# US 2008/0292844 A1 · Glass article having improved edge

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2008/0292844 A1
- Document ID: US20080292844A1
- Status: Published application
- Kind: A1
- Application number: 11/805,077
- Filed: 2007-05-22
- Published: 2008-11-27
- Earliest claimed: 2007-05-22
- Assignees: Corning Incorporated
- Inventors: Robert Sabia; Jiangwei Feng
- Web page: https://patentgrep.com/patent/US20080292844A1

## CPC

- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 19/00: Surface treatment of glass, not in the form of fibres or filaments, by mechanical means (sand-blasting, grinding, or polishing glass B24)
- C03C 2204/08: Glass having a rough surface
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- Y10T 428/24372: Particulate matter
- Y10T 428/24421: Silicon containing
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass article having an edge of which at least a portion that is ground and subsequently etched to provide a roughened edge. The roughened edge scatters light, thus enabling the glass article to be properly aligned. In some embodiments, the roughened edge also provides a surface having a coefficient of friction that facilitates handling of the glass article. The edge may further include at least one chamfer that may either be polished, so as to be transparent or ground and subsequently etched.

## Claims

### Claim 1

A glass article, the glass article having a peripheral surface, the peripheral surface comprising a roughened portion that has been ground and etched, wherein the roughened portion has a RMS roughness that is capable of scattering light of a predetermined wavelength, and wherein the peripheral surface having the roughened portion has a particle release of less than about 740 particles/cm2 area of the peripheral surface, wherein each of the particles released is greater than 2 μm in size.

### Claim 2 (depends on 1)

The glass article according to claim 1, wherein the peripheral surface further comprises at least one chamfer adjacent to and intersecting a major planar surface of the glass article.

### Claim 3 (depends on 2)

The glass article according to claim 2, wherein at least a portion of the chamfer has been polished.

### Claim 4 (depends on 2)

The glass article according to claim 2, wherein the chamfer has a roughness that is capable of scattering light of a predetermined wavelength.

### Claim 5 (depends on 4)

The glass article according to claim 4, wherein the chamfer includes an etched portion.

### Claim 6 (depends on 5)

The glass article according to claim 5, wherein the etched portion of the chamfer has a RMS roughness of at least about 200 nm.

### Claim 7 (depends on 1)

The glass article according to claim 1, wherein the peripheral surface has a static coefficient of friction in a range from about 0.80 to about 0.50, as measured using a Teflon rod in dry conditions.

### Claim 8 (depends on 1)

The glass article according to claim 1, wherein the glass article is a fused silica article.

### Claim 9 (depends on 8)

The glass article according to claim 8, wherein the fused silica article is a liquid crystal display image mask.

### Claim 10 (depends on 8)

The glass article according to claim 8, wherein the fused silica article has an aspect ratio of at least 100.

### Claim 11 (depends on 1)

The glass article according to claim 1, wherein the RMS roughness is at least about 200 nm.

### Claim 12 (depends on 11)

The glass article according to claim 11, wherein the RMS roughness is at least about 300 nm.

### Claim 13 (depends on 1)

The glass article according to claim 1, wherein the predetermined wavelength is in a range from about 500 nm to about 670 nm.

### Claim 14 (depends on 1)

The glass article according to claim 1, wherein the light scattered by the roughened portion, when measured at an angle in a range from about 5° to about 60° to incident light, has a normalized intensity in a range from about 120 to 20 with absolute total scattering in a range from about 1% up to about 20%.

### Claim 15 (depends on 1)

The glass article according to claim 1, wherein the peripheral surface has a static coefficient of friction in a range from about 0.80 to about 0.50, as measured using a Teflon rod in dry conditions.

### Claim 16

A fused silica article, the fused silica article having a peripheral surface having an etched portion that has a RMS roughness that is capable of scattering light of a predetermined wavelength, wherein the roughened portion has been formed by:
a. providing a near net shape of the fused silica article;
b. grinding the near net shape including the peripheral surface to a dimensional tolerance of the fused silica article; and
c. etching at least a portion of the peripheral surface to form an etched portion of the peripheral surface, wherein the peripheral surface having the etched portion has a particle release of less than about 740 particles/cm2 area of the peripheral surface, wherein each of the particles released is greater than 2 μm in size.

