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A power semiconductor substrate with an insulating sheet-like base, having at least one sequence of layers of: a thin adhesion promoting layer, a sintered metal layer and a conductive layer arranged on at least one main area of the substrate. The associated process includes the steps of: coating at least a portion of the one main area with the adhesion promoting layer; arranging a pasty layer of the sintered metal and a solvent on at least a portion of the adhesion promoting layer; arranging the conductive layer on the sintered metal layer; and applying pressure to the conductive layer of the power substrate.

## Claims

### Claim 1

A power semiconductor substrate having an insulating sheet-like base and at least one main area comprising:
at least one sequence of layers comprising
a thin adhesion promoting layer,
a sintered metal layer; and
a conductive layer arranged on the at least one main area.

### Claim 2 (depends on 1)

The power semiconductor substrate of claim 1, wherein the sheet-like base is formed of an industrial ceramic.

### Claim 3 (depends on 2)

The power semiconductor substrate of claim 2, wherein said industrial ceramic is selected from the group consisting of aluminium oxide, aluminium nitrite and silicon nitrite.

### Claim 4 (depends on 1)

The power semiconductor substrate of claim 1, wherein said adhesion promoting layer has a thickness of about between 0.5 μm and about 10 μm and include a precious metal surface facing said sintered metal layer.

### Claim 5 (depends on 1)

The power semiconductor substrate of claim 1, wherein said sintered metal layer has a thickness of between about 5 μm and about 50 μm.

### Claim 6 (depends on 1)

The power semiconductor substrate of claim 1, wherein said conductive layer is a copper foil having a thickness of between about 100 μm and about 800 μm and has a precious metal surface facing said sintered metal layer.

### Claim 7 (depends on 1)

The power semiconductor substrate of claim 1, wherein said sintered metal layer has a thickness of between about 5 μm and about 50 μm.

### Claim 8 (depends on 7)

The power semiconductor substrate of claim 7, wherein said conductive layer is a copper foil having a thickness of between about 100 μm and about 800 μm and has a precious metal surface facing said sintered metal layer.

### Claim 9 (depends on 1)

The power semiconductor substrate of claim 1, wherein said conductive layer is a copper foil having a thickness of between about 100 μm and about 800 μm and has a precious metal surface facing said sintered metal layer.

### Claim 10 (depends on 9)

The power semiconductor substrate of claim 9, wherein said adhesion promoting layer has a thickness of about between 0.5 μm and about 10 μm and include a precious metal surface facing said sintered metal layer.

### Claim 11

A method for producing a power semiconductor substrate having an insulating sheet-like base and at least one main area, at least one sequence of layers comprising a thin adhesion promoting layer, a sintered metal layer and a conductive layer arranged on the at least one main area, the method comprising the steps of:
coating at least a portion of the main area with the adhesion promoting layer;
arranging a pasty layer of the sintered metal and a solvent on a portion of the adhesion promoting layer;
arranging the conductive layer on the sintered metal layer; and
applying pressure to the conductive layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the pasty layer is applied by screen printing.

### Claim 13 (depends on 11)

The method of claim 11, the pressure is applied by means of a press and two press rams, at least one press ram being formed with a silicone pad arranged thereon, producing quasi-hydrostatic pressure.

### Claim 14 (depends on 11)

The method of claim 11, wherein the maximum final pressure when pressure is applied is at least 8 MPa.

### Claim 15 (depends on 7)

The method of claim 7, further comprising the step of heating the power semiconductor substrate to a temperature of between about 350 K and about 600 K when the pressure is being applied.

### Claim 16 (depends on 7)

The method of claim 7, further comprising the step of covering the power semiconductor substrate with a film before the pressure is applied.