### Claim 17 (depends on 16)

The fused silica article according to claim 16, wherein the peripheral surface has a static coefficient of friction in a range from about 0.80 to about 0.50, as measured using a Teflon rod in dry conditions.

### Claim 18 (depends on 16)

The fused silica article according to claim 16, wherein the fused silica article is a liquid crystal display image mask.

### Claim 19 (depends on 16)

The fused silica article according to claim 16, wherein the fused silica article has an aspect ratio of at least 100.

### Claim 20 (depends on 16)

The fused silica article according to claim 16, wherein etching the polished surface comprises etching the ground surface with one of an acid etchant and an alkali etchant.

### Claim 21 (depends on 20)

The fused silica article according to claim 20, wherein the alkali etchant comprises at least one of KOH, NH4OH, NH4HF2, and TMAH.

### Claim 22 (depends on 20)

The fused silica article according to claim 20, wherein the acid etchant comprises HF and at least one of a fluoride salt and an acid selected from the group consisting of H2SO4, HCl, H3PO4, and HNO3.

### Claim 23 (depends on 16)

The fused silica article according to claim 16, wherein the RMS roughness is at least about 200 nm.

### Claim 24 (depends on 23)

The fused silica article according to claim 23, wherein the RMS roughness is at least about 300 nm.

### Claim 25 (depends on 16)

The fused silica article according to claim 16, wherein the predetermined wavelength is in a range from about 500 nm to about 670 nm.

### Claim 26 (depends on 16)

The fused silica article according to claim 16, wherein the light scattered by the roughened portion, when measured at an angle in a range from about 5° to about 60° to incident light, has a normalized intensity in a range from about 120 to 20 with absolute total scattering in a range from about 1% up to about 20%.

### Claim 27 (depends on 16)

The fused silica article according to claim 16, wherein the peripheral surface has a static coefficient of friction in a range from about 0.80 to about 0.50, as measured using a Teflon rod in dry conditions.

### Claim 28

A fused silica article, the fused silica article having a peripheral surface, the peripheral surface comprising:
a. a roughened portion that has a roughness that is capable of scattering light of a predetermined wavelength, wherein the roughened portion has been formed by:
i. providing a near net shape of the fused silica article the near net shape having two planar surfaces and a peripheral surface;
ii. grinding the near net shape including the peripheral surface to a dimensional tolerance, and wherein at least one chamfer adjacent to and intersecting a major planar surface of the near net shape is formed by grinding the near net shape; and
iii. etching at least a portion of the peripheral surface to form an etched portion of the peripheral surface, wherein the peripheral surface having the etched portion has a particle release of less than about 740 particles/cm2 area of the peripheral surface, wherein each of the particles released is greater than 2 μm in size.

### Claim 29 (depends on 28)

The fused silica article according to claim 28, wherein at least a portion of the chamfer has been polished.

### Claim 30 (depends on 28)

The fused silica article according to claim 28, wherein the chamfer has a roughness that is capable of scattering light of a predetermined wavelength.

### Claim 31 (depends on 28)

The fused silica article according to claim 28, wherein at least a portion of the chamfer has been etched.

### Claim 32 (depends on 30)

The fused silica article according to claim 30, wherein the portion of the chamfer that has been etched has a RMS roughness of at least about 200 nm.

### Claim 33 (depends on 28)

The fused silica article according to claim 28, wherein the etched portion of the peripheral surface has a RMS roughness of at least about 200 nm.

### Claim 34 (depends on 33)

The fused silica article according to claim 33, wherein the roughened portion has a roughness of at least about 300 nm.

### Claim 35 (depends on 28)

The fused silica article according to claim 28, wherein the predetermined wavelength is in a range from about 500 nm to about 670 nm.

### Claim 36 (depends on 28)

The fused silica article according to claim 28, wherein the light scattered by the roughened portion, when measured at an angle in a range from about 5° to about 60° to incident light, has a normalized intensity in a range from about 120 to 20 with absolute total scattering in a range from about 1% up to about 20%.

### Claim 37 (depends on 28)

The fused silica article according to claim 28, wherein the fused silica article is a liquid crystal display image mask.

### Claim 38 (depends on 28)

The fused silica article according to claim 28, wherein the fused silica article has an aspect ratio of at least 100.

### Claim 39 (depends on 28)

The fused silica article according to claim 28, wherein the peripheral surface has a static coefficient of friction in a range from about 0.80 to about 0.50, as measured using a Teflon rod in dry conditions.

### Claim 40 (depends on 28)

The fused silica article according to claim 28, wherein etching the ground surface comprises etching the ground surface with one of an acid etchant and an alkali etchant.

### Claim 41 (depends on 40)

The fused silica article according to claim 40, wherein the alkali etchant comprises at least one of KOH, NH4OH, NH4HF2, and TMAH.

### Claim 42 (depends on 40)

The fused silica article according to claim 40, wherein the acid etchant comprises HF and at least one of a fluoride salt and an acid selected from the group consisting of H2SO4, HCl, H3PO4, and HNO3.

### Claim 43

A method of making a glass article having a roughened peripheral surface, the method comprising the steps of:
a. providing a near net shape of the fused silica article, the near net shape having two major planar surfaces and a peripheral surface;
b. grinding the near net shape including the peripheral surface to a dimensional tolerance; and
c. etching at least a portion of the ground peripheral surface to form a etched surface, wherein the etched surface has a roughness that is capable of scattering light of a predetermined wavelength to form the glass article.

### Claim 44 (depends on 43)

The method according to claim 43, wherein the step of etching at least a portion of the ground peripheral surface to form a etched surface comprises etching the surface with one of an acid etchant and an alkali etchant.

### Claim 45 (depends on 44)

The method according to claim 44, wherein the alkali etchant comprises at least one of KOH, NH4OH, NH4HF2, and TMAH.

### Claim 46 (depends on 45)

The method according to claim 45, wherein the step of etching at least a portion of the ground peripheral surface to form a etched surface comprises heating the alkali etchant to a temperature in a range from about 80° C. up to about 100° C.

### Claim 47 (depends on 44)

The method according to claim 44, wherein the acid etchant comprises HF and at least one of a fluoride salt and an acid selected from the group consisting of H2SO4, HCl, H3PO4, and HNO3.

### Claim 48 (depends on 43)

The method according to claim 43, wherein the glass article is a fused silica article.

### Claim 49 (depends on 43)

The method according to claim 43, wherein the fused silica article is a liquid crystal display image mask.

### Claim 50 (depends on 43)

The method according to claim 43, wherein the predetermined wavelength is in a range from about 500 nm to about 670 nm.

### Claim 51 (depends on 43)

The method according to claim 43, wherein the light scattered by the roughened portion, when measured at an angle in a range from about 5° to about 60° to incident light, has a normalized intensity in a range from about 120 to 20 with absolute total scattering in a range from about 1% up to about 20%.

### Claim 52 (depends on 43)

The method according to claim 43, wherein the etched surface has a RMS roughness of at least about 200 nm.

### Claim 53 (depends on 43)

The method according to claim 43, wherein the step of grinding the near net shape further comprises forming at least one chamfer on the peripheral surface, wherein the chamfer is adjacent to and intersects one of the two major planar faces of the glass article.

### Claim 54 (depends on 53)

The method according to claim 53, further comprising the step of polishing at least a portion of the chamfer to form a polished chamfer.

### Claim 55 (depends on 53)

The method according to claim 53, further comprising the step of etching the chamfer to form a chamfer having a roughened surface.

### Claim 56 (depends on 43)

The method according to claim 43, further including the step of polishing the two major planar faces.

### Claim 57 (depends on 43)

The method according to claim 43, wherein the glass article is a fused silica article.

### Claim 58 (depends on 43)

The method according to claim 43, wherein the fused silica article is a liquid crystal display image mask.

### Claim 59 (depends on 43)

The method according to claim 43, wherein the peripheral surface has a static coefficient of friction in a range from about 0.80 to about 0.50, as measured using a Teflon rod in dry conditions.

### Claim 60 (depends on 43)

The method according to claim 43, wherein the peripheral surface having the etched surface has a particle release of less than about 740 particles/cm2 area of the peripheral surface, wherein each of the particles released is greater than 2 μm in size.

### Claim 61

A method of roughening a surface of a glass article, the method comprising:
a. providing a glass article having a peripheral surface;
b. grinding at least a portion of the peripheral surface to produce a ground portion; and
c. etching the ground portion to form an etched surface, wherein the etched surface has a RMS roughness that is capable of scattering light of a predetermined wavelength.